Abstract

Abstract The SiO2-Ta2O5 binary scales with different Ta2O5 contents were prepared on MoSi2-based ceramics by pre-oxidation. Hot corrosion with Na2SO4 was carried out at 1000 °C for 8 h. The pre-oxidized SiO2-Ta2O5 scale on ceramics with 10 % Ta2O5 has an excellent hot corrosion resistance. Ta2O5 reacted preferentially with Na2SO4 forming solid sodium tantalates to retard the dissolution of SiO2. A dense reaction layer can be formed to prevent the further infiltration of Na2SO4. Compared to the pure SiO2 scale without Ta2O5, fewer Na2MoO4 and no obvious corrosion hole can be observed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. A MoSi2-based composite coating by supersonic atmospheric plasma spraying to protect Nb alloy against oxidation at 1500 °C10.1016/j.surfcoat.2018.07.091 ↗
2. A long-term ultrahigh temperature application of layered silicide coated Nb alloy in air10.1016/j.apsusc.2018.01.114 ↗
3. Effect of mullite on the microstructure and oxidation behavior of thermal-sprayed MoSi2 coating at 1500 °C
4. Isothermal oxidation and interdiffusion behavior of MoSi2/WSi2 compound coating on Nb-Ti-Si based alloy10.1016/j.apsusc.2019.144477 ↗
5. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
6. Comparison investigation of hot corrosion exposed to Na2SO4 salt and oxidation of MoSi2-based coating on Nb alloy at 1000 °C10.1016/j.surfcoat.2020.125388 ↗
7. Hot corrosion behavior of calcium magnesium aluminosilicate (CMAS) on the Yb2SiO5-8YSZ composite as a candidate for environmental barrier coatings10.1016/j.matchemphys.2019.122596 ↗
8. Atypical decomposition processes of Sm2Zr2O7+8YSZ dual-phase TBCs during hot corrosion10.1016/j.corsci.2020.108681 ↗
9. Microstructural evolution and hot corrosion behavior of La0.8Ba0.2TiO3-delta-YSZ double-layer thermal barrier coatings in Na2SO4 + V2O5 molten salt at 900 °C10.1016/j.surfcoat.2020.126175 ↗
10. Improved hot corrosion resistance of plasma sprayed YSZ/Gd2Zr2O7 thermal barrier coating over single layer YSZ10.1016/j.matchar.2018.11.007 ↗
11. Hot corrosion of Mo-Si-B coatings10.1007/s11085-017-9773-x ↗
12. Resistance of a Mo-Si-B-based boating to environmental salt-based hot corrosion10.1007/s11085-020-09961-y ↗
13. Effect of SiO2 barrier scale prepared by pre-oxidation on hot corrosion behavior of MoSi2-based coating on Nb alloy10.1016/j.corsci.2020.109051 ↗
14. Hot corrosion behavior of TiO2 doped, Yb2O3 stabilized zirconia exposed to V2O5 + Na2SO4 molten salt at 700-1000 °C10.1016/j.ceramint.2017.09.167 ↗
15. Hot corrosion behavior of nanostructured Gd2O3 doped YSZ thermal barrier coating in presence of Na2SO4 + V2O5 molten salts10.1016/j.pnsc.2017.06.010 ↗
16. Hot-corrosion resistance and phase stability of Yb2O3-Gd2O3-Y2O3 costabilized zirconia-based thermal barrier coatings against Na2SO4 + V2O5 molten salts10.1016/j.surfcoat.2020.126197 ↗
17. Microstructure modification of Y2O3 stabilized ZrO2 thermal barrier coatings by laser glazing and the effects on the hot corrosion resistance10.1007/s40145-020-0363-z ↗
18. Evolution of hot corrosion behavior of YSZ-Ta2O5 composites with different YSZ/Ta2O5 ratios10.1111/ijac.12224 ↗
19. Phase stability and hot corrosion behavior of ZrO2–Ta2O5 compound in Na2SO4-V2O5 mixtures at elevated temperatures10.1016/j.ceramint.2013.08.062 ↗
20. An investigation on hot corrosion behavior of YSZ-Ta2O5 in Na2SO4+V2O5 salt at 1100 °C10.1016/j.corsci.2013.06.025 ↗
21. The hot corrosion resistance of 20 mol% YTaO4 stabilized tetragonal zirconia and 14 mol% Ta2O5 stabilized orthorhombic zirconia for thermal barrier coating applications10.1016/S0257-8972(02)00393-6 ↗
22. Interactions of Ta2O5 with water vapor at elevated temperatures10.1111/jace.14796 ↗
23. Tantalum oxide coatings as candidate environmental barriers10.1007/s11666-004-0049-z ↗
24. Effects of temperature and reagent concentration on the morphology of chemically vapor deposited β-Ta2O510.1111/j.1151-2916.1995.tb08485.x ↗
25. Na2SO4-induced corrosion of Si3N4 coated with chemically vapor deposited Ta2O510.1111/j.1151-2916.1995.tb08911.x ↗
26. Role of tantalum in the hot corrosion of a Ni-base single crystal superalloy10.1016/j.corsci.2015.05.066 ↗
27. Chemical reactions involved in the initiation of hot corrosion of B-1900 and Nasa-Trw Via10.1149/1.2123928 ↗
28. Mechanism of beneficial effect of tantalum in hot corrosion of nickel-base superalloys10.1149/1.2133502 ↗
29. Phase relations in the system CaO-Ta2O5-SiO210.1111/j.1151-2916.1969.tb11968.x ↗
30. Phase relations in the Ta2O5-WO3-SiO2 system10.1016/j.ijrmhm.2017.01.004 ↗
31. Crystal structure of high temperature form of Ta2O510.1016/0022-4596(71)90018-1 ↗
32. Constructing self-healing ZrSi2-MoSi2 coating for C/C composites with enhanced oxidation protective ability10.1016/j.surfcoat.2018.05.002 ↗
33. Growth of Na2Ta4O11 crystals from a Na2Mo2O7 flux10.1021/cg050291t ↗