journal article·2024-02Open access

Integrating APS TBCs with a built-in Al2O3 protection network for superior CMAS resistance

Shiying Qin, Huatang Cao, Zhaohe Gao, João P. Martins, Yang Liu, Gyn Brewster, Ying Chen, Ping Xiao

Corrosion Science· Volume 227

Abstract

Calcium–magnesium–alumina–silicate (CMAS) attack poses a great threat to the durability of thermal barrier coatings (TBCs). We introduce a novel Al2O3-modified TBC architecture to counter this threat. The architecture integrates an Al2O3 protection network into the microstructure of an atmospheric plasma sprayed (APS) TBC by drip coating method, which modifies the vulnerable infiltration pathway of CMAS melt and promotes the self-crystallization of CMAS at the infiltration front. Moreover, during sintering, the built-in Al2O3 can inhibit inter-splat crack healing. This innovative TBC design achieves robust CMAS resistance and strain tolerance, while also offering advantages during sintering.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Phase stability in plasma sprayed partially stabilized zirconia-yttria
2. Mechanisms con- trolling the durability of thermal barrier coatings10.1016/S0079-6425(00)00020-7 ↗
3. A delamination mechanism for thermal barrier coatings subject to calcium-magnesium-alumino-silicate (CMAS) infiltration10.1016/j.actamat.2004.11.028 ↗
4. Calcia-magnesia-alumino-silicate (CMAS)-induced degradation and failure of air plasma sprayed yttria-stabilized zirconia thermal barrier coatings10.1016/j.actamat.2015.12.044 ↗
5. Plasma sprayed gadolinium zirconate thermal barrier coatings that are resistant to damage by molten Ca-Mg-Al-silicate glass10.1016/j.surfcoat.2012.03.051 ↗
6. Jet engine coatings for resisting volcanic ash damage10.1002/adma.201004783 ↗
7. Buckling failure in air-plasma sprayed thermal barrier coatings induced by molten silicate attack10.1016/j.scriptamat.2015.09.029 ↗
8. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
9. In situ Raman spectroscopy studies of high-temperature degradation of thermal barrier coatings by molten silicate deposits10.1016/j.scriptamat.2013.12.008 ↗
10. Thermochemical interaction of thermal barrier coatings with molten CaO–MgO–Al2O3–SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
11. Melting and crystallization of silicate systems relevant to thermal barrier coating damage10.1111/jace.13478 ↗
12. Role of environment deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
13. Evaluation of laser-glazed plasma-sprayed thermal barrier coatings under high temperature exposure to molten salts10.1016/j.surfcoat.2005.10.011 ↗
14. Interaction and infiltration behavior of Eyjafjallajökull, Sakurajima volcanic ashes and a synthetic CMAS containing FeO with/in EB-PVD ZrO2-65 wt% Y2O3 coating at high temperature10.1016/j.actamat.2017.06.055 ↗
15. Volcanic ash‐induced decomposition of EB‐PVD Gd2Zr2O7 thermal barrier coatings to Gd‐oxyapatite, zircon, and Gd, Fe‐zirconolite10.1111/jace.12251 ↗
16. Novel thermal barrier coatings that are resistant to high- temperature attack by glassy deposits10.1016/j.actamat.2007.08.028 ↗
17. Composition effects of thermal barrier coating ceramics on their interaction with molten Ca–Mg–Al–silicate (CMAS) glass10.1016/j.actamat.2012.06.053 ↗
18. Hot corrosion behaviour of La2(Zr0.7Ce0. 3)2O7 thermal barrier coating ceramics exposed to molten calcium magnesium alumina silicate at different temperatures10.1016/j.corsci.2015.08.031 ↗
19. La2 (Zr0.7Ce0.3)2O7 thermal barrier coatings prepared by electron beam-physical vapor deposition that are resistant to high temperature attack by molten silicate10.1016/j.corsci.2016.11.015 ↗
20. Calcium-magnesium-alumina-silicate (CMAS) resistance characteristics of LnPO4 (Ln= Nd, Sm, Gd) thermal barrier oxides10.1016/j.jeurceramsoc.2016.08.013 ↗
21. CMAS resistance characteristics of LaPO4/YSZ thermal barrier coatings at 1250° C–1350° C10.1016/j.corsci.2019.04.014 ↗
22. Calcium-magnesium-alumina-silicate (CMAS) resistant Ba2REAlO5 (RE= Yb, Er, Dy) ceramics for thermal barrier coatings10.1016/j.jeurceramsoc.2017.06.004 ↗
23. Air-plasma-sprayed thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2010.09.013 ↗
24. Effect of alumina additions upon electrical properties of 8 mol.% yttria-stabilized zirconia10.1016/S0167-2738(99)00015-6 ↗
25. Electrophoretically deposited alumina as protective overlay for thermal barrier coatings against CMAS degradation10.1016/j.surfcoat.2009.09.055 ↗
26. Thermal cycling of suspension plasma sprayed alumina‐YSZ coatings containing amorphous phases10.1111/j.1551-2916.2012.05292.x ↗
27. EB-PVD alumina (Al2O3) as a top coat on 7YSZ TBCs against CMAS/VA infiltration: deposition and reaction mechanisms10.1016/j.jeurceramsoc.2018.03.027 ↗
28. Coatings of metastable ceramics deposited by solution-precursor plasma spray: I. Binary ZrO2–Al2O3 system10.1016/j.actamat.2006.06.025 ↗
29. Cr3+-doped macroporous Al2O3 monoliths prepared by the metal-salt-derived sol–gel method10.1016/j.jnoncrysol.2007.06.091 ↗
30. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
31. Farokhi · 2015 · 483–488 · 7
32. Microstructural study of the theta-alpha transformation in alumina scales formed on nickel-aluminides10.1179/mht.2000.011 ↗
33. A.S.T.M. E1920-standard guide for metallographic preparation of thermal sprayed coatings
34. Transient-alumina transformations during the oxidation of magnetron-sputtered CoCrAl nanocrystalline coatings10.1023/A:1026015101783 ↗
35. Elastic and conductive properties of plasma-sprayed ceramic coatings in relation to their microstructure: an overview10.1007/s11666-009-9344-z ↗
36. Interaction between ceramic powder and molten calcia-magnesia-alumino-silicate (CMAS) glass, and its implication on CMAS-resistant thermal barrier coatings10.1016/j.scriptamat.2015.09.027 ↗
37. Tracking the calcium-magnesium-alumino-silicate (CMAS) infiltration into an air-plasma spray thermal barrier coating using X-ray imaging10.1016/j.scriptamat.2019.09.016 ↗
38. Measurement of Young’s modulus of oxides at high temperature related to the oxidation study10.3184/096034011X13182685579795 ↗
39. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
40. Deposition and characteristics of submicrometer-structured thermal barrier coatings by suspension plasma spraying10.1007/s11666-012-9762-1 ↗
41. Assessing coating reliability through pore architecture evaluation10.1007/s11666-010-9474-3 ↗
42. An image-based model for the sintering of air plasma sprayed thermal barrier coatings10.1016/j.actamat.2021.116649 ↗
43. The effect of thermal grooving on grain boundary motion10.1016/0001-6160(58)90020-8 ↗
44. Thermodynamics of sintering/sintering of advanced materials