journal article·2023-07Open access

On the sulfation reaction of protective and transient oxides at 650 °C and its role in the low temperature hot corrosion mechanism

R. Malacarne, S. Mathieu, M. Siblani, L. Aranda, S. Knittel, C. Desgranges, M. Vilasi

Corrosion Science· Volume 218

Abstract

MxOy-Na2SO4 (with M = Ni, Cr, Fe, Al, Ti, Nb) and NiSO4-Na2SO4 mixtures were prepared and their reactivity was examined at 650°C in air + SO2 (400 and 1000 ppm). The formation of a molten phase for NiSO4-Na2SO4 mixtures and the rapid sulfation of NiO in these conditions were demonstrated. NiO sulfation should be considered when explaining the Type II hot corrosion attacks. Cr2O3, Fe2O3 and Al2O3 also react with the gas phase showing these oxides dissolved according to an acidic-fluxing mechanism in air + SO2/SO3 (400 and 1000 ppm) environments. Al2O3 is more soluble than Cr2O3 in these conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Thermal and Kinetic Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Hot corrosion of metals and alloys10.1007/s11085-011-9254-6 ↗
2. Invited review paper in commemoration of over 50 years of oxidation of metals: current aspects of deposit-induced corrosion
3. A review on molten sulfate salts induced hot corrosion
4. High Temperature Corrosion.
5. Sulfate-induced hot corrosion of nickel10.1007/BF00656835 ↗
6. E. Kistler, Modes of Sulfate-Deposit-Induced Metallic Corrosion at Elevated Temperatures: Mechanisms and Mitigation Strategies, (n.d.) 251.
7. A new solid-state mode of hot corrosion at temperatures below 700°C10.1002/maco.201810751 ↗
8. Understanding the type II corrosion mechanism10.1007/s11661-021-06168-x ↗
9. Relationship between compounds of sodium and sulfur and sulfidaiton
10. Hot corrosion of materials: a fluxing mechanism?
11. Acidic and basic fluxing of Ni-base superalloys in a 90Na2SO4-10K2SO4 melt at 1173 K10.1007/BF00666645 ↗
12. Young · 2008
13. The Hot Corrosion of Metals by Fused Salts
14. On the hot corrosion of nickel at 700 °C10.1007/s11085-015-9588-6 ↗
15. Mechanism of Na2 SO 4 induced corrosion at 600°–900°C10.1149/1.2129375 ↗
16. Low temperature hot corrosion of cobalt-base alloys: Part II. reaction mechanism10.1007/BF02647842 ↗
17. Thermodynamics of molten sulfate mixtures10.1149/1.2124305 ↗
18. Role of temperature in Na2SO4–K2SO4 deposit induced Type II hot corrosion of NiAl coating on a commercial Ni-based superalloy10.1002/adem.201901244 ↗
19. Correlations between the kinetics and the mechanisms of hot corrosion of pure nickel at 700 °C10.1016/j.corsci.2019.04.022 ↗
20. Comparison of Na2SO4, K2SO4 and Na2SO4-K2SO4 deposit induced hot corrosion of a β-NiAl coating10.1016/j.corsci.2022.110146 ↗
21. Bol’shakov · ternary Syst. Sodium, Cobalt, Nickel Sulfates · 1958 · 3 · 1896
22. S. Andersson, Studies on phase Diagrams Na2S-Na2SO4, Na2CO3-Na2S-Na2SO4,Na2CO3-Na2SO4-NaOH and Na2CO3-Na2S-NaOH, 20 (n.d.) 164–170.
23. System NaOH-Na2SO4-Na2S10.1134/S0036023607070285 ↗
24. Constitution of binary alloys10.1149/1.2428700 ↗
25. The Ni-S system and related minerals10.1093/petrology/3.1.126 ↗
26. Thermodynamics and phase relationships of transition metal-sulfur systems: II. The nickel-sulfur system10.1007/BF03257200 ↗
27. Thermodynamic evaluation and optimization of the (Na+K+S) system10.1016/j.jct.2005.10.003 ↗
28. R. Malacarne, Étude de l′oxydation et de la corrosion à haute température d′alliages base nickel polycristallins, These de doctorat, Université de Lorraine, 2021. 〈https://www.theses.fr/2021LORR0340〉 (Accessed December 15, 2022).
29. Die schweflige Säure im Weine und deren Bestimmung. (Mitteilungen aus Schmitt’s Laboratorium, [Untersuchungs- Amt, chemische Versuchsstation und hygienisches Institut] zu Wiesbaden.)10.1002/prac.18920460131 ↗
30. Barin · 2013
31. Reaction morphologies developed by nickel aluminides in type II hot corrosion conditions: the effect of chromium10.1016/j.corsci.2015.08.029 ↗
32. The crystal structure determinations and refinements of K2S2O7, KNaS2O7 and Na2S2O7 from X-ray powder and single crystal diffraction data10.1016/j.jssc.2005.03.022 ↗
33. Thermodynamics of the Na2SO4-K2SO4-CoSO4 system and their relevance to low-temperature hot corrosion10.1007/BF00666464 ↗
34. Reactions of SO2(SO3) with NiO ‐ Na2SO4 in nickel‐sodium mixed sulfate formation and low temperature hot corrosion10.1149/1.2124219 ↗
35. Transport of oxidant in molten Na2 SO 4 in O 2 – SO 2 – SO 3 environments10.1149/1.2127417 ↗
36. Solubilities of CeO2, HfO2 and Y2O3 in Fused Na2SO4–30 mol% NaVO3 and CeO2 in Pure Na2SO4 at 900C10.5006/1.3583869 ↗
37. Solubilities of Cr2O3 and SiO2 in Na2SO4 – K2SO4 – Fe2(SO4)3 at 963 K10.1149/1.2056185 ↗
38. The solubilities of NiO, Co3 O 4, and ternary oxides in fused Na2 SO 4 at 1200°K10.1149/1.2129374 ↗
39. The role of chromium in the hot corrosion of metals10.1149/1.3159332 ↗
40. The reaction of nickel with SO2 + O2/SO3 at 500–900°C10.1016/0010-938X(83)90082-3 ↗
41. On the reaction mechanism of nickel with SO2+O2/SO310.1007/BF00741467 ↗
42. Chemistry and electrochemistry of hot corrosion of metals10.1016/0025-5416(87)90394-6 ↗
43. Bakai · 2015