The use of anion exchange pigments to inhibit the filiform corrosion of zinc-aluminium-magnesium coated steel

N. Wint, D. Eaves, G. Williams, H.N. McMurray

Corrosion Science· Volume 193

Abstract

Abstract In-coating natural (carbonate exchanged) hydrotalcite is shown to significantly reduce the extent of filiform corrosion (FFC) on zinc-aluminium-magnesium (ZAM) coated steels. The hydrotalcite pigment is dispersed within the model poly vinyl butyral (PVB) coating, which is then applied to ZAM. Acetic acid is applied to an artificial scribe penetrative PVB coating defect to initiate corrosion. Filiform corroded area and filament length are shown to decrease with increase in pigment volume fraction (ϕ). Tapering of filaments is also observed. Findings are consistent with hydrotalcite acting to sequester anions or neutralise the filiform head electrolyte.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Layered Double Hydroxides Synthesis and Applications · Corrosion Behavior and Inhibition · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Atmospheric corrosion of ZnAlMg coated steel during long term atmospheric weathering at different worldwide exposure sites10.1016/j.corsci.2018.12.033 ↗
2. Underfilm/coating corrosion
3. The kinetics and mechanism of filiform corrosion occurring on zinc-aluminium-magnesium coated steel10.1016/j.corsci.2019.06.028 ↗
4. Filiform corrosion in polymer-coated metals10.1016/0300-9440(95)00555-2 ↗
5. An analysis of mass transfer in filiform corrosion10.5006/1.3581907 ↗
6. Corrosion protection by organic coatings: electrochemical mechanism and novel methods of investigation10.1016/S0013-4686(00)00348-0 ↗
7. The mechanism of group (I) chloride initiated filiform corrosion on iron10.1016/j.elecom.2003.08.008 ↗
8. The effect of oxygen partial pressure on the filiform corrosion of organic coated iron10.1016/j.corsci.2014.08.004 ↗
9. Mechanism of filiform corrosion10.1021/ie50533a053 ↗
10. Scanning kelvinprobe investigations of filiform corrosion on aluminum alloy 2024-t310.1016/S0010-938X(98)00044-4 ↗
11. New knowledge on localized corrosion obtained from local measuring techniques10.1016/S0013-4686(01)00642-9 ↗
12. Effect of climatic parameters on filiform corrosion of coated aluminum alloys10.5006/1.3287763 ↗
13. The kinetics of chloride-induced filiform corrosion on aluminum alloy AA2024-T310.1149/1.1589020 ↗
14. Chromate inhibition of filiform corrosion on organic coated AA2024-T3 studied using the scanning kelvin probe10.1149/1.1757460 ↗
15. The kinetics and mechanisms of filiform corrosion on aluminium alloy AA611110.1016/j.electacta.2010.04.035 ↗
16. The role of chromate in filiform corrosion inhibition10.1016/S0013-4686(03)00256-1 ↗
17. The role of chromate in filiform corrosion inhibition10.1016/S0013-4686(02)00829-0 ↗
18. Chloride-induced filiform corrosion of organic-coated magnesium10.1016/j.electacta.2010.09.005 ↗
19. Award lecture: molecular in situ studies of atmospheric corrosion10.5006/1.3278420 ↗
20. Atmospheric corrosion of zinc by organic constituents: I. The role of the zinc/water and water/air interfaces studied by infrared reflection/absorption spectroscopy and vibrational sum frequency spectroscopy10.1149/1.2164788 ↗
21. Atmospheric corrosion of zinc by organic constituents: II. Reaction routes for zinc-acetate formation10.1149/1.2360740 ↗
22. GILDES model simulations of the atmospheric corrosion of zinc induced by low concentrations of carboxylic acids10.1149/2.072203jes ↗
23. Initial atmospheric corrosion of zinc induced by carboxylic acids: a quantitative in situ study10.1149/1.3240878 ↗
24. Molecular structural information of the atmospheric corrosion of zinc studied by vibrational spectroscopy techniques: I. Experimental approach10.1149/1.3479207 ↗
25. Molecular structural information of the atmospheric corrosion of zinc studied by vibrational spectroscopy techniques: II. Two and three-dimensional growth of reaction products induced by formic and acetic acid10.1149/1.3479255 ↗
26. Metal carboxylate formation during indoor atmospheric corrosion of Cu, Zn, and Ni10.1149/1.2048598 ↗
27. Characterisation of corrosivity in indoor atmospheres with different metals and evaluation techniques10.1179/bcj.1998.33.1.59 ↗
28. The toxicology of chromium with respect to its chemical speciation: a review10.1002/jat.2550130314 ↗
29. Occurrence of lung cancer in workers producing chromium pigments
30. Cancer mortality in a pigment plant utilizing lead and zinc chromates10.1080/00039896.1982.10667532 ↗
31. Clays and catalysis: a promising future10.1016/S0169-1317(98)00058-1 ↗
32. New members of the hydrotalcite-manasseite group10.1346/CCMN.1987.0350601 ↗
33. Anion-exchange properties of hydrotalcite like compounds10.1346/CCMN.1983.0310409 ↗
34. A hydrotalcite-like pigment containing an organic anion corrosion inhibitor10.1149/1.1857743 ↗
35. Inhibition of filiform corrosion on organic coated aluminium alloy by hydrotalcite-like anion-exchange pigments10.5006/1.3287724 ↗
36. Physico-chemical properties of synthetic hydrotalcites in relation to composition10.1346/CCMN.1980.0280107 ↗
37. Anionic clay minerals
38. On-demand treatment of acute heartburn with the antacid hydrotalcite compared with famotidine and placebo: randomized double-blind cross-over study10.1097/MCG.0b013e31802e7efb ↗
39. New proposal in a biorefinery context: recovery of acetic and formic acids by adsorption on hydrotalcites10.1021/acs.jced.0c00340 ↗
40. Intercalation behavior of carboxylic acids and their sodium salts with layered double hydroxide in methanol
41. How pigment volume concentration (PVC) and particle connectivity affect leaching of corrosion inhibitive species from coatings10.1016/j.porgcoat.2019.05.008 ↗
42. Functional and smart coatings for corrosion protection: a review of recent advances10.1016/j.surfcoat.2014.06.031 ↗
43. Characterization of inhibitor release from Zn-Al-[V10 O28]6- hydrotalcite pigments and corrosion protection from hydrotalcite-pigmented epoxy coatings10.5006/1.3278468 ↗
44. Active protection coatings with layered double hydroxide nanocontainers of corrosion inhibitor10.1016/j.corsci.2009.10.020 ↗
45. Effect of the synthesis parameters of in situ grown Mg-Al LDHs on the filiform corrosion susceptibility of painted AA500510.1016/j.electacta.2021.138288 ↗
46. H.D. Van Der Weijde, H.N. McMurray, T. Watson, Packaging for Packaging Food Products, Coated Substrates and Coating System for Producing Said Packaging and Use of Said Packaging, WO2006/029842, 2006.