Abstract

The effect of tantalum addition on corrosion resistance in HAZ of duplex stainless steel was investigated by pitting corrosion test and material characterizations (SEM, TEM, APT). The Ta addition improved corrosion resistance of HAZ simulating welding at low heat input and rapid cooling rate since Ta segregated in the Cr nitrides and suppressed formation of Cr-depleted zone. The Ta addition also improved corrosion resistance in HAZ subjected to isothermal aging heat treatment assuming welding at high heat input and low cooling rate because Ta promotes the formation of χ phase and delays the formation of σ phase and Cr-depleted zone.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. Super duplex stainless steels10.1179/mst.1992.8.8.685 ↗
2. Super duplex stainless steel tubular “DP-3W”
3. Stainless steel in construction: a review of research, applications, challenges and opportunities10.1016/j.jcsr.2008.07.011 ↗
4. J.-O. Nilsson, G. Chai, The physical metallurgy of duplex stainless steels, in: Proceedings of the International Conference & Expo DUPLEX Associazione Italiana Di Metallurgia-AIM, Grado, Italy (2007).
5. Influence of isothermal phase transformations on toughness and pitting corrosion of super duplex stainless steel SAF 250710.1179/mst.1993.9.7.545 ↗
6. Recent development of welding consumables for Ni-base alloys and stainless steel
7. Duplex – a new generation of stainless steels for desalination plants10.1016/j.desal.2006.02.051 ↗
8. Hyper duplex stainless steel for deep subsea applications
9. Effect of prolonged thermal cycles on the pitting corrosion resistance of a newly developed LDX 2404 lean duplex stainless steel10.1016/j.corsci.2015.11.018 ↗
10. Duplex steels used in building structures and their resistance to chloride corrosion10.3390/ma14195666 ↗
11. Precipitation behavior of σ phase in a duplex phase stainless steel10.2355/tetsutohagane1955.67.3_577 ↗
12. Depletion effects at phase boundaries in 2205 duplex stainless steel characterized with SKPFM and TEM/EDS10.1016/j.corsci.2009.05.012 ↗
13. Microstructural evolution and localized corrosion resistance of an aged superduplex stainless steel10.1016/j.corsci.2003.09.024 ↗
14. Evaluation of localized corrosion in duplex stainless steel aged at 850 ◦C with critical pitting temperature measurement10.1016/j.electacta.2008.11.038 ↗
15. Characterisation of duplex stainless steel subjected to long-term annealing in the sigma phase formation temperature range by the DLEPR test10.1016/j.corsci.2011.07.013 ↗
16. Effects of sigma (σ) phase on the pitting corrosion of 25% Cr duplex stainless steel; investigations by means of electrochemical noise measurement
17. Effects of sigma phase precipitation on seawater pitting of duplex stainless steel10.1016/j.desal.2006.05.021 ↗
18. Pitting evolution of hyper duplex stainless steel 2707 at nose temperature by electrochemical tests and developed mixed potential model10.1016/j.corsci.2022.110759 ↗
19. The influence of aging on the intergranular corrosion of 22 chronium-5 nickel duplex stainless steel10.1016/0010-938X(94)00120-U ↗
20. Effects of alloying elements on sigma phase precipitation in duplex stainless steel (1) -modelling of effects of chrovmium, molybdenum and tungsten on sigma phase growth rate in super duplex stainless steel10.2355/isijinternational.ISIJINT-2018-477 ↗
21. The effect of large heat input on the microstructure and corrosion behaviour of simulated heat affected zone in 2205 duplex stainless steel10.1016/j.corsci.2011.07.022 ↗
22. Microstructure and pitting corrosion in simulated heat affected zones of duplex stainless steels10.1016/S0254-0584(01)00409-6 ↗
23. Study of nobility of chromium nitrides in isothermally aged duplex stainless steels by using SKPFM and SEM/EDS10.1016/j.corsci.2009.08.057 ↗
24. Microstructure and corrosion studies on different zones of super duplex stainless steel UNS S32750 weldment10.3389/fmats.2020.00251 ↗
25. Influence of cooling rate on microstructure evolution and pitting corrosion resistance in the simulated heat affected zone of 2304 duplex stainless steels10.1016/j.corsci.2012.01.018 ↗
26. Influence of welding thermal cycles on microstructure and pitting corrosion resistance of 2304 duplex stainless steels10.1016/j.corsci.2011.10.039 ↗
27. Pitting and crevice corrosion behavior of the duplex stainless steel UNS S32205 welded by using the GTAW process10.1590/1980-5373-mr-2022-0179 ↗
28. Welding consumables for super duplex stainless steel10.2207/jjws.80.142 ↗
29. Effect of heat treatment atmospheres on microstructure evolution and corrosion resistance of 2205 duplex stainless steel weldments
30. Modeling of effects of temperature and alloying elements on sigma phase precipitation rate in duplex stainless steel -(Effects of alloying elements on sigma phase precipitation in duplex stainless steel)10.2207/qjjws.33.55 ↗
31. HAZ toughness of high silicon containing duplex stainless steel -study on welding of high silicon containing stainless steels (II)-10.2207/qjjws.9.269 ↗
32. Effect of tungsten on the pitting and crevice corrosion resistance of type 25Cr super duplex stainless steels10.5006/2185 ↗
33. Effect of Cu addition on phase fraction, mechanical properties and corrosion properties of Fe-Cr-Mn-Al duplex stainless steel10.1016/j.msea.2022.144095 ↗
34. Effects of cooling time and alloying elements on the microstructure of the Gleeble-simulated heat affected zone of 22% Cr duplex stainless steels10.1361/105994901770344665 ↗
35. Effects of nitrogen in shielding gas on microstructure evolution and localized corrosion behavior of duplex stainless steel welding joint10.1016/j.apsusc.2017.01.252 ↗
36. Effects of solution heat-treatment and nitrogen in shielding gas on the resistance to pitting corrosion of hyper duplex stainless steel welds10.1016/j.corsci.2011.02.013 ↗
37. Properties of the heat affected zone of welded joints in lean duplex stainless steels10.2207/jjws.82.435 ↗
38. Y. Oikawa, H. Urashima, S. Tsuge, H. Inoue, R. Matsuhashi, Low-alloy duplex stainless steel wherein heat-affected zone have good corrosion resistance and toughness, Patent No. EP2258885A1.
39. Initiation of pitting at sulfide inclusions in stainless steel10.1149/1.2401840 ↗
40. A new microelectrochemical method to study pit initiation on stainless steels10.1016/S0013-4686(70)01783-8 ↗
41. Microelectrochemical measurements of the dissolution of single MnS inclusions, and the prediction of the critical conditions for pit initiation on stainless steel10.1149/1.1360205 ↗
42. Microelectrochemical measurements of dissolution of MnS inclusions and morphological observation of metastable and stable pitting on stainless steel10.1149/1.2745639 ↗
43. Pit initiation mechanism at MnS inclusions in stainless steel: synergistic effect of elemental sulfur and chloride ions10.1149/2.081310jes ↗
44. Effect of tantalum addition on pitting corrosion behavior of super duplex stainless steels - development of high corrosion resistant duplex stainless steels by inclusion control (1)10.3323/jcorr.64.320 ↗
45. Effect of amount of tantalum on corrosion behavior of high corrosion resistant standard duplex stainless steels - development of high corrosion resistant duplex stainless steels by inclusion control (2)10.3323/jcorr.64.324 ↗
46. Effect of tantalum addition on crevice corrosion of super duplex stainless steels10.3323/jcorr.64.497 ↗
47. Pitting corrosion resistance of Ta-bearing duplex stainless steel10.2320/matertrans.C-M2021835 ↗
48. Influence of sulfur content on the pitting corrosion behavior of the surface and the cross section of type 304 stainless steel plate10.3323/jcorr.62.259 ↗
49. Cerium addition to CaS inclusions in stainless steel: insolubilizing water-soluble inclusions and improving pitting corrosion resistance10.1016/j.corsci.2020.109222 ↗
50. Identification of MnCr2O4 nano-octahedron in catalysing pitting corrosion of austenitic stainless steels10.1016/j.actamat.2010.05.043 ↗
51. Mechanism of (Mg, Al, Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
52. Effects of non-metallic inclusions on the initiation of pitting corrosion in 11% Cr ferritic stainless steel examined by micro-droplet cell10.1016/j.corsci.2006.08.017 ↗
53. The initiation of pitting corrosion of stainless steels at oxide inclusions10.1016/0010-938X(92)90137-R ↗
54. SCC and crevice corrosion resistances of stainless steel modified with tantalum addition10.3327/taesj.J18.036 ↗
55. Effect of Ta addition on crevice corrosion resistance for Ni based corrosion resistant alloys10.3323/jcorr.59.222 ↗
56. Effects of composition on embrittlement of austenitic stainless steels
57. Kobelco Welding Today, 13 (2020) 1–10.
58. Kawano · Zairyo-to-Kankyo · 2015 · 64 · 55210.3323/jcorr.64.552 ↗
59. Duplex Stainless Steel Processing Manual, IMOA (2009) 50.
60. Miller · 2000
61. On the nitrogen diffusion in a duplex stainless steel10.1590/1516-1439.337714 ↗
62. Nitride precipitation in weld HAZs of a duplex stainless steel10.2355/isijinternational.41.460 ↗
63. Formation of chromium nitride and intragranular austenite in a super duplex stainless steel10.1007/s11661-019-05489-2 ↗
64. Microstructural features and corrosion properties in laser welded duplex stainless steels10.2207/qjjws1943.68.475 ↗
65. Relationship between pitting corrosion resistance and Cr-depleted zone in duplex stainless steel weld metals -metallurgical study on weld metal of duplex stainless steel SUS329J1-10.2207/qjjws.39.180 ↗
66. Localized corrosion of stainless steels part 2 intergranular corrosion10.2355/tetsutohagane1955.63.5_585 ↗
67. Effects of boron, niobium and titanium on grain growth in ultra-high purity 18% Cr ferritic stainless steel10.2355/isijinternational.44.1568 ↗
68. Micro-electrochemical insights into pit initiation site on aged UNS S32750 super duplex stainless steel10.1038/s41529-023-00335-8 ↗
69. Effect of tungsten on precipitation behavior of intermetallic compound in HAZ of duplex stainless steel and its mechanism -Study on weldability of high tungsten duplex stainless steel (2)-10.2207/qjjws.14.368 ↗
70. The role of tungsten on the phase transformation kinetics and its correlation with the localized corrosion resistance of 25Cr super duplex stainless steels10.1149/1945-7111/ab90af ↗