Abstract

The oxidation behavior of austenitic stainless steels with 0 and 2.5 wt% Al exposed to 500–600 °C supercritical water was studied. The oxidation rate-temperature dependence of base steel (0 wt% Al) followed the conventional Arrhenius law, while the alumina-forming austenitic stainless steel (AFA steel, 2.5 wt% Al) exhibited an anomalous oxidation rate-temperature dependence, which is attributed to the special phase transition and oxidation behavior of B2-NiAl precipitates in the AFA steel.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Materials for future nuclear energy systems10.1016/j.jnucmat.2019.151837 ↗
2. 4 - Corrosion phenomena induced by supercritical water in Generation IV nuclear reactors
3. Supercritical water-cooled reactor materials – Summary of research and open issues10.1016/j.pnucene.2014.02.008 ↗
4. Creep-Resistant, Al2O3-Forming Austenitic Stainless Steels10.1126/science.1137711 ↗
5. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
6. Corrosion of alumina-forming austenitic steel Fe–20Ni–14Cr–3Al–0.6Nb–0.1Ti in supercritical water10.1016/j.jnucmat.2010.01.025 ↗
7. The corrosion and stress corrosion cracking behavior of a novel alumina-forming austenitic stainless steel in supercritical water10.1016/j.jnucmat.2016.10.039 ↗
8. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
9. Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam10.1016/j.actamat.2022.117634 ↗
10. Alumina scale formation: a new perspective
11. Research progress of alumina-forming austenitic stainless steels: a review10.3390/ma15103515 ↗
12. Effects of Nb/Ti/V/Ta on phase precipitation and oxidation resistance at 1073 K in alumina-forming austenitic stainless steels10.1016/j.matchar.2018.07.007 ↗
13. The effect of aluminium addition on the high-temperature oxidation behaviour and Cr evaporation of aluminised and alumina-forming alloys for SOFC cathode air pre-heaters10.1016/j.corsci.2020.108612 ↗
14. Chromium evaporation and oxidation characteristics of alumina-forming austenitic stainless steels for balance of plant applications in solid oxide fuel cells10.1016/j.ijhydene.2021.04.002 ↗
15. Chromium vaporization from alumina-forming and aluminized alloys10.1016/j.ssi.2008.09.015 ↗
16. Oxidation of ferritic–martensitic alloys T91, HCM12A and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
17. Effect of exposure temperature on the corrosion behaviors of TP347H austenitic stainless steel in supercritical water10.1016/j.corsci.2019.108188 ↗
18. Analyses of oxide films grown on AISI 304L stainless steel and Incoloy 800HT exposed to supercritical water environment10.1016/j.jnucmat.2011.05.007 ↗
19. Corrosion behavior of alloy 800H (Fe–21Cr–32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
20. Oxidation behavior of Incoloy 800 under simulated supercritical water conditions10.1016/j.jnucmat.2008.12.004 ↗
21. Temperature Dependence of Oxidation behaviour of a ferritic–martensitic steel in supercritical water at 600–700 °C10.1007/s11085-016-9647-7 ↗
22. Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650 °C10.1016/j.corsci.2004.01.010 ↗
23. W.J. Quadakkers. Temperature and gas composition dependence of internal oxidation kinetics of an Fe - 10%Cr alloy in water vapour containing environments10.1002/maco.201005865 ↗
24. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
25. Design of alumina-forming austenitic stainless steel using genetic algorithms10.1016/j.matdes.2019.108198 ↗
26. Overview of strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels10.1007/s11661-010-0295-2 ↗
27. Correlating oxidation resistance to stress corrosion cracking of 309L and 308L stainless steel claddings in simulated PWR primary water10.1016/j.jnucmat.2022.153509 ↗
28. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
29. Microstructural understanding of the oxidation and inter-diffusion behavior of Cr-coated Alloy 800H in supercritical water10.1016/j.corsci.2022.110910 ↗
30. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
31. One dimensional wormhole corrosion in metals10.1038/s41467-023-36588-9 ↗
32. Interdiffusion in the FCC-structured Al-Co-Cr-Fe-Ni high entropy alloys: experimental studies and numerical simulations10.1016/j.jallcom.2016.03.046 ↗
33. Ni tracer diffusion in CoCrFeNi and CoCrFeMnNi high entropy alloys10.1016/j.jallcom.2016.07.239 ↗
34. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
35. Formation of a well-ordered aluminium oxide overlayer by oxidation of NiAl (110)10.1016/0039-6028(91)90555-7 ↗
36. Temperature effect on growth of well-ordered thin Al2O3 film on NiAl (110)10.1116/1.1515907 ↗
37. Oxidation-driven surface dynamics on NiAl (100)10.1073/pnas.1420690112 ↗
38. Enhancing fatigue life by ductile-transformable multicomponent B2 precipitates in a high-entropy alloy10.1038/s41467-021-23689-6 ↗
39. Accelerated precipitation in the AFA stainless steel Fe–20Cr–30Ni–2Nb–5Al via cold working10.1016/j.intermet.2014.04.018 ↗
40. High temperature deformation of Laves phase precipitates in alumina-forming austenitic stainless steels10.1016/j.matlet.2017.02.086 ↗
41. Brittle-to-ductile transition in NiAl single crystal10.1016/S1359-6454(97)00370-4 ↗
42. Heat treatment of investment cast PH 13-8 Mo stainless steel: Part I. mechanical properties and microstructure10.1007/BF02665455 ↗
43. On the loss of protective scale formation in creep-resistant, alumina-forming austenitic stainless steels at 900 °C in air10.4028/www.scientific.net/MSF.595-598.725 ↗
44. Effects of silicon additions on the oxide scale formation of an alumina-forming austenitic alloy10.1016/j.corsci.2012.08.039 ↗