Abstract
Effect of aging at 900 ℃ on the microstructure and pitting of HDSS 2707 was examined. The pitting resistance of HDSS 2707 decreases over the first 10 h because of the presence of the secondary precipitates, and then increases due to Cr/Mo back diffusion from the matrix into the Cr/Mo-depleted regions. Pitting nucleates around the sigma phase, and propagates within the ferrite, but is blocked by austenite . The developed Mixed Potential Model (MPM) was used to analyze the character of the barrier layer, which is in accordance with the potentiodynamic polarization experiments and morphological observation of pitting.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Understanding the relation between pitting corrosion resistance and phase fraction of S32101 duplex stainless steel10.1016/j.corsci.2019.01.001 ↗
2. Effect of Mo on interaction between α/γ phases of duplex stainless steel10.1016/j.electacta.2018.02.082 ↗
3. Passivation behavior and surface chemistry of 2507 super duplex stainless steel in artificial seawater: influence of dissolved oxygen and pH10.1016/j.corsci.2019.02.002 ↗
4. Influence of annealing treatment on the corrosion resistance of lean duplex stainless steel 210110.1016/j.electacta.2009.04.023 ↗
5. Effect of annealing temperature on the pitting corrosion resistance of super duplex stainless steel UNS S3275010.1016/j.matchar.2009.04.009 ↗
6. Effect of annealing treatment on microstructure evolution and the associated corrosion behavior of a super-duplex stainless steel10.1016/j.jallcom.2009.12.127 ↗
7. Effect of annealing temperature on pitting behavior and microstructure evolution of hyper‐duplex stainless steel 270710.1002/maco.201910801 ↗
8. Welding behaviour of duplex stainless steel AISI 2205: a review
9. Effect of a brief post-weld heat treatment on the microstructure evolution and pitting corrosion of laser beam welded UNS S31803 duplex stainless steel10.1016/j.corsci.2012.08.054 ↗
10. Influence of welding thermal cycles on microstructure and pitting corrosion resistance of 2304 duplex stainless steels10.1016/j.corsci.2011.10.039 ↗
11. Effect of post-weld heat treatment on microstructure evolution and pitting corrosion behavior of UNS S31803 duplex stainless steel welds10.1016/j.corsci.2012.04.047 ↗
12. Influence of Creq/Nieq on pitting corrosion resistance and mechanical properties of UNS S32304 duplex stainless steel welded joints10.1016/j.corsci.2013.01.037 ↗
13. Effect of thermal cycles on the corrosion and mechanical properties of UNS S31803 duplex stainless steel10.1016/j.corsci.2009.08.015 ↗
14. Determination of pitting initiation of duplex stainless steel using potentiostatic pulse technique10.1016/j.electacta.2010.02.035 ↗
15. Understanding pitting corrosion10.1016/S1369-7021(08)70206-2 ↗
16. Effect of aging on the corrosion resistance of 2101 lean duplex stainless steel10.1016/j.matchar.2009.08.009 ↗
17. Effect of prolonged thermal cycles on the pitting corrosion resistance of a newly developed LDX 2404 lean duplex stainless steel10.1016/j.corsci.2015.11.018 ↗
18. New insights into the hardening and pitting corrosion mechanisms of thermally aged duplex stainless steel at 475° C: A comparative study between 2205 and 2101 steels10.1016/j.jmst.2021.04.046 ↗
19. Evaluation of localized corrosion in duplex stainless steel aged at 850C with critical pitting temperature measurement10.1016/j.electacta.2008.11.038 ↗
20. Effect of aging on the corrosion resistance of 2209 duplex stainless steel weldments10.1007/s12540-018-0206-4 ↗
21. Effect of the heat treatment on the corrosion resistance of duplex stainless steels10.1007/s11665-018-3408-5 ↗
22. Studies on the degree of sensitization of hyper-duplex stainless steel 2707 at 900℃ using a modified DL-EPR test10.1016/j.corsci.2021.109432 ↗
23. Precipitation behavior and phase transformation of hyper duplex stainless steel UNS S32707 at nose temperature10.1016/j.matchar.2017.04.018 ↗
24. Resistance of thermally aged DSS 2304 against localized corrosion attack10.3390/met8121022 ↗
25. Effect of spinodal decomposition on the pitting corrosion resistance of Z3CN20. 09M duplex stainless steel10.1002/maco.201709738 ↗
26. Comparative studies on microstructure evolution and corrosion resistance of 304 and a newly developed high Mn and N austenitic stainless steel welded joints10.1016/j.corsci.2021.109338 ↗
27. Effect of Mo and Cr additions on the microstructure, mechanical properties and pitting corrosion resistance of austenitic Fe-30Mn-10.5 Al-1.1C lightweight steels10.1016/j.jallcom.2018.10.253 ↗
28. On the in-situ characterisation of metastable pitting using 316L stainless steel as a case study10.1016/j.corsci.2020.109004 ↗
29. Localized corrosion: passive film breakdown vs pit growth stability: Part II. A model for critical pitting temperature10.1149/2.0591809jes ↗
30. Abreu, Influence of the grain size on deleterious phase precipitation in superduplex stainless steel UNS S3275010.1016/j.matchar.2008.08.007 ↗
31. Influence of sigma-phase formation on the localized corrosion behavior of a duplex stainless steel10.1007/BF02648847 ↗
32. Mixed potential model for passivity characters of hyper-duplex stainless steel 2707 in ammonium carbonate solution containing chloride
33. Point defect model for passivity breakdown on hyper-duplex stainless steel 2707 in solutions containing bromide at different temperatures
34. Effects of temperature and pH on the electrochemical behaviour of alloy 600 in simulated pressurized water reactor primary water10.1016/j.jnucmat.2019.151850 ↗
35. The electrochemical properties of alloy 690 in simulated pressurized water reactor primary water: Effect of temperature10.1016/j.jnucmat.2019.03.016 ↗
36. Effect of temperature on corrosion of carbon steel in simulated concrete pore solution under anoxic conditions10.1016/j.corsci.2020.108886 ↗
37. On the impedance plane displays for irreversible electrode reactions based on the stability conditions of the steady-state—I. One state variable besides electrode potential10.1016/0013-4686(90)90077-D ↗
38. Quantitative study of the corrosion evolution and stress corrosion cracking of high strength aluminum alloys in solution and thin electrolyte layer containing Cl10.1016/j.corsci.2020.109076 ↗
39. Application of potentiostatic pulse technique and statistical analysis in evaluating pitting resistance of aged 317L stainless steel10.1002/maco.201810622 ↗
40. The kinetics of nucleation of metastable pits on metal surfaces: the point defect model and its optimization on data obtained on stainless steel, carbon steel, iron, aluminum and Alloy-2210.1149/2.0401605jes ↗
41. Monte-Carlo simulation of pitting corrosion with a deterministic model for repassivation10.1149/1945-7111/ab67a0 ↗
42. Point defect model for passivity breakdown on hyper-duplex stainless steel 2707 in solutions containing bromide at different temperatures
43. Pitting of carbon steel in the synthetic concrete pore solution10.1002/maco.202011875 ↗
44. Unification of the deterministic and statistical approaches for predicting localized corrosion damage. I. Theoretical foundation10.1016/j.corsci.2004.03.014 ↗
45. Exploration of the effect of chloride ion concentration and temperature on pitting corrosion of carbon steel in saturated Ca (OH) 2 solution10.1016/j.corsci.2015.06.010 ↗
46. Effects of copper addition on the formation of inclusions and the resistance to pitting corrosion of high performance duplex stainless steels10.1016/j.corsci.2011.01.005 ↗
47. The metastable pitting corrosion of 2205 duplex stainless steel under bending deformation, J10.1016/j.jallcom.2020.154422 ↗
48. Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method10.1016/j.corsci.2012.11.024 ↗
49. Correlation between critical pitting temperature and degree of sensitisation on alloy 2205 duplex stainless steel10.1016/j.corsci.2010.10.009 ↗
50. Evaluation of selective corrosion in UNS S31803 duplex stainless steel with electrochemical impedance spectroscopy10.1016/j.electacta.2005.02.105 ↗
51. Pitting corrosion of metals: a review of the critical factors10.1149/1.1838615 ↗
52. Perspective—localized corrosion: passive film breakdown vs pit growth stability10.1149/2.1381704jes ↗
53. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
54. The point defect model for the passive state10.1149/1.2069096 ↗
55. Metastable pitting of stainless steel
56. Pit growth studies in stainless steel foils. I. Introduction and pit growth kinetics10.1016/S0010-938X(01)00133-0 ↗
57. Perforated covers for propagating pits10.1149/1.1838423 ↗
58. Effect of sigma phase precipitation on the pitting corrosion mechanism of duplex stainless steels10.20964/2018.10.38 ↗