Effect of ultrasonic-assisted abrasive peening on near-surface characteristics and electrochemical behaviour of Al-6061 alloy
Source abstract
Abstract
This study investigates the influence of ultrasonic-assisted abrasive peening (UAP) on the microstructural evolution and corrosion characteristics of Al-6061 alloy. A 3 min peened sample demonstrated a 50 % reduction in grain size and a 14-fold increase in residual stress compared to its unpeened state. The corrosion rate for the 3 min peening also decreased to 9.42 × 10 −3 mm/year, compared to 89.4 × 10 −3 mm/year for the unpeened alloy specimen. Peening beyond 3 min was observed to be susceptible to pitting. Hence, the UAP is found to be an effective method of improving the corrosion resistance of Al-6061.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Residual Stress · High Entropy Alloys Studies · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Enhanced corrosion resistance of 15–15Ti austenitic steel in liquid lead-bismuth eutectic at 550 ℃ by shot peening processing10.1016/j.corsci.2023.111640 ↗
2. S. Bena, D. Retraint, S.Y. Brou, B. Panicaud, J.L.G. Poussard, 2018, Influence of Surface Mechanical Attrition Treatment on the oxidation behaviour of 316L stainless steel, 136 (2018) 188–200..10.1016/j.corsci.2018.03.007 ↗
3. Effect of water jet cavitation peening on electrochemical corrosion behavior of nickel-based alloy 600 in NaCl solution10.1016/j.matchemphys.2022.127122 ↗
4. Laser shock peening of AlCoCrCuFeNi high-entropy alloy fabricated by laser powder bed fusion: an enhanced oxidation-resistance mechanism at high-temperature10.1016/j.corsci.2023.111667 ↗
5. Effect of ultrasonic shot peening duration on the microstructure and mechanical properties of CrMnFeCoNi high-entropy alloy
6. Microstructure changes and mechanical properties of U-2Nb alloy induced by shot peening treatment10.1016/j.jallcom.2021.162977 ↗
7. Obvious improvement in electrochemical and long-term immersion corrosion resistance of AISI 420 martensitic stainless steel using laser shock peening10.1016/j.corsci.2022.110688 ↗
8. Study on the effect of laser peening with different power densities on fatigue life of fastener hole10.1016/j.optlastec.2018.04.025 ↗
9. Introduction of compressive residual stresses in Ti-6Al-4V simulated airfoils via laser shock processing10.1361/105994901770344539 ↗
10. Influence of severe surface plastic deformation induced by shot peening on microstructure and corrosion resistance of fine grained 316L stainless steel10.1016/j.corsci.2024.111988 ↗
11. Influence of surface mechanical attrition treatment (SMAT) on the corrosion behaviour of AISI 304 stainless steel10.1016/j.corsci.2013.04.056 ↗
12. Surface & coatings technology influence of ultrasonic-assisted abrasive peening treatment on Ti-6Al-4V and OFHC Cu alloys10.1016/j.surfcoat.2024.131317 ↗
13. Material removal in ultrasonic abrasive polishing of additive manufactured components10.3390/app9245359 ↗
14. Ultrasonic abrasive polishing of additive manufactured parts: an experimental study on the effects of process parameters on polishing performance
15. K.L. Tan, S.H. YeoCavitation erosion study in deionized water containing abrasive particles, Ann. DAAAM Proc. Int. DAAAM Symp. 2015-Janua (2015) 818–824. .1142015, https://doi.org/10.2507/26th.daaam.proceedings.10.2507/26th.daaam.proceedings ↗
16. Surface modification of additive manufactured components by ultrasonic cavitation abrasive finishing10.1016/j.wear.2017.02.030 ↗
17. Deburring and surface conditioning of micro milled structures by micro peening and ultrasonic wet peening10.1007/s00542-006-0087-1 ↗
18. A. Kienzler, V. Schulze, D. Löhe, Surface conditioning by ultrasonic wet peening, (2006).
19. Surface finishing on IN625 additively manufactured surfaces by combined ultrasonic cavitation and abrasion
20. Cavitation damages on solid surfaces in suspensions containing spherical and irregular microparticles10.1016/j.wear.2008.05.010 ↗
21. Corrosion behaviour of AISI 304 stainless steel subjected to massive laser shock peening impacts with different pulse energies10.1016/j.corsci.2013.11.003 ↗
22. Effect of laser shock peening on the dissolution of precipitates and pitting corrosion of AA6061-T6 with different original surface roughness10.1016/j.corsci.2023.111794 ↗
23. Effect of laser shock peening on corrosion behaviors of ultra-high strength Al-Zn-Mg-Cu alloys prepared by spray forming and ingot metallurgy10.1016/j.corsci.2022.110458 ↗
24. Localized corrosion behaviour of AA7150 after ultrasonic shot peening: corrosion depth vs. impact energy10.1016/j.corsci.2017.11.008 ↗
25. Effects of nanofeatures induced by severe shot peening (SSP) on mechanical, corrosion and cytocompatibility properties of magnesium alloy AZ3110.1016/j.actbio.2017.11.032 ↗
26. Thermal relaxation of residual stresses in shot peened surface layer of SiCw/Al composite10.1007/s11665-011-9982-4 ↗
27. Effect of laser shock peening on mechanical and microstructural aspects of 6061-T6 aluminum alloy10.1016/j.jmatprotec.2020.116640 ↗
28. Tailoring of residual stress by ultrasonic vibration-assisted abrasive peening in liquid cavitation of metallic alloys10.1016/j.ijmachtools.2023.104100 ↗
29. Capability evaluation of ultrasonic cavitation peening at different standoff distances10.1016/j.ultras.2017.10.013 ↗
30. Ultrasonic-assisted abrasive micro-deburring of micromachined metallic alloys10.1016/j.jmapro.2021.04.019 ↗
31. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
32. Improving microstructural and mechanical characteristics of cold-sprayed Inconel 718 deposits via local induction heat treatment10.1016/j.jallcom.2019.05.099 ↗
33. Microstructural evolution of nanocrystalline chips particles produced via large strain machining during ball milling10.1016/j.powtec.2013.07.028 ↗
34. X-ray and neutron diffraction measurements of dislocation density and subgrain size in a friction stir welded aluminium alloy
35. Effect of grit blasting parameters on surface and near-surface properties of different metal alloys10.1007/s11666-020-01127-1 ↗
36. X-ray and neutron diffraction measurements of dislocation density and subgrain size in a friction-stir-welded aluminum alloy10.1007/s11661-009-9963-5 ↗
37. Uphill quenching to reduce residual stress in aluminium alloy 7449 hollow structures10.1007/s11340-022-00836-8 ↗
38. Influence of peening on the corrosion properties of AISI 304 stainless steel10.1016/j.corsci.2009.08.008 ↗
39. Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T810.1016/j.surfcoat.2021.127354 ↗
40. Influence of combined shot peening and PEO treatment on corrosion fatigue behavior of 7A85 aluminum alloy10.1016/j.apsusc.2019.04.242 ↗
41. Experimental investigation into the effect of process parameters on the Inconel 718 surface integrity for abrasive waterjet peening10.1016/j.surfcoat.2022.129186 ↗
42. Improving peening efficacy through high-amplitude short duration pulsed current10.1016/j.jallcom.2022.166987 ↗
43. Influence of ultrasonic shot peening on corrosion behavior of 7075 aluminum alloy10.1016/j.jallcom.2017.06.310 ↗
44. Influence of second phase precipitates on mechanical and in-vitro corrosion behaviour of Mg-4Zn-0.5Ca-0.8Mn alloy in optimum homogenized conditions10.1016/j.jma.2022.11.011 ↗
45. Enhanced in-vitro degradation resistance and cytocompatibility of a thermomechanically processed novel Mg alloy: Insights into the role of microstructural attributes10.1016/j.jma.2024.01.022 ↗
46. Corrosion and stress corrosion cracking characteristics of 4043 aluminium alloy fabricated through directed energy deposition process10.1016/j.jallcom.2023.173154 ↗
47. On the corrosion of a high solute Al-Zn-Mg alloy produced by laser powder bed fusion10.1016/j.corsci.2021.109626 ↗
48. Cavitation erosion of face centered cubic metals10.1007/BF02661573 ↗
49. Strategy of residual stress determination on selective laser melted al alloy using XRD
50. Effect of pitting corrosion on fatigue performance of shot-peened aluminium alloy 7075-T65110.1016/j.jmatprotec.2010.03.004 ↗
51. Role of ultrasonic shot peening on low cycle fatigue behavior of 7075 aluminium alloy10.1016/j.ijfatigue.2017.06.033 ↗
52. Effect of combined shot-peening and PEO treatment on fatigue life of 2024 Al alloy10.1016/j.tsf.2006.07.123 ↗
53. Surface characteristics and stress corrosion behavior of AA 7075-T6 aluminum alloys after different shot peening processes10.1016/j.surfcoat.2022.128481 ↗
54. Mechanical and corrosion properties in 3.5% NaCl solution of cold sprayed Al-based coatings10.1016/j.surfcoat.2020.125372 ↗
55. Surface modifications induced in 316L steel by laser peening and shot-peening. Influence on pitting corrosion resistance10.1016/S0921-5093(99)00698-X ↗
56. Improving corrosion resistance properties of nickel-aluminum bronze (NaB) alloys via shot peening treatment10.2320/matertrans.M2019031 ↗
57. Local electrochemical impedance spectroscopy study of the influence of ageing in air and laser shock processing on the micro-electrochemical behaviour of AA2050-T8 aluminium alloy10.1016/j.electacta.2011.01.091 ↗
58. Significant improvement of corrosion resistance of biodegradable metallic implants processed by laser shock peening10.1016/j.cirp.2012.03.125 ↗
59. Influence of thermal and mechanical surface modifications induced by laser shock processing on the initiation of corrosion pits in 316L stainless steel10.1007/s10853-007-1502-4 ↗
60. Effects of compressive stress on localized corrosion in AA2024-T310.1016/j.corsci.2005.12.003 ↗
61. Grain refinement of LY2 aluminum alloy induced by ultra-high plastic strain during multiple laser shock processing impacts10.1016/j.actamat.2010.03.026 ↗
62. Corrosion behaviour improvement from the ultrafine-grained Al–Zn–In alloys in Al–air battery10.1016/j.egyr.2022.03.132 ↗
63. Evaluation of corrosion resistance of AA6082-T651 aluminium alloy after laser shock peening by means of cyclic polarisation and ElS methods10.1016/j.corsci.2012.03.019 ↗
64. Laser shock peening without coating induced residual stress distribution, wettability characteristics and enhanced pitting corrosion resistance of austenitic stainless steel10.1016/j.apsusc.2017.09.138 ↗
65. Effect of warm shot peening treatments on surface properties and corrosion behavior of AZ31 magnesium alloy10.1016/j.surfcoat.2020.126285 ↗
66. The electrochemical deposition of polyaniline at pure aluminium: electrochemical activity and corrosion protection properties10.1016/S0013-4686(02)00741-7 ↗
67. Effect of surface mechanical attrition treatment on corrosion behavior of 316 stainless steel10.1016/S1006-706X(09)60030-3 ↗