journal article·2024-11

Advancing the hydrogen tolerance of ultrastrong aluminum alloys via nanoprecipitate modification

Yafei Wang, Jianwei Tang, Hiro Fujihara, Nozomu Adachi, Yoshikazu Todaka, Yuantao Xu, Mainak Saha, Taisuke Sasaki, Kazuyuki Shimizu, Kyosuke Hirayama, Akihisa Takeuchi, Masayuki Uesugi, Hiroyuki Toda

Corrosion Science· Volume 240
Publisher page

Abstract

Ultrastrong metallic alloys, possessing unparalleled load-bearing abilities, are coveted in many sectors, thus attracting growing research efforts. However, these alloys encounter persistent usability challenges posed by hydrogen embrittlement, which causes unpredictable fracture through crack initiation. Due to complex hydrogen-microstructure interactions and their exacerbation under high stress, advances in hydrogen resistance in ultrastrong materials are sparse throughout their long history. Herein, we report a quantum-mechanics-informed strategy for hydrogen tolerance enhancement in ultrafine-grain-hardened Al-Zn-Mg-Cu alloys, approaching their current strength limit of approximately 1 GPa. This method involves the incorporation of hydrogen-absorbing T-phase precipitates into nanograins, to substantially reduce hydrogen coverage at potential crack initiation sites. We demonstrate, via synchrotron radiation X-ray micro-/nano-tomography, scanning transmission electron microscopy and atom probe tomography, that nanoprecipitates successfully withstand shear strains exceeding 1000 and are exploitable essentials for ultra strength-hydrogen synergy, contrasting their often-assumed secondary roles in nanocrystalline alloys due to possible strain-induced dissolution, which has intuitively excluded exploring them as central elements. Our approach potentially inspires new hydrogen-resisting alloys across a broad strength-composition space.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
2. II. On some remarkable changes produced in iron and steel by the action of hydrogen and acids10.1098/rspl.1874.0024 ↗
3. Generalised boundary conditions for hydrogen transport at crack tips10.1016/j.corsci.2020.108698 ↗
4. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
5. Hydrogen embrittlement mechanisms in advanced high strength steel10.1016/j.actamat.2021.117488 ↗
6. Microstructure and defect effects on strength and hydrogen embrittlement of high-entropy alloy CrMnFeCoNi processed by high-pressure torsion10.1016/j.msea.2022.143179 ↗
7. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
8. Quantitative tests revealing hydrogen-enhanced dislocation motion in α-iron
9. Hydrogen embrittlement of aluminum: the crucial role of vacancies10.1103/PhysRevLett.94.155501 ↗
10. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: Overview10.1016/j.actamat.2018.12.013 ↗
11. A decohesion pathway for hydrogen embrittlement in nickel: Mechanism and quantitative prediction10.1016/j.actamat.2019.11.062 ↗
12. Hydrogen-accelerated spontaneous microcracking in high-strength aluminium alloys10.1038/s41598-020-58834-6 ↗
13. Hydrogen induced fast-fracture10.1016/j.jmps.2019.103740 ↗
14. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
15. Hydrogen embrittlement of aluminum and aluminum-based alloys
16. Hydrogen microprint technique in the study of hydrogen in steels10.1007/BF00556094 ↗
17. The first direct observation of hydrogen trapping sites in TiC precipitation-hardening steel through atom probe tomography10.1016/j.scriptamat.2010.03.012 ↗
18. Hydrogen trapped at intermetallic particles in aluminum alloy 6061-T6 exposed to high-pressure hydrogen gas and the reason for high resistance against hydrogen embrittlement10.1016/j.ijhydene.2017.08.035 ↗
19. P.M. Ordin, Safety standard for hydrogen and hydrogen systems guidelines for hydrogen system design, materials selection, operations, storage and transportation, (1997).
20. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
21. First-principles study of hydrogen diffusion in α− Al2O3 and liquid alumina10.1103/PhysRevB.69.024302 ↗
22. The diffusion and trapping of hydrogen in high purity aluminum10.1016/S1359-6454(98)00333-4 ↗
23. The effect of hydrogen atoms on the screw dislocation mobility in bcc iron: A first-principles study10.1016/j.actamat.2013.07.064 ↗
24. First-principles calculation of multiple hydrogen segregation along aluminum grain boundaries10.1016/j.commatsci.2018.10.015 ↗
25. Suppressed hydrogen embrittlement of high-strength Al alloys by Mn-rich intermetallic compound particles10.1016/j.actamat.2022.118110 ↗
26. Hydrogen trapping in Mg2Si and Al7FeCu2 intermetallic compounds in aluminum alloy: first-principles calculations10.2320/matertrans.MT-M2020201 ↗
27. Equilibrium and kinetic studies of the hydrogen-assisted cracking of steel10.1016/0001-6160(77)90126-2 ↗
28. Assessment of hydrogen embrittlement via image-based techniques in Al–Zn–Mg–Cu aluminum alloys10.1016/j.actamat.2019.06.056 ↗
29. Switching nanoprecipitates to resist hydrogen embrittlement in high-strength aluminum alloys10.1038/s41467-022-34628-4 ↗
30. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
31. Nanostructural hierarchy increases the strength of aluminium alloys10.1038/ncomms1062 ↗
32. Probing novel microstructural evolution mechanisms in aluminum alloys using 4D nanoscale characterization10.1002/adma.201703482 ↗
33. Design of hydrogen embrittlement resistant 7xxx-T6 aluminum alloys based on wire arc additive manufacturing: Changing nanochemistry of strengthening precipitates10.1016/j.matdes.2024.113030 ↗
34. Revisiting stress-corrosion cracking and hydrogen embrittlement in 7xxx-Al alloys at the near-atomic-scale10.1038/s41467-022-31964-3 ↗
35. New insights into hydrogen trapping and embrittlement in high strength aluminum alloys10.1016/j.corsci.2023.111453 ↗
36. Crack arrest markings in stress corrosion cracking of 7xxx aluminium alloys: Insights into active hydrogen embrittlement mechanisms10.1016/j.scriptamat.2023.115690 ↗
37. Effect of hydrogen accumulation on θ' precipitates on the shear strength of Al-Cu alloys10.1016/j.ijplas.2022.103475 ↗
38. Microstructure design strategies to mitigate hydrogen embrittlement in metallic materials10.1111/ffe.14074 ↗
39. Influence of equal-channel angular pressing on precipitation in an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2009.03.017 ↗
40. The effect of severe plastic deformation on precipitation in supersaturated Al–Zn–Mg alloys10.1016/j.msea.2007.01.001 ↗
41. A review on high-pressure torsion (HPT) from 1935 to 198810.1016/j.msea.2015.11.074 ↗
42. Significance of temperature increase in processing by high-pressure torsion10.1016/j.msea.2011.06.031 ↗
43. Influence of hydrogen on strain localization and fracture behavior in AlZnMgCu aluminum alloys10.1016/j.actamat.2018.08.024 ↗
44. In-situ 3D observation of hydrogen-assisted particle damage behavior in 7075 Al alloy by synchrotron X-ray tomography10.1016/j.actamat.2022.117658 ↗
45. High-energy x-ray nanotomography introducing an apodization Fresnel zone plate objective lens10.1063/5.0020293 ↗
46. Effect of hydrogen on the integrity of aluminium–oxide interface at elevated temperatures10.1038/ncomms14564 ↗
47. Multimodal assessment of mechanically induced transformation in metastable multi-phase steel using X-ray nano-tomography and pencil-beam diffraction tomography10.1016/j.actamat.2022.117956 ↗
48. The crystal structure of the metallic phase Mg32 (Al, Zn)4910.1107/S0365110X57000808 ↗
49. On the potential of aluminum crossover alloys10.1016/j.pmatsci.2021.100873 ↗
50. Prototypic lightweight alloy design for stellar-radiation environments10.1002/advs.202002397 ↗
51. The evolution of precipitates in an Al–Zn–Mg alloy10.1016/j.jmrt.2023.02.144 ↗
52. Age-hardening response of AlMgZn alloys with Cu and Ag additions10.1016/j.actamat.2020.05.066 ↗
53. Structure refinement of (Al, Zn)49Mg32-type phases by single-crystal X-ray diffraction10.1016/S0921-5093(00)01094-7 ↗
54. The crystal structure of magnesium di-zincide10.1103/PhysRev.29.34 ↗
55. Structural studies of stacking variants in Mg-base Friauf–Laves phases10.1107/S0567740880006565 ↗
56. GP-zones in Al–Zn–Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
57. Structure analysis of embedded nano-sized particles by precession electron diffraction. η′-precipitate in an Al–Zn–Mg alloy as example10.1016/j.ultramic.2006.01.009 ↗
58. PTCLab: free and open-source software for calculating phase transformation crystallography10.1107/S1600576716006075 ↗
59. The charge-density study of the Laves phases, MgZn2 and MgCu210.1107/S0108270184002791 ↗
60. Evidence for two-stage hardening in an Al-Zn-Mg-Cu alloy processed by high-pressure torsion10.1016/j.jallcom.2023.168839 ↗
61. Coupling of dislocations and precipitates: Impact on the mechanical behavior of ultrafine grained Al–Zn–Mg alloys10.1016/j.actamat.2015.09.017 ↗
62. Ultrahigh-strength low carbon steel obtained from the martensitic state via high pressure torsion10.1016/j.actamat.2018.12.028 ↗
63. On the microstructure and mechanical properties of an Fe-10Ni-7Mn martensitic steel processed by high-pressure torsion10.1016/j.msea.2019.02.002 ↗
64. Low-temperature and high-strain-rate superplasticity of ultrafine-grained A7075 processed by high-pressure torsion10.2320/matertrans.L-M2018825 ↗
65. Tensile deformation of an ultrafine-grained aluminium alloy: Micro shear banding and grain boundary sliding10.1016/j.actamat.2008.01.020 ↗
66. Effect of Mg on microstructure and mechanical properties of Al-Mg alloys produced by high pressure torsion10.1016/j.scriptamat.2018.09.033 ↗
67. Outstanding mechanical properties of high-pressure torsion processed multiscale TWIP-cored three layer steel sheet10.1016/j.scriptamat.2016.06.009 ↗
68. Microstructural evolution and mechanical properties of nanocrystalline Fe–Mn–Al–C steel processed by high-pressure torsion10.1016/j.msea.2021.142073 ↗
69. The defining role of initial microstructure and processing temperature on microstructural evolution, hardness and tensile response of Al-Mg-Sc-Zr (AA5024) alloy processed by high pressure torsion10.1016/j.jallcom.2021.163548 ↗
70. G. Shen, M. Li, J. Liu, R. Zheng, Z. Xiang, X. Ma, J. Huang, J. Li, Z. Zhou, Z. Chen, Approaching 1 GPa ultra-high tensile strength in a nanostructured Al-Zn-Mg-Cu-Zr-Sc alloy prepared by severe plastic deformation, Adv. Eng. Mater.
71. Hierarchical nanostructured aluminum alloy with ultrahigh strength and large plasticity10.1038/s41467-019-13087-4 ↗
72. High-strength nanotwinned Al alloys with 9R phase10.1002/adma.201704629 ↗
73. Atomic scale HAADF-STEM study of η′ and η1 phases in peak-aged Al–Zn–Mg alloys10.1007/s10853-017-1873-0 ↗
74. First-principles study of hydrogen segregation at the MgZn2 precipitate in Al-Mg-Zn alloys10.1016/j.commatsci.2018.03.009 ↗
75. An atomic-resolution investigation of precipitation evolution in Al-Mg-Ag alloys10.1016/j.matlet.2019.04.054 ↗
76. Dynamic precipitation, segregation and strengthening of an Al-Zn-Mg-Cu alloy (AA7075) processed by high-pressure torsion10.1016/j.actamat.2018.09.060 ↗
77. Softening of nanostructured Al–Zn and Al–Mg alloys after severe plastic deformation10.1016/j.actamat.2006.04.025 ↗
78. The development of vacancies during severe plastic deformation10.2320/matertrans.MF201937 ↗
79. An unreported precipitate orientation relationship in Al-Zn-Mg based alloys10.1016/j.matchar.2019.109958 ↗
80. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
81. Mechanisms of hydrogen-enhanced localized plasticity: an atomistic study using α-Fe as a model system10.1016/j.actamat.2014.01.008 ↗
82. Hydrogenated vacancies lock dislocations in aluminium10.1038/ncomms13341 ↗
83. Improving the hydrogen embrittlement resistance by straining the ferrite / cementite interfaces10.1016/j.actamat.2024.119850 ↗
84. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
85. Hydrogen-assisted ductile fracture in spheroidized 1518 steel10.1016/0956-7151(90)90127-3 ↗
86. Influence of nanovoids in the hydrogen embrittlement fracture of Al–Zn–Mg–Cu alloys10.1016/j.mtla.2020.100667 ↗
87. Effect of microstructure on stress corrosion cracking of an Al-Zn-Mg-Cu alloy10.1016/S0010-938X(98)00002-X ↗
88. Stress corrosion cracking in Al-Zn-Mg-Cu aluminum alloys in saline environments10.1007/s11661-012-1528-3 ↗
89. An atomic scale structural investigation of nanometre-sized η precipitates in the 7050 aluminium alloy10.1016/j.actamat.2019.05.041 ↗
90. Shearing and rotation of β″ and β′ precipitates in an Al-Mg-Si alloy under tensile deformation: In-situ and ex-situ studies10.1016/j.actamat.2021.117310 ↗
91. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗
92. Deformation of electrodeposited nanocrystalline nickel10.1016/S1359-6454(02)00421-4 ↗
93. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
94. Three-dimensional shear-strain patterns induced by high-pressure torsion and their impact on hardness evolution10.1016/j.actamat.2011.03.015 ↗
95. First-principles calculation of multiple hydrogen segregation along aluminum grain boundaries10.1016/j.commatsci.2018.10.015 ↗
96. Hydrogen-trapping energy in screw and edge dislocations in aluminum: first-principles calculations10.2320/matertrans.MT-M2020375 ↗
97. First-principles estimation of hydrogen occupancy around lattice defects in Al10.2472/jsms.59.596 ↗
98. Surface energy reduction by dissociative hydrogen adsorption on inner surface of pore in aluminum10.2464/jilm.68.588 ↗
99. First-principles calculations of hydrogen trapping energy on incoherent interfaces of aluminum alloys10.2320/matertrans.MT-M2023106 ↗
100. Precipitation kinetics in a severely plastically deformed 7075 aluminium alloy10.1016/j.actamat.2013.11.071 ↗