A thick SiC-Si coating prepared by one-step pack cementation for long-term protection of carbon/carbon composites against oxidation at 1773 K
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Microstructure and ablation behaviour of a carbon/carbon-ZrC-Cu composite prepared by adding Ti to Zr/Cu powder mixture10.1016/j.corsci.2019.108175 ↗
2. Ablation of the carbon/carbon composite nozzle-throats in a small solid rocket motor10.1016/j.carbon.2010.11.037 ↗
3. Understanding the ultra-high-temperature mechanical behaviors of advanced two-dimensional carbon-carbon composites10.1016/j.ceramint.2020.05.237 ↗
4. Effects of silanization of C/C composites and grafting of h-BN fillers on the microstructure and interfacial properties of CVI-based C/C-BN composites10.1016/j.ceramint.2020.09.192 ↗
5. A CrSi2-HfB2-SiC coating providing oxidation and ablation protection over 1973 K for SiC coated C/C composites10.1016/j.corsci.2020.108536 ↗
6. Isothermal and cyclic oxidation behavior of a sandwiched coating for C/C composites10.1016/j.ceramint.2021.07.167 ↗
7. Microstructure and oxidation of multi-layer MoSi2-CrSi2-Si coatings for SiC coated carbon/carbon composites10.1016/j.corsci.2010.05.020 ↗
8. Oxidation inhibition behaviors of the HfB2-SiC-TaSi2 coating for carbon structural materials at 1700 °C10.1016/j.corsci.2020.108982 ↗
9. Oxidation and ablation resistant properties of pack-siliconized Si-C protective coating for carbon/carbon composites10.1016/j.jallcom.2018.01.214 ↗
10. Blasting treatment and chemical vapor deposition of SiC nanowires to enhance the thermal shock resistance of SiC coating for carbon/carbon composites in combustion environment10.1016/j.jallcom.2016.01.124 ↗
11. Effect of the surface microstructure of SiC inner coating on the bonding strength and ablation resistance of ZrB2-SiC coating for C/C composites10.1016/j.ceramint.2016.09.003 ↗
12. Advances in oxidation and ablation resistance of high and ultra-high temperature ceramics modified or coated carbon/carbon composites10.1016/j.jeurceramsoc.2017.08.013 ↗
13. Ways to reduce the negative consequences of the thermal expansion coefficient mismatch of a carbon-carbon composite and a protective silicide coating10.1016/j.jallcom.2018.07.193 ↗
14. Effect of thermal expansion coefficient on the stress distribution in solar panel10.1016/j.ijadhadh.2006.01.011 ↗
15. Growth mechanism and ablation behavior of CVD-HfC coating on the surface of C/C composites and CVD-SiC coating10.1016/j.corsci.2021.109819 ↗
16. Preparation of a double layer SiC coating and its oxidation resistance at 1773K10.1016/j.corsci.2014.06.024 ↗
17. Ablation resistance of supersonic-atmosphere-plasma-spraying ZrC coating doped with ZrO2 for SiC-coated carbon/carbon composites10.1016/j.corsci.2017.03.019 ↗
18. Oxidation protection of C/C composites: coating development with thermally stabile SiC@PyC nanowires and an interlocking TaB2-SiC structure10.1016/j.corsci.2018.12.024 ↗
19. Reactive pack-cementation coating of silicon carbide on carbon-carbon composite
20. Oxidation and ablation resistance of ZrB2-SiC-Si/B-modified SiC coating for carbon/carbon composites10.1016/j.corsci.2012.10.041 ↗
21. oxidation protective coating for carbon/carbon composites prepared by a two-step pack cementation10.1016/j.ceramint.2009.01.005 ↗
22. TaxHf1−xB2-SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
23. SiC-Si coating with micro-pores to protect carbon/carbon composites against oxidation10.1016/j.jeurceramsoc.2020.08.045 ↗
24. Oxidation behavior of carbon-carbon composites10.1016/0008-6223(79)90056-3 ↗
25. Microstructural evolution of SiC coating on C/C composites exposed to 1500 °C in ambient air10.1016/j.ceramint.2018.09.255 ↗
26. Suppression of through-the-thickness cracks in SiC coating on C/C composites
27. Oxidation resistance of a SiC–ZrB2 coating prepared by a novel pack cementation on SiC-coated graphite10.1007/s10853-016-0457-8 ↗
28. The novel effect mechanism of Al2O3 nano-powder in the pack cementation process to prepare SiC coating on C/C composites10.1016/j.jeurceramsoc.2020.10.014 ↗
29. Passive-oxidation kinetics of high-purity silicon carbide from 800° to 1100°C10.1111/j.1151-2916.1996.tb08724.x ↗
30. Corrosion characteristics of silicon carbide and silicon nitride10.6028/jres.098.040 ↗
31. TaB2-SiC-Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2013.06.028 ↗
32. Sealing role of B2O3 in MoSi2-CrSi2-Si/B-modified SiC coating for C/C composites10.1016/j.corsci.2012.04.018 ↗
33. Microstructure and anti-oxidation property of CrSi2 -SiC coating for carbon/carbon composites10.1016/j.apsusc.2005.05.018 ↗
34. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites10.1016/j.carbon.2004.01.066 ↗
35. Preparation of oxidation protective ZrB2-SiC coating by in-situ reaction method on SiC-coated carbon/carbon composites10.1016/j.surfcoat.2014.03.017 ↗
36. Oxidation protection of ultra-high temperature ceramic ZrxTa1−xB2-SiC/SiC coating prepared by in-situ reaction method for carbon/carbon composites10.1016/j.jeurceramsoc.2014.09.038 ↗
37. The oxidation resistance of two-temperature synthetic HfB2-SiC coating for the SiC coated C/C composites10.1016/j.jallcom.2018.03.043 ↗
38. Improvement in oxidation properties of SiC-coated carbon/carbon composites through modification of the SiC/carbon interface10.1016/j.surfcoat.2014.02.036 ↗
39. Oxidation protective SiC-Si coating for carbon/carbon composites by gaseous silicon infiltration and pack cementation: A comparative investigation10.1016/j.jeurceramsoc.2020.07.040 ↗
40. Silicon carbide coating to protect carbon/carbon composites against oxidation10.1016/j.scriptamat.2004.12.029 ↗
41. Siliconization elimination for SiC coated C/C composites by a pyrolytic carbon coating and the consequent improvement of the mechanical property and oxidation resistances10.1016/j.jeurceramsoc.2021.04.008 ↗
42. Oxidation protective glass coating for SiC coated carbon/carbon composites for application at 1773 K10.1016/j.matlet.2005.09.006 ↗
43. A dense structure Si-SiC coating for oxidation and ablation protection of graphite fabricated by impregnation-pyrolysis and gaseous silicon infiltration10.1016/j.ceramint.2018.06.201 ↗
44. SiC/SiC-ZrSi2 coating with micro-pore to protect C/C composites against oxidation for long-life service at high temperatures10.1016/j.corsci.2021.109780 ↗
45. A gradient composite coating to protect SiC-coated C/C composites against oxidation at mid and high temperature for long-life service10.1016/j.jeurceramsoc.2021.09.013 ↗
46. Bamboo-shaped SiC nanowire-toughened SiC coating for oxidation protection of C/C composites10.1016/j.corsci.2012.12.009 ↗
47. Microstructure and oxidation of multi-layer MoSi2-CrSi2-Si coatings for SiC coated carbon/carbon composites10.1016/j.corsci.2010.05.020 ↗
48. SiCn/SiC oxidation protective coating for carbon/carbon composites10.1016/j.carbon.2009.01.002 ↗
49. Oxidation protection and behavior of in-situ zirconium diboride-silicon carbide coating for carbon/carbon composites10.1016/j.jallcom.2015.04.215 ↗