Oxidation behavior of Ti-Zr-Ni-Cu metallic glass
Source abstract
Abstract
Abstract Oxidation behavior during continuous heating of Ti40Zr10Ni40Cu10 metallic glass in a dry air has been studied by a combination of thermal analysis, thermogravimetric analysis (TGA) and detailed structural analysis using STEM and TEM. With increasing temperature, three different types of oxide growth took place: amorphous Ti(Zr) oxide formation with Ni enrichment beneath the oxide layer on glass substrate; Crystallization of Ni enriched amorphous layer into Ni3Ti structure, followed by oxide growth with lamellar structure consisted of Ti(Zr) amorphous oxide and Ni3Ti until crystallization of matrix; oxide growth with particulate structure in crystalline substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Phase-change materials and chalcogenides · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Capillary flow of amorphous metal for high performance electrode10.1038/srep02185 ↗
2. Bulk metallic glass: the smaller the better10.1002/adma.201002148 ↗
3. Controllable nanoimprinting of metallic glasses: effect of pressure and interfacial properties10.1088/0957-4484/24/10/105301 ↗
4. Processing of bulk metallic glass10.1002/adma.200902776 ↗
5. Thermoplastic forming of bulk metallic glass – a technology for MEMS and microstructure fabrication10.1109/JMEMS.0007.892889 ↗
6. Cyclic properties of superelastic shape memory alloy wires and bars10.1061/(ASCE)0733-9445(2004)130:1(38) ↗
7. Amorphous (Ti, Zr, Hf)-Ni-Cu ternary alloys with a wide supercooled liquid region10.1016/0921-5093(94)90877-X ↗
8. The microstructure of melt spun Ti-Zr-Cu-Zr shape memory alloys10.1016/S0254-0584(03)00026-9 ↗
9. Mechanical and corrosion properties of Ti-Ni-Cu-Zr metallic glass matrix composites10.1016/j.jallcom.2017.08.120 ↗
10. Correlation between the thermal and superelastic behavior of Ni50-xTi35Zr15Cux shape memory alloys10.1016/j.intermet.2019.01.005 ↗
11. Oxidation behavior of equiatomic TiNi alloy in high temperature air environment10.1016/0921-5093(96)10409-3 ↗
12. Oxidation of an NiTi alloy10.1002/sia.740150602 ↗
13. Oxidation of nitinol, SMST
14. The oxidation of alloys10.1088/0034-4885/39/5/001 ↗
15. Oxidation behavior of a Ti16.7Zr16.7Hf16.7Cu16.7Ni16.7Be16.7 high-entropy bulk metallic glass10.1016/j.matlet.2018.10.056 ↗
16. Effect of minor addition of Zr on the oxidation behavior of Ti-Cu metallic glasses10.1007/s12540-016-5587-7 ↗
17. Diffusion studies in amorphous NiZr alloys and their relevance for solid state amorphizing reactions10.1016/0022-5088(88)90395-5 ↗
18. Multilayered scale formation during Zr-based metallic glass oxidation in the supercooled liquid region10.1016/j.corsci.2016.05.044 ↗
19. Effect of thermal stability of the amorphous substrate on the amorphous oxide growth on Zr-Al-(Cu, Ni) metallic glass surfaces10.1016/j.corsci.2013.04.009 ↗
20. Oxidation behavior of Ti-Cu binary metallic glass10.1016/j.corsci.2015.07.027 ↗
21. The thermodynamic stability of amorphous oxide overgrowths on metals10.1016/j.actamat.2007.10.023 ↗
22. Thermal stability of amorphous oxide in Al87Ni3Y10 metallic glass10.1016/j.corsci.2013.08.010 ↗
23. Remarkably stable amorphous metal oxide grwon on Zr-Cu-Be metallic glass10.1038/srep18196 ↗
24. Investigation on the oxidation mechanism of titanium10.3891/acta.chem.scand.12-0239 ↗
25. Oxygen vacancy and hole conduction in amorphous TiO210.1039/C4CP04209C ↗