Photoactivity of brookite–rutile TiO2 nanocrystalline mixtures obtained by heat treatment of hydrothermally prepared brookite
Source abstract
Abstract
Abstract Pure brookite phase was prepared by hydrothermal synthesis of titanium peroxo-complex in the presence of glycolic acid at 220 °C. The structure of prepared brookite samples was determined by X-ray powder diffraction (XRD) and selected area electron diffraction (SAED). The prepared brookite was studied by in situ high temperature XRD in air. The morphology and microstructure characteristics were also obtained by transmission electron microscopy (TEM). The nitrogen adsorption–desorption was used for determination of surface area (BET) and porosity. The method of UV–vis diffuse reflectance spectroscopy was employed to estimate band-gap energies of prepared brookite. The photocatalytic activity of the prepared titania samples were assessed by photocatalytic decomposition of Orange II dye in an aqueous slurry under UV irradiation at 365 nm wavelength. The photocatalytic activity of the prepared sample brookite heated to 800 °C in air was higher than nanocrystalline unheated brookite powder.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Photocatalysis Techniques · TiO2 Photocatalysis and Solar Cells · Pigment Synthesis and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Synthesis of brookite TiO2 nanoparticles by thermolysis of TiCl4 in strongly acidic aqueous media10.1039/b100435m ↗
2. Synthesis of brookite TiO2 nanoparticles by ambient condition sol process10.1016/j.matlet.2005.10.114 ↗
3. Experimental variables in the synthesis of brookite phase TiO2 nanoparticles10.1016/j.msea.2007.02.092 ↗
4. Nanocrystalline brookite-type titanium(IV) oxide photocatalysts prepared by a solvothermal method: correlation between their physical properties and photocatalytic activities10.1023/B:CATL.0000006316.45620.30 ↗
5. Monodispersed spherical particles of brookite-type TiO2: synthesis, characterization, and photocatalytic property10.1111/j.1151-2916.2004.tb07735.x ↗
6. Phase-pure TiO2 nanoparticles: anatase, brookite and rutile10.1088/0957-4484/19/14/145605 ↗
7. Hydrothermal synthesis of brookite10.1246/cl.1999.911 ↗
8. Novel hydrothermal preparation of pure brookite-type titanium(IV) oxide nanocrystal under strong acidic conditions10.1016/j.catcom.2008.12.038 ↗
9. Synthesis of brookite-typed titania from titanium chloride solution10.4028/www.scientific.net/MSF.610-613.285 ↗
10. Hydrothermal preparation and characterization of brookite-type TiO2 nanocrystallites10.1023/A:1011010306699 ↗
11. Direct synthesis of brookite-type titanium oxide by hydrothermal method using water-soluble titanium complexes10.1007/s10853-007-1912-3 ↗
12. Transformation of brookite-type TiO2 nanocrystals to rutile: correlation between microstructure and photoactivity10.1039/b514632a ↗
13. Home-prepared anatase, rutile, and brookite TiO2 for selective photocatalytic oxidation of 4-methoxybenzyl alcohol in water: reactivity and ATR-FTIR study10.1039/b818353h ↗
14. Adsorption and photoinduced decomposition of acetone and acetic acid on anatase, brookite, and rutile TiO2 nanoparticles10.1021/jp103263n ↗
15. Tailored titanium dioxide nanomaterials: anatase nanoparticles and brookite nanorods as highly active photocatalysts10.1021/cm903472p ↗
16. Visible light photocatalytic properties of polymorphic brookite titania10.1063/1.3096606 ↗
17. Tailored preparation methods of TiO2 anatase, rutile, brookite: mechanism of formation and electrochemical properties10.1021/cm902613h ↗
18. 2001
19. ICSD Database FIZ Karlsruhe, Germany, 2008.
20. Adsorption of gases in multimolecular layers10.1021/ja01269a023 ↗
21. The determination of pore volume and area distributions in porous substances. I. Computations from nitrogen isotherms10.1021/ja01145a126 ↗
22. Application of the Kubelka–Munk theory for the determination of the optical properties of solar absorbing paints10.1016/S0300-9440(96)00659-5 ↗
23. Photocatalytic degradation of various types of dyes (Alizarin S, Crocein Orange G, Methyl Red, Congo Red, Methylene Blue) in water by UV-irradiated titania10.1016/S0926-3373(02)00078-4 ↗
24. Fresnel lens to concentrate solar energy for the photocatalytic decoloration and mineralization of Orange II in aqueous solution10.1016/j.chemosphere.2006.04.057 ↗
25. Optically transparent titanium dioxide particles incorporated in poly(hydroxyethyl methacrylate) thin layers10.1021/jp803194p ↗
26. Understanding polymorphic phase transformation behavior during growth of nanocrystalline aggregates: insights from TiO210.1021/jp000499j ↗
27. Thermal stability of brookite-TiO2 nanoparticles with controlled size and shape: in-situ studies by XRD
28. Quantitative analysis in diffuse reflectance spectrometry: a modified Kubelka–Munk equation10.1016/0924-2031(94)00065-O ↗
29. Bandgap studies on anatase titanium dioxide nanoparticles10.1016/S0254-0584(02)00343-7 ↗
30. Size effects on the photophysical properties of colloidal anatase TiO2 particles: size quantization or direct transitions in this indirect semiconductor?10.1021/j100045a026 ↗
31. Effect of the preparation method on the band gap of titania and platinum titania sol–gel materials10.1016/0167-577X(95)00190-5 ↗
32. Wannier functions and Born charge tensors of brookite TiO210.1103/PhysRevB.74.125113 ↗
33. Electronic and optical properties of three phase of titanium dioxide: rutile, anatase and brookite10.1103/PhysRevB.51.13023 ↗
34. Ozonation of cationic Red X-GRL in aqueous solution: degradation and mechanism10.1016/j.chemosphere.2004.08.014 ↗
35. Visible light-induced photocatalytic degradation of Acid Orange 7 in aqueous TiO2 suspensions10.1016/j.apcatb.2003.09.014 ↗
36. Low temperature synthesis of crystalline mesoporous titania with high photocatalytic activity by post-treatment in nitric acid ethanol solution10.1016/j.matlet.2008.09.020 ↗
37. Synthesis and photocatalytic properties of nano bi-crystalline titania of anatase and brookite by hydrolyzing TiOCl2 aqueous solution at low temperatures10.1163/1568567053956554 ↗
38. Photocatalytic dehydrogenation of aliphatic-alcohols by aqueous suspensions of platinized titanium-dioxide10.1039/f19858102467 ↗
39. Linear relationship between the crystallite size and the photoactivity of non-porous titania ranging from nanometer to micrometer size10.1016/S0926-860X(01)00784-0 ↗
40. Photoactivity of anatase–rutile TiO2 nanocrystalline mixtures obtained by heat treatment of homogeneously precipitated anatase10.1016/j.apcatb.2004.06.019 ↗