Abstract
Abstract Previous findings demonstrated roughness increase in the oxide/ferritic Mn-depleted zone interface in an austenitic FeMnSiCrNi shape memory stainless steel (SMSS) cyclic oxidized, generated by plastic deformation. The main aim here was to assess the causes of roughness evolution during cyclic oxidation of an FeMnSiCrNiCe SMSS at 950 °C. Thus, isothermal and cyclic oxidation tests were conducted, metal/oxide interface roughness was measured and the oxide layers characterized. The isothermal tests on the FeMnSiCrNiCe SMSS samples demonstrated increasing roughness, however less than after cyclic tests, allowing the identification of a more complete mechanism, where oxide growth and chemical effects also take place.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Reconciling viability and cost-effective shape memory alloy options – a review of copper and iron based shape memory metallic systems
2. Corrosion behavior of shape memory stainless steel in acid media10.1016/j.jallcom.2011.02.051 ↗
3. Characterization of passive films on shape memory stainless steels10.1016/j.corsci.2011.12.022 ↗
4. Influence of alloying elements on the corrosion properties of shape memory stainless steels10.1016/j.matchemphys.2012.01.049 ↗
5. Effects of alloying additions on Fe-Mn-Si shape memory alloys10.2355/isijinternational.30.674 ↗
6. Oxidation behavior of an austenitic stainless FeMnSiCrNi shape memory alloy10.1016/j.corsci.2012.09.029 ↗
7. Kinetics oxidation and characterization of cyclically oxidized layers at high temperatures for FeMnSiCrNiCe and FeSiCrNi alloys10.1590/1980-5373-mr-2017-0098 ↗
8. Microstructure and surface oxidation behavior of an austenitic Fe-Mn-Si-Cr-Ni-Co shape memory stainless steel at 800 °C in air10.1016/j.corsci.2019.108103 ↗
9. Anomalous cyclic oxidation behaviour of a Fe–Mn–Si–Cr–Ni shape memory alloy10.1016/j.corsci.2017.02.026 ↗
10. The effect of Mn-depleted surface layer on the corrosion resistance of shape memory Fe-Mn-Si-Cr alloys10.1007/s11661-997-0287-z ↗
11. Fabrication of ferrite-coated magnetic Fe–Mn–Si–Cr–Ni alloy utilizing selective oxidation of Mn element
12. A novel sandwich Fe-Mn damping alloy with ferrite shell prepared by vacuum annealing10.1088/1361-665X/aaaf95 ↗
13. Improvement of oxidation resistance of an Fe-Mn-Si-Cr shape memory alloy by annealing under vacuum10.2320/matertrans.46.1745 ↗
14. High temperature oxidation resistance improvement in an FeMnSiCrNi alloy by Mn-depletion under vacuum annealing10.1016/j.matlet.2019.01.074 ↗
15. Anomalous cyclic oxidation behaviour of an Fe-Mn-Si-Cr-Ni alloy - A finite element analysis10.1016/j.corsci.2018.11.018 ↗
16. On the rumpling mechanism in nickel-aluminide coatings part I: an experimental assessment
17. On the rumpling mechanism in nickel-aluminide coatings part II: characterization of surface undulations and bond coat swelling
18. Rumpling of nickel aluminide coatings: a reassessment of respective influence of thermal grown oxide and phase transformations10.1080/09603409.2016.1177997 ↗
19. Test methods and data on the mechanical properties of protective oxide scales10.1179/mht.2001.004 ↗
20. High temperature behavior of the metal/oxide interface of ferritic stainless steels10.1016/j.corsci.2012.02.025 ↗
21. Influence of cooling rate and initial surface roughness on the residual stresses in chromia scales thermally grown on pure chromium10.1016/S0921-5093(00)02037-2 ↗
22. A model for the oxide growth stress and its effect on the creep of metals10.1007/BF02668546 ↗
23. The role of the surface roughness on the integrity of thermally generated oxide scales. Application to the Al2O3/MA956 system10.1016/S0921-5093(97)00029-4 ↗
24. Li · 2014 · 27 · 501
25. Effect of cerium addition on oxidation behavior of 25Cr20Ni alloy under low oxygen partial pressure10.1016/S1002-0721(12)60016-7 ↗
26. The oxidation improvement of Fe3Al based alloy with cerium addition at temperature above 1000°C10.1016/S0921-5093(03)00468-4 ↗
27. Cyclic oxidationguidelines for test standardisation, aimed at the assessment of service behaviour
28. Relation between oxidation kinetics and chromium diffusion in stainless steels10.4028/www.scientific.net/MSF.461-464.45 ↗
29. High temperature corrosion behavior of siliconized 310 stainless steel10.1016/S0254-0584(99)00264-3 ↗
30. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
31. Atomic mobilities, uphill diffusion and proeutectic ferrite growth in Fe – Mn – C alloys, CALPHAD Comput10.1016/j.calphad.2009.07.002 ↗
32. Influence of temperature on the oxidation behaviour of an austenitic stainless FeMnSiCrNi shape memory alloy10.1007/s11085-019-09916-y ↗
33. The effect of Mn on the oxidation behavior and electrical conductivity of Fe-17Cr alloys in solid oxide fuel cell cathode atmosphere10.1016/j.jpowsour.2011.05.007 ↗
34. Critical evaluation and thermodynamic modeling of the Mn – Cr – O system for the oxidation of SOFC interconnect10.1016/j.ssi.2006.01.012 ↗
35. Thermodynamic assessment of the Cr – Mn – O system10.1016/j.jallcom.2010.04.252 ↗
36. Stress effects in high temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
37. The air oxidation of an austenitic Fe-Mn-Cr stainless steel for fusion-reactor applications10.1007/BF00655899 ↗
38. Oxidation of alloys involving noble metals10.1149/1.2430159 ↗
39. Diffusion of chromium, manganese, and iron in MnCr2O4 spinel10.1007/s11669-005-0051-2 ↗