Revealing the excellent corrosion performance of SIMP steel in CO2 at 600 ℃: The role of Si and Mn

Chao Liu, Le Qi, Tielong Shen, Zhiguang Wang

Corrosion Science· Volume 240
Publisher page

Abstract

Compared with T91 and 321, SIMP steel exhibit excellent corrosion resistance in CO 2 at 600 °C. The structure and composition of surface oxide films on the steels were characterized in detail using advanced micro/nano analytical techniques. Different from the typical internal and external spinel oxide layers formed on T91 and 321, a multi-layer oxide film consisting of continuous Cr-rich oxides [Cr 2O 3 and (Cr, Mn) 3O 4] and nearly continuous SiO 2 is external grown on SIMP, acting an excellent protective barrier against oxidation and carbonization. The role of Si, Mn in the corrosion resistance of SIMP steel was discussed.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Development of accelerator driven advanced nuclear energy (ADANES) and nuclear fuel recycle
2. Development of a novel structural material (SIMP steel) for nuclear equipment with balanced resistances to high temperature, radiation and liquid metal corrosion
3. Corrosion behavior of ferritic–martensitic steels SIMP and T91 in fast-flowing steam10.1016/j.corsci.2021.109474 ↗
4. Accelerated steam corrosion behavior of Fe-ion irradiated RAFM steel: the role of displacement damage10.1016/j.corsci.2023.111074 ↗
5. Oxidation behavior of ferritic/martensitic steels in flowing supercritical water10.1016/j.jmst.2020.01.009 ↗
6. Oxidation behavior of ferritic/martensitic steels in stagnant liquid LBE saturated by oxygen at 600 °C10.1016/j.jnucmat.2014.11.018 ↗
7. Performance of the new ferritic/martensitic steel SIMP against liquid lead-bismuth eutectic corrosion: comparison with T91 and 316L steels10.1002/maco.202213372 ↗
8. Experimental investigation on corrosion of structural steels in molten Pb-Mg and LBE
9. Comparison investigation on corrosion of SIMP and T91 steels exposed to liquid LBE at 450 ℃: The role of Si on reducing oxidation rate10.1016/j.corsci.2023.111553 ↗
10. Influence of temperature on the microstructural evolution of SIMP and T91 steels in liquid lead-bismuth eutectic: Experiments and molecular dynamics simulations10.1016/j.corsci.2023.111411 ↗
11. Corrosion of 9Cr Steel in CO2 at intermediate temperature i: mechanism of void-induced duplex oxide formation10.1007/s11085-011-9271-5 ↗
12. Corrosion by Hot CO2 Gases10.1149/2.F08212IF ↗
13. Materials Performance in CO2 and Supercritical CO2
14. State of the art overview material degradation in high-temperature supercritical CO2 environments10.1016/j.pmatsci.2023.101107 ↗
15. Corrosion of 9-12Cr ferritic–martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
16. Corrosion Behavior of Different Metallic Materials in Supercritical Carbon Dioxide at 550°C and 250 bars10.5006/1.3628683 ↗
17. Corrosion behaviour of Fe-25Cr alloy in wet CO2 gas at 650 °C: effects of chloride deposits and Si+Mn alloying addition10.1016/j.corsci.2021.110001 ↗
18. Effect of silicon on corrosion of Fe-20Cr and Fe-20Cr-20Ni alloys in wet CO2 with and without HCl at 650 °C10.1016/j.corsci.2020.109096 ↗
19. Effects of Si and SO2 on Corrosion of Fe–20Cr and Fe–20Cr–20Ni Alloys in Reducing Waste Combustion Gases10.1007/s11085-023-10200-3 ↗
20. Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2 at 700 °C10.1016/j.corsci.2017.11.005 ↗
21. Effects of Silicon and Water Vapour on Corrosion of Fe–20Cr and Fe–20Cr–20Ni Alloys in CO2 at 650 °C10.1007/s11085-016-9681-5 ↗
22. Effects of Silicon on High Temperature Corrosion of Fe–Cr and Fe–Cr–Ni Alloys in Carbon Dioxide10.1007/s11085-013-9467-y ↗
23. Oxidation kinetics and microstructure evolution of high Mn stainless-steel alloy in CO2 at 700 °C10.1016/j.corsci.2021.110013 ↗
24. Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650 °C10.1016/j.corsci.2016.07.014 ↗
25. Effects of cerium and manganese on corrosion of Fe–Cr and Fe–Cr–Ni alloys in Ar–20CO2 gas at 818 °C10.1016/j.corsci.2013.06.046 ↗
26. C. Liu, T. Shen, L. Qi, Z. Ma, H. Chang, Z. Wang, Microstructural evolution of pre-oxidized T91 steel during LBE dissolution corrosion, Research Square, (2024). https://doi.org/10.21203/rs.3.rs-4239651/v1.10.21203/rs.3.rs-4239651/v1 ↗
27. A research on the corrosion and stress corrosion cracking susceptibility of 316L stainless steel exposed to supercritical water10.1016/j.corsci.2017.08.027 ↗
28. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
29. Microstructural evolution of early-stage oxide film on 15–15Ti austenitic stainless steel under 500 ℃ steam10.1016/j.corsci.2022.110557 ↗
30. Identification by photoelectrochemistry of oxide phases grown during the initial stages of thermal oxidation of AISI 441 ferritic stainless steel in air or in water vapour10.1016/j.corsci.2008.12.002 ↗
31. Effect of δ-ferrite on the stress corrosion cracking behavior of 321 stainless steel10.1016/j.corsci.2019.07.005 ↗
32. Corrosion behavior of a new alumina-forming duplex stainless steel with different surface treatment in supercritical carbon dioxide10.1016/j.surfcoat.2023.129619 ↗
33. Understanding the stress corrosion cracking growth mechanism of a cold worked alumina-forming austenitic steel in supercritical carbon dioxide10.1016/j.corsci.2022.110179 ↗
34. The beneficial effect of surface carbon coating on stress corrosion cracking of Type 304 austenitic stainless steels in high temperature water10.1016/j.scriptamat.2018.08.033 ↗
35. TEM comparative study on oxide films of 316L and T91 steel exposed to 350–500 °C steam10.1016/j.jmst.2023.07.046 ↗
36. Improving the oxidation resistance of SIMP steel to liquid Pb-Bi eutectic by shot peening treatments10.1016/j.apsusc.2021.151910 ↗
37. Chapter 2 - Enabling Theory
38. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
39. Effects of cerium and manganese on corrosion of Fe–Cr and Fe–Cr–Ni alloys in Ar–20CO2 and Ar–20CO2–20H2O gases at 650 °C10.1016/j.corsci.2015.08.012 ↗
40. Determination of diffusion coefficient of oxygen in α-iron from internal oxidation measurements in Fe-Si alloys10.1007/BF00547959 ↗
41. Diffusion of Chromium in α-Iron10.1002/pssa.2210900219 ↗
42. A high-resolution study of the different surface state effects on the corrosion behaviors of a ferritic steel and an austenitic steel in supercritical water10.1016/j.corsci.2022.110757 ↗
43. Diffusion of Si in Fe-Si Containing 8 to 11 at% Si10.1002/pssa.2210140218 ↗
44. Bocquet · 1996 · 536
45. The diffusion of Fe3+ in amorphous SiO2 and the protective properties of SiO2 layers10.1016/0010-938X(81)90063-9 ↗
46. Study of Fe diffusion in Cr2O3 by secondary ion mass spectrometry10.4028/www.scientific.net/DDF.237-240.940 ↗
47. Diffusion Rates of 51Cr, 54Mn and 59Fe in MnCr2O4 and FeCr2O4 Spinels10.4028/www.scientific.net/AST.46.27 ↗
48. Effects of Si, Mn on the corrosion behavior of ferritic–martensitic steels in supercritical water (SCW) environments10.1016/j.corsci.2020.108432 ↗
49. Carburization behaviour of Mn–Cr–O spinel in high temperature hydrocarbon cracking environment10.1016/j.corsci.2009.06.006 ↗
50. Stability of MnCr2O4 spinel and Cr2O3 in high temperature carbonaceous environments with varied oxygen partial pressures10.1016/j.corsci.2010.02.040 ↗