Dynamic oxide film evolution and corrosion mechanisms of 308L stainless steel in simulated SMR environments

Pengfei Gao, Yanhui Li, Wang Zhu, Jie Qiu, Zhouyang Bai, Qibo Wang, Shaoming Ding

Corrosion Science· Volume 248
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Global sensitivity analysis of nuclear district heating reactor primary heat exchanger and pressure vessel optimization10.1016/j.energy.2024.133393 ↗
2. Matching analysis of technical parameters and safety standards for nuclear replacement of coal-fired units
3. Opportunities and challenges for a sustainable energy future10.1038/nature11475 ↗
4. A boron-adjustment-free control strategy for large pressurized water reactors10.1016/j.anucene.2022.109106 ↗
5. Some features of the effect the pH value and the physicochemical properties of boric acid have on mass transfer in a VVER reactors core10.1134/S0040601513070045 ↗
6. Effect of boric-acid on pit growth in alloy-600 steam-generator tubing10.5006/1.3299816 ↗
7. Core neutronics and safety characteristics of a boron-free core for small modular reactors10.1016/j.anucene.2019.04.017 ↗
8. Hydrodynamics of the effectiveness of the AP-CITROX decontamination technology10.1023/A:1021662726609 ↗
9. A review of the application of chemical decontamination technology in the United States10.1016/0149-1970(90)90013-U ↗
10. A study on the removal of impurities in a SP-HyBRID decontamination wastewater of the primary coolant system in a pressurized water reactor10.1007/s10967-018-6219-0 ↗
11. Boron-free small modular pressurized water reactor design with new burnable absorber10.1002/er.3590 ↗
12. Neutronic design and analysis of advanced long-cycle boron-free operation of a small modular reactor core with particle type burnable poison rods10.1002/er.4207 ↗
13. Fouling behavior of a printed circuit steam generator under simulated operating conditions of a small modular reactor10.1016/j.anucene.2022.109127 ↗
14. Design optimization of cylindrical burnable absorber inserted into annular fuel pellets for soluble-boron-free SMR10.1016/j.net.2021.09.043 ↗
15. Investigation on long-term daily load follow operation capability of soluble boron-free SMR10.1016/j.anucene.2020.107764 ↗
16. Feasibility study of a soluble boron-free small modular integral pressurized water reactor10.13182/NT13-135 ↗
17. Correlating oxidation resistance to stress corrosion cracking of 309L and 308L stainless steel claddings in simulated PWR primary water10.1016/j.jnucmat.2022.153509 ↗
18. A review on the behavior of 308L cladding material and their corrosion in nuclear power plants10.20964/2020.01.67 ↗
19. Short time oxidation behavior of 308L weld metal and 316L stainless steel with different surface state in simulated primary water with 0.1 mg/L dissolved oxygen10.1002/maco.201408013 ↗
20. Effect of surface state on the oxidation behavior of welded 308L in simulated nominal primary water of PWR10.1016/j.apsusc.2015.02.066 ↗
21. An insight into PWR primary water SCC mechanisms by comparing surface and crack oxidation10.1016/j.corsci.2018.12.020 ↗
22. Stress corrosion cracking of fusion boundary for 316L/52M dissimilar metal weld joints in borated and lithiated high temperature water10.1016/j.corsci.2017.01.024 ↗
23. Comparison of stress corrosion cracking susceptibilities of 308L and 309L cladding layers in high-temperature water with various dissolved oxygen concentrations10.1016/j.jnucmat.2022.153913 ↗
24. Characterization of microstructure of A508III/309L/308L weld and oxide films formed in deaerated high-temperature water10.1016/j.jnucmat.2017.10.030 ↗
25. Effect of surface state of austenitic type 304L SS on oxide characteristics formed in high temperature high pressure water10.1016/j.jnucmat.2022.153672 ↗
26. Investigation of the corrosion behavior of 304L and 316L stainless steels at high-temperature borated and lithiated water10.1080/00223131.2015.1125311 ↗
27. Effects of surface treatments and temperature on the oxidation behavior of 308L stainless steel cladding in hydrogenated high-temperature water10.1016/j.jnucmat.2022.153741 ↗
28. Effect of boron distribution on the intergranular corrosion resistance of UNS S32506 duplex stainless steels10.1149/2.1101912jes ↗
29. Interphase corrosion inhibition mechanism of sodium borate on carbon steel rebars in simulated concrete pore solution10.1016/j.conbuildmat.2023.133763 ↗
30. Effect of nickel ion from autoclave material on oxidation behaviour of 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.12.008 ↗
31. Analysis of oxide film formed on type 304 stainless steel in 288 °C water containing oxygen, hydrogen, and hydrogen peroxide10.5006/1.3283969 ↗
32. Microstructural characteristics of the oxide scale formed on 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.07.015 ↗
33. Influence of dissolved oxygen concentration on the oxide film formed on 304 stainless steel in high temperature water10.1016/j.corsci.2012.06.007 ↗
34. Micro-Raman spectroscopic study of fine-grained, shock-metamorphosed rock fragments from the Australasian microtektite layer10.1111/j.1945-5100.2008.tb01023.x ↗
35. High-pressure phase transitions in FeCr2O4 and structure analysis of new post-spinel FeCr2O4 and Fe2Cr2O5 phases with meteoritical and petrological implications10.2138/am.2014.4736 ↗
36. Investigation of multiplet splitting of Fe 2p XPS spectra and bonding in iron compounds10.1002/sia.1984 ↗
37. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni10.1016/j.apsusc.2010.10.051 ↗
38. Early oxidation mechanism of austenitic stainless steel TP347H in supercritical water10.1016/j.corsci.2017.09.023 ↗
39. Analysis of oxyanion (BO33-, CO32-, SO42-, PO43-, SeO44-) substitution in Y123 compounds studied by X-ray photoelectron spectroscopy10.1007/BF00728433 ↗
40. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
41. The mechanism of high-temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
42. Point defect model for the corrosion of steels in supercritical water: Part I, film growth kinetics
43. Novel design concept for a commercial-scale plant for supercritical water oxidation of industrial and sewage sludge10.1016/j.jenvman.2018.11.142 ↗
44. Formation mechanism of the outer layer of duplex scales on stainless steels in oxygenated supercritical water10.1016/j.matlet.2020.127731 ↗
45. Fundamental atomic-scale kinetic models for the oxidation of iron/nickel-based alloys in low-density supercritical water10.1016/j.cplett.2023.140631 ↗
46. Point defects and transport properties of binary and ternary oxides10.1016/0167-2738(84)90126-7 ↗
47. Pourbaix diagrams for the nickel-water system extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.007 ↗
48. Pourbaix diagrams for the iron–water system extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2011.10.034 ↗
49. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
50. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
51. Effects of boric acid and lithium hydroxide on the corrosion behaviors of 316LN stainless steel in simulating hot functional test high-temperature pressurized water10.1016/j.corsci.2022.110157 ↗
52. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
53. Investigation on early formation and evolution of oxide scales on ferritic-martensitic steels in supercritical water10.1016/j.corsci.2018.02.036 ↗
54. Formation of nanocrystalline δ-ZrHx in Zircoloy-4: orientation relationship and twinning10.1016/j.jallcom.2015.10.256 ↗