High temperature oxidation behaviors of steels at initial stages in air
Source abstract
Abstract
The initial stage oxidation behaviors of commercial low carbon steel (LCS) and advanced high strength steel (AHSS) were comparatively studied at 1150 °C in air. Two reaction fronts were in situ observed during the oxidation of LCS, which was not found for AHSS. It was confirmed that the early detachment of LCS occurred after 30-s oxidation, however, the scale of AHSS maintained adherence due to the formation of a liquid phase. Besides, the scale thickness increased parabolically with oxidation time for both LCS and AHSS, with the estimated parabolic rate constants of 4.7 × 10 −6 µm 2/s and 4.9 × 10 −6 µm 2/s, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. Advanced high strength steels for automotive industry10.1016/S1644-9665(12)60197-6 ↗
2. Failure mode transition in AHSS resistance spot welds. Part I. Controlling factors10.1016/j.msea.2011.08.017 ↗
3. Development of 3rd generation AHSS with medium Mn content alloying compositions10.1016/j.msea.2012.11.113 ↗
4. Effect of chromium and water vapor of low carbon steel on oxidation behavior at 1050 °C10.1002/srin.201500429 ↗
5. Thickness dependent chemical and microstructural properties of DC reactive magnetron sputtered titanium nitride thin films on low carbon steel cross-section10.1016/j.jmrt.2018.02.010 ↗
6. Metallographic sample preparation and characterisation of oxide scales on hot-rolled steel strips10.1017/S143192761501212X ↗
7. Review of the high-temperature oxidation of iron and carbon steels in air or10.1023/A:1023685905159 ↗
8. High temperature oxide scale characteristics of low carbon steel in hot rolling10.1016/j.jmatprotec.2004.04.167 ↗
9. The effect of scaling on interfacial friction in hot rolling of steels10.1016/S0924-0136(98)00392-6 ↗
10. Growth rate and phase composition of oxide scales during hot rolling of low carbon steel10.2355/isijinternational.44.1554 ↗
11. Prevention of red scale formation during hot rolling of steels10.2355/isijinternational.35.886 ↗
12. Effects of hot rolling and descaling condition on red scale defects formation10.2355/tetsutohagane1955.80.11_849 ↗
13. Effect of S in steel on hydraulic-descaling-ability in Si-added hot-rolled steel sheets10.2355/tetsutohagane1955.81.5_559 ↗
14. Effect of small amount of Ni on hydranlic-descaling-ability in Si-added hot-rolled steel sheets10.2355/tetsutohagane1955.82.1_63 ↗
15. Effect of temperature sequence during hot strip rolling on structure and properties of mild steels10.1002/srin.199301043 ↗
16. Oxidation of low-carbon, low-silicon mild steel at 450–900°C under conditions relevant to hot-strip processing10.1023/A:1013390628475 ↗
17. Ridge-buckle defect in thin-rolled steel strip
18. Effect of annealing atmosphere on scale formation and pickling performance of 410 SS10.1023/A:1027316918546 ↗
19. Characterization and properties of oxide scales on hot-rolled strips10.1016/j.msea.2006.10.151 ↗
20. Effect of sandblasting and subsequent acid pickling and passivation on the microstructure and corrosion behavior of 316L stainless steel10.1016/j.matdes.2015.08.113 ↗
21. The thermal and metallurgical state of steel strip during hot rolling: part III. Microstructural evolution10.1007/BF02656802 ↗
22. Influence of oxidation temperature and Cr content on the adhesion and microstructure of scale on low Cr steels10.1007/s11085-009-9167-9 ↗
23. Effects of initial scale structure on transformation behavior of wüstite10.2355/isijinternational.52.105 ↗
24. Effects of Si and its content on the scale formation on hot-rolled steel strips10.1016/j.matchemphys.2008.06.021 ↗
25. Effects of Si, Mn contents on the descalability behavior of the scale of annealed austenitic stainless steels10.2355/tetsutohagane1955.90.7_487 ↗
26. Evolution of near-surface internal and external oxide morphology during high-temperature selective oxidation of steels10.1007/s11837-018-2885-1 ↗
27. Challenges in hot-dip galvanizing of high strength dual phase steel: surface selective oxidation and mechanical property degradation10.1016/j.surfcoat.2012.02.001 ↗
28. Kinetics of internal oxidation of Mn-steel alloys10.1007/s11085-014-9490-7 ↗
29. Selective oxidation of TWIP steel during continuous annealing10.1002/srin.201100296 ↗
30. Galvanizability of advanced high-strength steels 1180TRIP and 1180CP10.1007/s11661-009-9880-7 ↗
31. Surface selective oxidation of Sn-added CMnSi TRIP steel10.1007/s11661-016-3331-z ↗
32. Effects of dew point on selective oxidation of TRIP steels containing Si, Mn, and B10.1007/s12540-011-0411-x ↗
33. Descaling ability of low-alloy steel wires depending on composition and rolling process10.1016/j.corsci.2009.12.028 ↗
34. Contributions to the data on theoretical metallurgy. XII
35. Patnaik · 2003
36. Young · 2016
37. High-temperature oxidation of sintered austenitic stainless steel containing boron or yttria10.1016/j.corsci.2017.09.002 ↗
38. Silicon enhances high temperature oxidation resistance of SIMP steel at 700 °C10.1016/j.corsci.2020.108519 ↗
39. In situ observations of early oxide formation in steel under hot-rolling conditions10.1111/j.1365-2818.2007.01726.x ↗
40. Coalescence of wustite grains during iron oxidation in a hot-stage environmental SEM10.1007/BF00667058 ↗
41. High temperature oxidation of iron at 1200 °C in a hot-stage environmental scanning electron microscope10.1007/BF02647106 ↗
42. In situ observation of whiskers, pyramids and pits during the high-temperature oxidation of metals10.1007/BF00659470 ↗
43. In situ observation of reaction fronts during the initial stages of iron surface oxidation at 1150 °C10.1007/s11085-020-09965-8 ↗
44. Thermodynamics and phase diagram of the Fe-C system10.1007/BF02680585 ↗
45. Theory of thermal grooving10.1063/1.1722742 ↗
46. Determination of free energy of δ-ferrite/γ-austenite interphase boundary of low carbon steels by in-situ observation10.2355/isijinternational.38.794 ↗
47. Morphological instability of δ-ferrite/γ-austenite interphase boundary in low carbon steels10.1016/S1359-6454(99)00022-1 ↗
48. A study of nonisothermal austenite formation and decomposition in Fe-C-Mn alloys10.1007/s11661-006-0122-y ↗
49. Compositional effects on the creep ductility of a low alloy steel10.1007/BF02655098 ↗
50. Effect of silicon in dual phase steel on the alloy reaction in continuous hot-dip galvanizing and galvannealing10.2355/isijinternational.54.2380 ↗
51. Influence of silicon, aluminium, phosphorus and boron on hot ductility of transformation induced plasticity assisted steels10.1179/174328413X13789824293948 ↗
52. The kinetics of the air oxidation of iron in the range 700–1250°C10.1016/0001-6160(58)90006-3 ↗
53. A study of the scale structure of hot-rolled steel strip by simulated coiling and cooling10.1023/A:1004637127231 ↗
54. Principles of metal oxidation10.1179/cmq.1971.10.3.149 ↗
55. Theorie der geordneten Mischphasen. III: Fehlordnungserscheinungen in polaren Verbindungen als Grundlage für Ionen-und Elektronenleitung10.1515/zpch-1933-2213 ↗
56. The effect of oxygen concentration on the oxidation of low-carbon steel in the temperature range 1000 to 1250°C10.1007/BF01048639 ↗
57. Scale growth during re-heating cycles10.1002/maco.19700211110 ↗
58. Oxidation of ultra low carbon and silicon bearing steels10.1016/j.corsci.2010.02.001 ↗
59. The Fe-O (iron-oxygen) system10.1007/BF02645713 ↗
60. The structure of magnetite10.1107/S0567740881004597 ↗
61. Cornell · 2003
62. Stress effects in high temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
63. On the formation of porosity and microchannels in growing scales10.1007/BF00657061 ↗
64. Pelton · 2018
65. Holman · 1986
66. Oxidation properties of transition metals10.1016/0079-6786(75)90003-5 ↗
67. Mehrer · 2007
68. The self diffusion of iron in Fe2SiO4 and CaFeSiO4 melts10.1007/BF02913568 ↗