journal article·2024-01

Effect of tellurium treatment on the pitting behavior of 38MnVS6 Non-quenched and tempered steel in alkaline environment

Wenbo Wu, Songang Yang, Donghua Suo, Xin Tan, Yiming Jiang, Jin Li, Yangting Sun

Corrosion Science· Volume 226
Publisher page

Abstract

This paper investigates the impact of tellurium (Te) treatment on the pitting behavior of 38MnVS6 Non-quenched and Tempered steel (NQTS) in an alkaline environment. The electrochemical tests demonstrate an increase in pitting potential within the Te content from 0 to 500 ppm and a decrease from 500 to 1600 ppm. Pitting can be ascribed to the preferential dissolution at the inclusion/matrix interface, which is caused by the stress concentration. At the presence of micro-crevices, it is easier for inclusions to induce stable pitting.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Constitutive modeling of dynamic recrystallization behavior and processing Map of 38MnVS6 non-quenched steel10.1007/s11665-013-0808-4 ↗
2. Microstructural effects on high-cycle fatigue properties of microalloyed medium carbon steel 38MnVS10.1016/j.msea.2015.05.054 ↗
3. Gigacycle fatigue of high-strength steel caused by MnS inclusions10.1016/j.msea.2021.141840 ↗
4. The effect of nonmetal inclusions and microstructure on local corrosion of carbon and low-alloyed steels10.1023/B:PROM.0000043062.19272.c5 ↗
5. Pit INitiation at Single Sulfide Inclusions in Stainless Steel: I. Electrochemical microcell measurements10.1149/1.1474430 ↗
6. Effect of casting overheat and rolling temperature on morphology of sulfide in 30MnVS steel10.4028/www.scientific.net/AMR.457-458.270 ↗
7. Inclusions modification and improvement of machinability in a non-quenched and tempered steel with Mg treatment10.1051/metal/2020021 ↗
8. Effect of rare earth ce on sulfide characteristics and microstructure in non-quenched and tempered steel
9. Effect of Ca/Mg on distribution and morphology of MnS inclusions in 45MnVS non-quenched and tempered steel10.3390/met13010023 ↗
10. Effect of rare earth–magnesium alloy on inclusion evolution in industrial production of die steel10.1002/srin.201900103 ↗
11. Preparation and molten salts corrosion behavior of high-entropy (Ca,Sr,Ba)TMO3 (TM= Zr, Hf and Ta): promising protecting materials of reference electrode for metal smelting through fused salts electrolysis10.1016/j.corcom.2021.11.002 ↗
12. Thermodynamic examination of inclusion modification and precipitation from calcium treatment to solidified steel10.1179/030192303225001748 ↗
13. Thermodynamic characterization of multiphase non-metallic inclusions in re-sulphurised steel grades
14. Sulfide transformation with tellurium treatment for Y15 free-cutting steel10.1007/s11663-019-01627-8 ↗
15. Modification of MnS inclusion by tellurium in 38MnVS6 micro-alloyed steel10.1051/metal/2020066 ↗
16. Control of MnS inclusions in high- and low-sulfur steel by tellurium treatment10.3390/ma12071034 ↗
17. Development and Application of Non-quenched and Tempered Steels
18. Chloride-induced corrosion of steel rebars in simulated pore solutions of alkali-activated concretes10.1016/j.cemconres.2017.08.006 ↗
19. Corrosion behavior of low-Cr steel rebars in alkaline solutions with different pH in the presence of chlorides10.1016/j.jelechem.2017.09.016 ↗
20. Effect of inclusions on pitting corrosion of C70S6 non-quenched and tempered steel doped with Ca and Mg
21. A new microelectrochemical method to study pit initiation on stainless steels10.1016/S0013-4686(70)01783-8 ↗
22. Why stainless steel corrodes10.1038/415770a ↗
23. Occluded solution chemistry control and the role of alloy sulfur on the initiation of crevice corrosion in type 304ss10.1016/S0010-938X(98)00084-5 ↗
24. The role of dislocation channeling in IASCC initiation of neutron irradiated stainless steel10.1016/j.jnucmat.2016.09.001 ↗
25. Pitting corrosion behavior in advanced high strength steels10.1016/j.jallcom.2014.08.243 ↗
26. Pitting corrosion of very clean type 304 stainless steel10.5006/0995 ↗
27. Effect of Ce on the inclusions and pitting resistance of 2Cr13 stainless steel
28. J.D. Enobong Felix Daniel, Corrosion Behaviour of Carbon Steel Fasteners in Neutral Chloride Solution, Acta Metall. Sin. Engl. Lett. 35 (n.d.) 563–576. 〈https://doi.org/10.1007/s40195–021-01284–4〉.10.1007/s40195-021-01284-4 ↗
29. Progress on a corrosion study of low carbon steel for HLW container in a simulated geological disposal environment in China10.1016/j.corcom.2021.05.002 ↗
30. Effect of chloride on the pitting corrosion of carbon steel in alkaline solutions10.1149/1945-7111/ac580c ↗
31. Pitting corrosion of iron in weakly alkaline chloride solutions10.5006/1.3293637 ↗
32. On the volta potential measured by SKPFM – fundamental and practical aspects with relevance to corrosion science10.1080/1478422X.2019.1583436 ↗
33. The effect of tellurium on the formation of MnTe-MnS composite inclusions in non-quenched and tempered steel10.3390/met8080639 ↗
34. Enhancement of impurity, machinability and mechanical properties in Te-Treated 0Cr18Ni9 steel10.1007/s12540-019-00545-3 ↗
35. Roles of interstitial nitrogen, carbon, and boron in steel corrosion: generation of oxyanions and stabilization of electronic structure10.1149/1945-7111/ab8926 ↗
36. Influence of nitrogen addition on the crevice corrosion resistance of nitrogen-bearing austenitic stainless steels10.1023/A:1004740905317 ↗
37. The influence of phosphorus on the corrosion of iron in calcium nitrate10.1149/1.2069229 ↗
38. The influence of minor alloying elements (Nb, Ti and Cu) on the corrosion resistivity of ferritic stainless steel in sulfuric acid solution10.1016/0010-938X(86)90085-5 ↗
39. Deformation of MnS–MnTe Inclusions in a sulfur-containing free-cutting steel with tellurium treatment10.1007/s11663-022-02698-w ↗
40. Mechanism of the dual effect of Te addition on the localised corrosion resistance of 15–5PH stainless steel10.1016/j.corsci.2023.110970 ↗
41. The influence of non-metallic inclusion nature and shape on the pitting corrosion susceptibility of 18Cr9Ni and 17Cr11Ni2Mo austenitic stainless steels10.1016/0010-938X(79)90009-X ↗
42. Tellurium treatment for the modification of sulfide inclusions and corresponding industrial applications in special steels: a review10.1002/srin.202200375 ↗
43. A study on resulfurized free-machining steel containing a small amount of Tellurium10.4262/denkiseiko.53.195 ↗
44. Characterization of AA2024–T3 by scanning kelvin probe force microscopy10.1149/1.1838633 ↗
45. Mechanisms of inclusion-induced pitting of stainless steels: a review10.1016/j.jmst.2023.06.008 ↗
46. A critical review of the recent advances in inclusion-triggered localized corrosion in steel10.1038/s41529-022-00294-6 ↗
47. Roles of different components of complex inclusion in pitting of 321 stainless steel: induction effect of CaS and inhibition effect of TiN10.1016/j.corsci.2022.110692 ↗
48. Effects of hydrogen charge on the intergranular corrosion of high-defect-density ultrapure ferrite stainless steel10.1016/j.corsci.2023.111360 ↗
49. Role of Al2O3 inclusions on the localized corrosion of Q460NH weathering steel in marine environment10.1016/j.corsci.2018.04.007 ↗
50. Effect of complex inclusions on localized corrosion behavior in ferritic steel
51. Characterisation of inclusions in resulphurised microalloyed steel10.1179/1743281212Y.0000000031 ↗
52. Local analysis of the mechanical behaviour of inclusions-containing stainless steels under straining conditions10.1016/S1359-6462(03)00411-1 ↗
53. The initiation of pitting corrosion at Mns inclusions10.1016/0010-938X(93)90279-P ↗
54. Characterization of inclusions in clean steels: a review including the statistics of extremes methods10.1016/S0079-6425(02)00014-2 ↗
55. Internal stress and strain energy yielded by γ→ε martensitic transformation in a polycrystalline ferrous alloy10.2320/matertrans1989.41.727 ↗
56. Initiation mechanism of localized corrosion induced by Al2O3-MnS composite inclusion in low-alloy structural steel10.3390/met12040587 ↗
57. Localized attack at inclusions in 42CrMo4 QT steel10.1016/j.electacta.2023.142754 ↗
58. Influence of inclusions on early corrosion development of ultra-low carbon bainitic steel in NaCl solution10.5006/1837 ↗
59. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
60. Effects of cerium on the compositional variations in and around inclusions and the initiation and propagation of pitting corrosion in hyperduplex stainless steels10.1016/j.corsci.2013.06.020 ↗
61. Understanding the pitting mechanism of super ferritic stainless steel in bromide solutions: the role of Ti/Nb–Mo precipitates with a core–shell structure10.1016/j.corsci.2022.110176 ↗
62. Localized corrosion: passive film breakdown vs. Pit growth stability: Part III. A unifying set of principal parameters and criteria for Pit stabilization and salt film formation10.1149/2.0251811jes ↗