journal article·2023-08Open access

Stability of Cr oxide formed on Fe-20Cr-2Si alloy in 1200 °C steam or oxygen

Joonho Moon, Sungyu Kim, Michael P. Short, Ji Hyun Kim, Chi Bum Bahn

Corrosion Science· Volume 220

Abstract

Fe-20Cr-2Si alloy, proposed as a high-temperature oxidation barrier for accident-tolerant fuel cladding in light water reactors, maintained oxidation resistance at 1200 degrees C under Ar-50%H2O and Ar-20%O2 environments for up to 24 h. However, Cr2O3 on the Fe-20Cr-2Si alloy volatilized above 1000 degrees C, degradation started under Ar20%O2, and voids were observed at the metal/oxide interface. These were attributed to the copious formation of volatile species owing to the high oxygen partial pressure in Ar-20%O2. Thus, more vacancies were generated and moved to the metal/oxide interface. Contrastingly, degradation was not initiated under Ar-50%H2O, indicating sufficient resistance of Fe-20Cr-2Si to highly oxidizing environments.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Nuclear Engineering Thermal-Hydraulics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Accident Tolerant Fuel Concepts for Light Water Reactors, INTERNATIONAL ATOMIC ENERGY AGENCY, Vienna, 2016. 〈https://www.iaea.org/publications/10972/accident-tolerant-fuel-concepts-for-light-water-reactors〉.
2. 2018
3. Commission Delegated Regulation (EU) 2022/1214 of 9 March 2022 amending Delegated Regulation (EU) 2021/2139 as regards economic activities in certain energy sectors and Delegated Regulation (EU) 2021/2178 as regards specific public disclosures for those economic activities (Text with EEA relevance), 2022. http://data.europa.eu/eli/reg_del/2022/1214/oj/eng (accessed September 22, 2022).
4. Review on chromium coated zirconium alloy accident tolerant fuel cladding10.1016/j.jallcom.2021.162450 ↗
5. K.G. Field, M.A. Snead, Y. Yamamoto, K.A. Terrani, Handbook on the Material Properties of FeCrAl Alloys for Nuclear Power Production Applications (FY18 Version: Revision 1), 2018. https://doi.org/10.2172/1474581.10.2172/1474581 ↗
6. Improving Accident Tolerance of Nuclear Fuel with Coated Mo-alloy Cladding10.1016/j.net.2015.12.003 ↗
7. M.A. Snead, Y. Katoh, T. Koyanagi, G.P. Singh, SiC/SiC Cladding Materials Properties Handbook, 2017. https://doi.org/10.2172/1399957.10.2172/1399957 ↗
8. Initial oxidation behavior of Fe-Cr-Si alloys in 1200 °C steam10.1016/j.jnucmat.2018.10.010 ↗
9. M.P. Short, S. McAlpine, M. Tonks, A. Rezwan, J. Zhang, A. Leong, Y. Xie, J. Rausch, J. Salkin, M. Bachav, U. Ehrnstén, S. Penttilä, S. Peltonen, P. Nevasmaa, R. Pohja, H. Hänninen, T. Sarikka, R. Qiang, NEUP Final Report: Multilayer Composite Fuel Cladding and Core Internals for LWR Performance Enhancement and Severe Accident Tolerance, United States, 2019. doi: 10.2172/1572872.10.2172/1572872 ↗
10. Analysis of cracking during hot isostatic pressing of a multi-metallic layered composite nuclear fuel cladding mother tube10.3795/KSME-A.2021.45.12.1057 ↗
11. Accident-tolerant fuel valuation: safety and economic benefits (Revision 1)
12. Oxidation behavior of Fe-Cr-2Si alloys in high temperature steam10.1016/j.corsci.2020.109114 ↗
13. The volatilization of chromium oxide10.1149/1.2428106 ↗
14. Oxidation/vaporization kinetics of Cr2O310.1111/j.1151-2916.1971.tb12225.x ↗
15. Kinetics of high temperature oxidation and chromia volatilization for a binary Ni–Cr Alloy10.1007/s11085-005-6562-8 ↗
16. On the oxidation and nitridation of chromium at 1300 °C10.1007/s11085-010-9198-2 ↗
17. Oxidation behavior of Cr-coated zirconium alloy cladding in high-temperature steam above 1200 °C10.1038/s41529-021-00155-8 ↗
18. Microstructure evolution and adhesion properties of thick Cr coatings under different thermal shock temperatures10.1016/j.surfcoat.2021.127224 ↗
19. 2017
20. 2014
21. Morphology of oxide scales formed on chromium-silicon alloys at high temperatures10.1016/j.corsci.2020.109023 ↗
22. Corrosion resistance of alloys F91 and Fe–12Cr–2Si in lead–bismuth eutectic up to 715°C10.1016/j.jnucmat.2012.11.010 ↗
23. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
24. Effect of alloy grain size and silicon content on the oxidation of austenitic Fe-Cr-Ni-Mn-Si alloys in pure O210.1007/BF00662967 ↗
25. Comparison of the effects of small additions of silicon or aluminum on the oxidation of iron-chromium alloys10.1007/BF00666463 ↗
26. Development of alumina-forming duplex stainless steels as accident-tolerant fuel cladding materials for light water reactors10.1016/j.jnucmat.2018.04.027 ↗
27. Mechanism of the transition from external oxide scales to internal oxidation for Fe-Si alloys in the atmosphere with very low oxygen partial pressure
28. Calculation of reactive-evaporation Rates of Chromia10.1007/s11085-008-9091-4 ↗
29. Volatility of common protective oxides in high-temperature water vapor: current understanding and unanswered questions10.4028/www.scientific.net/MSF.461-464.765 ↗
30. Predicting oxide stability in high-temperature water vapor10.1007/s11837-006-0063-3 ↗
31. Evaporation of Cr2O3 in atmospheres containing H2O10.1023/A:1023671206976 ↗
32. Thermocenter of the Russian Academy of Sciences
33. Roine · 2002 · 5 · 11
34. Chromium vaporization from high-temperature alloys10.1149/1.2434690 ↗
35. Determination of chromium vaporization rates of different interconnect alloys by transpiration experiments
36. Thermodynamics of gas phase chromium species: the chromium oxides, the chromium oxyhydroxides, and volatility calculations in waste incineration processes10.1016/0010-2180(93)90087-J ↗
37. Aaltonen · 1997
38. The effect of water-vapor content and gas flow rate on the oxidation mechanism of a 10%cr-ferritic steel in Ar-H2O mixtures10.1007/s11085-005-4394-1 ↗
39. Effects of water vapour on isothermal oxidation of chromia-forming alloys in Ar/O2 and Ar/H2 atmospheres10.1016/j.corsci.2009.08.032 ↗
40. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr Alloys10.1149/1.2424115 ↗
41. Kinetic analysis of high‐temperature oxidation of metals accompanied by scale volatilization10.1149/1.1392534 ↗
42. Factors affecting isothermal oxidation of pure chromium in air10.1016/j.corsci.2017.11.006 ↗
43. The effect of temperature on chromium vaporization and oxide scale growth on interconnect steels for solid oxide fuel cells10.1016/j.jpowsour.2015.04.040 ↗
44. Chromia evaporation in advanced ultra-supercritical steam boilers and turbines
45. Effect of water vapour on growth and adherence of chromia scales formed on Cr in high and low pO 2 -environments at 1000 and 1050°C10.3184/096034005782744443 ↗
46. Paralinear oxidation of chromium in O2 + H2O environment at 600–700 °C10.1007/s11085-008-9114-1 ↗
47. The oxidation of lithided chromium10.1149/1.2411050 ↗
48. High-temperature oxidation of Fe-Cr base alloys with particular reference to Fe-Cr-Y alloys10.1149/1.2428122 ↗
49. Scaling kinetics and scale microstructure of chromia scales formed on ni-25%cr model alloy during oxidation in H2o-containing high and low pO2 test gas at 1000°C10.1149/06618.0001ecst ↗
50. High temperature oxidation and microstructural evolution of cold spray chromium coatings on Zircaloy-4 in steam environments10.1016/j.jnucmat.2019.151737 ↗
51. Role of water vapor in chromia-scale growth at low oxygen partial pressure10.1023/A:1023040010859 ↗
52. Kinetics of the oxidation of chromium10.1149/1.2428576 ↗
53. Challenges in developing oxidation-resistant chromium-based alloys for applications above 900°C10.1007/s11837-016-2079-7 ↗
54. Chromium transport through Cr2O3 scales. II. Changes in scale morphology during high vacuum treatment of oxidized chromium specimens10.1007/BF00738382 ↗
55. Microstructure, adhesion and growth kinetics of protective scales on metals and alloys10.1007/BF00656571 ↗
56. Effect of oxide grain structure on the high-temperature oxidation of Cr10.1007/BF00611694 ↗
57. Oxidation kinetics of chromium and morphological phenomena10.1007/BF00665448 ↗
58. Material selection for accident tolerant fuel cladding
59. Birks · 2006
60. Jones · 1995