journal article·2011-03

Inert anode composed of Ni–Cr alloy substrate, intermediate oxide film and α-Al2O3/Au (Au–Pt, Au–Pd, Au–Rh) surface composite coating for aluminium electrolysis

X.X. Ma, Y.D. He, D.R. Wang

Corrosion Science· Volume 53· Issue 3
Publisher page

Abstract

Abstract An inert anode composed of alloy substrate, intermediate oxide film and surface composite coating for aluminium electrolysis has been fabricated. The intermediate oxide film (ZrO 2 /Y 2 O 3 ) provides good adhesion and mutual diffusion resistance between the substrate and the surface coating which consists of α-Al 2 O 3 particles embedded in Au (Au–Pt, Au–Pd, Au–Rh) matrix. The results of electrolysis test revealed that aluminium with high purity (>99.999%) can be produced. It is demonstrated that the inert anode exhibits superior erosion and corrosion resistance during aluminium electrolysis, especially in low-temperature (800 °C) electrolytes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. W. Haupin, in: W.S. Peterson, R.E. Miller (Eds.), History of Electrical Energy Consumption by Hall–Héroult Cells, Hall–Héroult Centennial Volume, The Metallurgical Society, Inc., Warrendale, PA, 1986.
2. C.M. Hall, US Patent No. 400, 664, Process of Reduction Aluminum from its Fluoride Salts by Electrolysis, April 2, 1889.
3. Electrochemical oxidation of binary copper–nickel alloys in cryolite melts10.1016/j.corsci.2007.03.020 ↗
4. H. Kvande, Inert Anodes – Latest Developments, Industrial Aluminum Electrolysis, Theory and Practice of Primary Aluminum Production, September 8–12, 2003, Quebec, Canada.
5. R.P. Pawlek, Inert anodes: an update, in: Light Metals, TMS, 2008, pp. 1039–1042.
6. X.S. Zhang, Current status of inert anodes study in aluminum electrolysis, J. Mater. Metall. 4 (2005) 1, 13–16.
7. I. Galasiu, R. Galasiu, J. Thonstad, Inert Anodes for Aluminum Electrolysis, 1st Aluminium, Verlag, Düsseldorf, 2007, p. 207.
8. Inert anodes: research, development, and potential
9. David H. De Young, Solubilities of oxides for inert anodes in cryolite-based melts, in: R.E. Miller (Ed.), Light Metals, TMS, Warrendale, PA, 1986, pp. 299–307.
10. Alan D. McLeod, Jean-Marc Lihrmann, John S. Haggerty, Donald R. Sadoway, Selection and testing of inert anode materials for Hall cells, in: R.D. Zabreznik (Ed.), Light Metals, TMS/AIME, Warrendale, PA, 1987, pp. 357–365.
11. Inert anodes for the Hall–Héroult cell: the ultimate materials challenge10.1007/s11837-001-0206-5 ↗
12. Anode overvoltage on platinum in cryolite–alumina melts10.1016/0013-4686(68)87016-1 ↗
13. Alan D. McLeod, John S. Haggerty, Donald R. Sadoway, Inert anode materials for Hall cells, in: R.E. Miller (Ed.), Light Metals, TMS/AIME, Warrendale, PA, 1986, pp. 269–273.
14. E.S. Scherba, US Patent No. 6551476, Noble-Metal Coated Inert Anode for Aluminum Production, April 22, 2003.
15. High temperature mechanical properties of the platinum group metals10.1595/003214001X4527482 ↗
16. Status report on inert anode technology for primary aluminum
17. V. De Nora, Inert Anode are Knocking at the Door of Aluminium Producers, CRU Annual Meeting, London, 2001.
18. Al2O3–Y2O3 composite ceramic coatings prepared by sol-gel thermal pressure and their high temperature oxidation resistance
19. Research on liquidus temperature of electrolyte in K3AlF6–Na3AlF6–AlF3 system
20. Novel materials synthesis by mechanical alloying/milling10.1179/imr.1998.43.3.101 ↗
21. Coarsening kinetics at 600°C of Al2O3 dispersoids in a mechanically alloyed aluminium alloy10.1016/S1359-6462(02)00153-7 ↗
22. The influence of grinding on the surface properties of alumina10.1006/jcis.1993.1087 ↗
23. Liu Xinkuan, Ma Mingliang, Xi shengqi, Zhou Jingen, Wang Qudong, Ding Wenjiang, Mechanochemical effects of alumina in high-energy ball milling, Mater. Sci. Technol. 8 (2000) 41–45.
24. Mass transport considerations for the development of oxygen-evolving anodes in aluminum electrolysis10.1016/S0013-4686(96)00381-7 ↗
25. Tin dioxide-based ceramics as inert anodes for aluminum smelting: a laboratory study
26. He Hanbing, Zhou Kechao, Li Zhiyou, Progress in studies on corrosion of NiFe2O4 based cermet inert anodes, Corros. Prot. 29 (2008) 359–364.
27. T.B. Massalski, H. Okamoto, P.R. Subramanian, L. Kacprzak, Binary Alloy Phase Diagrams, second ed., ASM International, Ohio, 1990.
28. Energetics of metal/ceramic interfaces, metal–semiconductor Schottky contacts, and their relationship10.1016/S0254-0584(97)80041-7 ↗
29. Surface energy of liquid copper and single-crystal sapphire and the wetting behavior of copper on sapphire10.1163/156856188X00264 ↗
30. Resistance of solid surfaces to wetting by water10.1021/ie50320a024 ↗
31. Wetting of (0001) α-Al2O3 crystals by molten Al10.1016/S1359-6462(02)00518-3 ↗
32. Joonho Lee, Hiromichi Ishimura, Toshihiro Tanaka, Anisotropy of wetting of molten Au on differently oriented α-Al2O3 single crystals, Scr. Mater. 54 (2006) 1369–1373.10.1016/j.scriptamat.2005.12.006 ↗
33. Nano-crystalline oxide ceramics prepared by high-energy ball milling10.1023/A:1011324429011 ↗
34. Magnetic and structural properties of magnetoresistive FexAu100−x alloys produced by mechanical alloying10.1016/S0921-4526(02)00660-9 ↗
35. Benoit Panicaud, Jean-Luc Grosseau-Poussard, Mbaihoudou Kemdehoundja, Jean-Francois Dinhut, Mechanical features optimization for α-Cr2O3 oxide films growing on alloy NiCr30, Comput. Mater. Sci. 46 (2009) 42–48.10.1016/j.commatsci.2009.02.003 ↗
36. Dispersion hardening of metals by nanoscaled ceramic powders10.1016/S0921-5093(97)00269-4 ↗
37. Study of solid electrolyte polarization by a complex admittance method10.1016/0022-3697(69)90039-0 ↗
38. Qi Huibin, D.G. Lees, He Yedong, Effect of surface-applied rare earth containing thin oxide films on high-temperature oxidation of Fe25Cr, Corros. Sci. Prot. Technol. 11 (1999) 193.