journal article·2014-03

High temperature corrosion behavior of Cu–20Co–30Cr alloys with different grain size

Z.Q. Cao, H.J. Sun, J. Lu, K. Zhang, Y. Sun

Corrosion Science· Volume 80
Publisher page

Abstract

Abstract The corrosion behavior of Cu–20Co–30Cr alloys with different grain size was investigated at 700–900 °C in 0.1 MPa pure oxygen. The corrosion rates of fine-grained MACu–20Co–30Cr alloy are significantly lower than those of coarse-grained PMCu–20Co–30Cr alloy. PMCu–20Co–30Cr alloy forms the external scales of Cu oxides followed by an internal oxidation region containing alloy and a mixture of Cu, Co and Cr oxides as well as their complex oxides. MACu–20Co–30Cr alloy forms the continuous scales of chromia and a Cr-depleted layer occurs beneath the scales. The grain refinement is helpful to form the continuous scales of chromia in a Cu–Co–Cr alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Kofstad · 1988
2. Sims · 1987
3. Types of reaction in the oxidation of alloys
4. Effect of an Al2O3 coating on the oxidation process of a γ-TiAl phase based alloy10.1016/j.corsci.2012.06.009 ↗
5. Predicting the depletion of chromium in two high temperature Ni alloys10.1016/j.corsci.2012.11.040 ↗
6. The high-temperature oxidation of bulk nanocrystalline 304 stainless steel in air10.1016/j.corsci.2013.03.008 ↗
7. High temperature oxidation of γ/γ′-strengthened Co-base superalloys10.1016/j.corsci.2011.02.033 ↗
8. Oxidation kinetics of a Ni–Cu based cermet at high temperature10.1016/j.corsci.2012.11.007 ↗
9. Experimental and numerical study of the effects of a nanocrystallisation treatment on high-temperature oxidation of a zirconium alloy10.1016/j.corsci.2012.03.033 ↗
10. The possible scaling modes in the high-temperature oxidation of two-phase binary alloys. Part II: High oxidant pressures10.1007/BF01046758 ↗
11. The air oxidation of two-phase Co–Cu alloys at 600–800°C10.1016/S0010-938X(99)00115-8 ↗
12. The air oxidation of two-phase Cu–Cr alloys at 700–900°C10.1007/BF02153456 ↗
13. Microstructual effects on the high temperature oxidation of two-phase Cu–Cr alloys in 1 atm O210.1016/S0010-938X(02)00141-5 ↗
14. Anomalous behavior of the internal oxidation of dilute Cu–Ni alloys under 1atm O2 at 900°C10.1007/s11085-011-9232-z ↗
15. High temperature scaling of two-phase Fe–Cu alloys under low oxygen pressure10.1016/S0010-938X(99)00051-7 ↗
16. Transitions between different oxidation modes of binary Cu–Zn alloys in 0.1MPa O2 at 1073K10.1007/s11085-008-9098-x ↗
17. Criteria for the formation of protective Al2O3 scales on Fe–Al and Fe–Cr–Al alloys10.1016/j.corsci.2005.01.012 ↗
18. The third-element effect in the oxidation of Ni–xCr–7Al (x=0, 5, 10, 15at.%) alloys in 1 atm O2 at 900–1000°C10.1016/j.corsci.2006.03.008 ↗
19. The internal oxidation of ternary alloys. VIII: the transition from the internal to the external oxidation of the two most-reactive components under high-oxidant pressures10.1007/s11085-006-9022-1 ↗
20. High temperature scaling of Ni–xSi–10at.% Al alloys in 1atm of pure O210.1016/j.corsci.2006.08.011 ↗
21. High-temperature scaling of Cu–Al and Cu–Cr–Al alloys. An example of a non-classical third-element effect10.1007/s11085-006-9012-3 ↗
22. The nature of the third-element effect in the oxidation of Fe–xCr–3at.% Al alloys in 1 atm O2 at 1000°C10.1016/j.corsci.2007.06.019 ↗
23. The effect of Si additions on the high temperature oxidation of a ternary Ni–10Cr–4Al alloy in 1atm O2 at 1100°C10.1016/j.corsci.2008.10.023 ↗
24. The oxidation of two ternary Cu–Ni–Cr alloys at 700–800°C under high oxygen pressures10.1023/A:1010376812471 ↗
25. Oxidation of the three-phase alloy Cu–Ni–20Cr at 973–1073K in 101kPa O210.1515/HTMP.2001.20.5-6.377 ↗
26. Oxidation of two three-phase Cu–30Ni–Cr lloys at 700–800°C in 1atm of pure oxygen10.1016/j.msea.2006.03.052 ↗
27. Villars · 1997
28. On the role of dislocations in bulk diffusion10.1016/0001-6160(57)90127-X ↗
29. K. Kosuge, Nagai, in: Proceedings of 2000 powder metallurgy world Congress, Japan Society of Powder and Powder Metallurgy, Kyoto, 2000.
30. Nanocrystalline materials10.1016/0921-5093(89)90083-X ↗