Abstract
Abstract Amorphous Cu66Zr34 alloy decomposes into Cu, ZrO2, and residual amorphous phase after oxidation, mainly due to differences between the oxygen affinity to Cu and Zr. A four-layer structure formed near the surface consisting of two oxidized layers, a transition region, and the matrix. The crystalline phases exhibited a gradient distribution along the thickness. The oxidized ribbons showed an adjustable temperature coefficient of electrical resistivity as a function of thickness. Near constant electrical resistivity (TCR ≈ 0) could be obtained with a thickness of 20 μm. Such transformation can be utilized for producing precision wires or thin-film chip resistors through oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Phase-change materials and chalcogenides · Surface Roughness and Optical Measurements
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Bulk metallic glass nanowire architecture for electrochemical applications10.1021/nn200033c ↗
2. Capillary flow of amorphous metal for high performance electrode10.1038/srep02185 ↗
3. The effect of oxidation on the corrosion resistance and mechanical properties of a Zr-based metallic glass10.1016/j.corsci.2011.06.032 ↗
4. Enhancement of oxidation resistance of the supercooled liquid in Cu-Zr-based metallic glass by forming an amorphous oxide layer with the high thermal stability10.1016/j.corsci.2012.09.018 ↗
5. Effect of thermal stability of the amorphous substrate on the amorphous oxide growth on Zr-Al-(Cu,Ni) metallic glass surfaces10.1016/j.corsci.2013.04.009 ↗
6. Structure and hardness evolution of the scale of a Zr-based metallic glass during oxidation10.1016/j.jnoncrysol.2012.11.018 ↗
7. Oxidation behavior of Cu60Zr30Ti10 bulk metallic glass10.1557/JMR.2005.0182 ↗
8. Oxidation behavior of an Zr53Ni23. 5Al23. 5 bulk metallic glass at 400–600°C10.1016/j.intermet.2007.05.006 ↗
9. Oxidation behavior of a Zr–Cu–Al–Ni amorphous alloy in air at 300–425 °C10.1016/S0966-9795(02)00163-2 ↗
10. Thermal stability of amorphous oxide in Al87Ni3Y10 metallic glass10.1016/j.corsci.2013.08.010 ↗
11. Oxidation of Zr-based metallic glasses and nanocrystalline alloys10.1016/j.msea.2006.02.316 ↗
12. Oxidation behavior of Zr56Co28Al16 bulk metallic glasses10.1016/j.corsci.2012.08.057 ↗
13. Air-oxidation of a Zr50Cu43Al7 bulk metallic glass at 400–500°C
14. Air oxidation of a Zr58Cu22Al12Fe8 bulk metallic glass at 350–550°C10.1016/j.jallcom.2008.10.133 ↗
15. Diffusion mechanism of Zr-based metallic glass during oxidation under dry air10.1016/j.intermet.2012.04.003 ↗
16. Multilayered scale formation during Zr-based metallic glass oxidation in the supercooled liquid region10.1016/j.corsci.2016.05.044 ↗
17. Effect of tetragonal ZrO2 on the catalytic activity of Ni/ZrO2 catalyst prepared from amorphous Ni-Zr alloys10.1016/j.catcom.2005.08.005 ↗
18. Composition dependence of the CO2 methanation activity of Ni/ZrO2 catalysts prepared from amorphous Ni-Zr alloy precursors10.1016/S0926-860X(97)00142-7 ↗
19. Hydrogen-induced decomposition of Cu-Zr binary amorphous metallic alloys10.1016/j.jallcom.2015.11.113 ↗
20. The oxidation of amorphous binary alloys in air10.1016/0010-938X(93)90308-4 ↗
21. Electronic structure of metallic glasses10.1016/0079-6425(83)90001-4 ↗
22. Origin of saturation effects in electron transport10.1103/PhysRevLett.40.1586 ↗
23. Resistivity in amorphous and disordered crystalline alloys10.1103/PhysRevLett.39.102 ↗
24. Experimental test of the extended Ziman theory, using free electron-like Ag-Cu based amorphous alloys10.1088/0305-4608/12/10/023 ↗
25. Hydrogenation of Pd-coated Zr–Cu–Ni–Al metallic glasses and quasicrystals10.1016/S0925-8388(02)01288-4 ↗
26. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20% Cr steels10.1016/j.corsci.2003.09.004 ↗
27. Oxidation and crystallization of an amorphous Zr60Al15Ni25 alloy10.1557/JMR.1996.0347 ↗
28. Barin · 1995
29. Oxidation resistance of the supercooled liquid in Cu50Zr50 and Cu46Zr46Al8 metallic glasses10.1557/jmr.2012.23 ↗
30. Oxidation behavior of Ti-Cu binary metallic glass10.1016/j.corsci.2015.07.027 ↗
31. Oxidation of Zr55Cu30Al10Ni5 bulk in the glassy state and super cooled liquid state10.1007/s00339-003-2470-4 ↗
32. Air oxidation of a Zr55Cu30Al10Ni5 bulk metallic glass at its super cooled liquid state10.1016/j.corsci.2014.02.007 ↗
33. The effect of surface morphology on the oxidation behavior of bulk metallic glass10.1016/j.corsci.2015.06.021 ↗
34. Observation of giant diffusivity along dislocation cores10.1126/science.1151771 ↗
35. Process of bulk metallic glass10.1002/adma.200902776 ↗
36. High temperature oxidation behavior of amorphous Zr-Ni alloys in air10.2320/matertrans1989.36.988 ↗
37. Birks · 2006
38. The hydrogen permeability of the Cu-Zr binary amorphous metallic membranes and the importance of thermal stability10.1016/j.memsci.2015.03.098 ↗
39. Activation of amorphous Cu-Zr alloys10.1016/0021-9517(87)90175-8 ↗
40. Methanol synthesis reaction over copper-Group IV metal amorphous alloys as catalyst precursor10.1016/0021-9517(85)90384-7 ↗
41. Electrical properties and structural defects of Ni-Cr thin film10.1016/0040-6090(86)90043-X ↗
42. Segregation phenomena in thin NiCr layers10.1016/0042-207X(83)90527-4 ↗
43. Low temperature heat capacity and electrical resistivity of the Ti40Zr25Cu12Ni3Be20 glass forming alloy10.1016/j.intermet.2016.05.010 ↗
44. Adjustment of temperature coefficient of resistance in NiCr/CuNi(Mn)/NiCr films10.1063/1.362531 ↗
45. Relationship between t-ZrO2 stability and the crystallization of a Zr-based bulk metallic glass during oxidation10.1016/j.intermet.2012.05.009 ↗
46. Influence of the crystalline structure of ZrO2 on the metallic properties of Pt in Pt/WO3–ZrO210.1023/A:1019050228894 ↗