Abstract This study focuses on the temperature capability of CoWO4 as the oxidation protection layer of ferritic stainless steel (FSS). The thermogravimetric-differential thermal analysis revealed that until CoWO4 started to melt at 1297 °C, little mass change was observed. In addition, the coefficient of thermal expansion of CoWO4 was 11.5 ± 0.2 (×10−6 K−1), which was similar to that of FSS, evidencing its good thermal stability and compatibility for the protection of FSS. The oxidation test of the Co–W coated specimens at 700 °C – 1000 °C in air confirmed effectiveness of the CoWO4 layer at T ≤ 850 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Thermal Expansion and Ionic Conductivity · Advancements in Solid Oxide Fuel Cells
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Development of design rules in the AISC Design Guide for structural stainless steel10.1016/j.tws.2014.02.007 ↗
2. Ferritic stainless steels in structural applications10.1016/j.tws.2014.03.014 ↗
3. High temperature oxidation of ferritic stainless steels10.2355/tetsutohagane1955.70.11_1541 ↗
4. Evaporation of Cr2O3 in atmospheres containing H2O10.1023/A:1023671206976 ↗
5. High-temperature oxidation of Fe-Cr alloys in wet oxygen10.1007/BF01670507 ↗
6. Breakaway oxidation behaviour of ferritic stainless steels at 1150 ºC in humid air10.1016/j.corsci.2016.02.042 ↗
7. Cr-poisoning of a LaNi0.6Fe0.4O3 cathode under current load10.1016/j.jpowsour.2012.02.083 ↗
8. Cr-poisoning in (La,Sr)(Co,Fe)O3 cathodes after 10,000 h SOFC stack testing10.1016/j.jpowsour.2012.03.045 ↗
9. Oxidation of an austenitic stainless steel with or without alloyed aluminum in O2+ 10% H2O environment at 800 °C10.1016/j.corsci.2017.03.015 ↗
10. Electrical and microstructural characterization of spinel phases as potential coatings for SOFC metallic interconnects10.1016/j.jpowsour.2005.03.137 ↗
11. Spinel coatings for UNS 430 stainless steel interconnects10.1016/j.surfcoat.2006.10.011 ↗
12. Thermal expansion and electrical conductivity of Fe and Cu doped MnCo2O4 spinel10.1016/j.ssi.2018.09.018 ↗
13. The effect of manganese additions on the reactive evaporation of chromium in Ni–Cr alloys10.1016/j.scriptamat.2006.01.026 ↗
14. High temperature oxidation of Co–W electroplated type 430 stainless steel for the interconnect of solid oxide fuel cells10.1016/j.corsci.2018.02.026 ↗
15. Microstructure and diffusion behavior in the multilayered oxides formed on a Co–W electroplated ferritic stainless steel followed by oxidation treatment10.1016/j.actamat.2020.04.048 ↗
16. A diffusion barrier for flexible thin film photovoltaics10.1149/2.045303jes ↗
17. Effect of W content on the oxidation and electrical behaviors of Co–W coatings for sofc interconnects fabricated by electrodeposition10.2320/matertrans.MT-M2019319 ↗
18. 2019
19. High temperature reactions of WC-Co nanopowders in various atmospheres, 15th International Plansee Seminar
20. Reactivity in the solid state between CoWO4 and RE2WO6 where RE = Sm, Eu, Gd10.1016/j.tca.2006.05.002 ↗
21. Anisotropy of thermal expansion of 3Y-TZP, α-Al2O3 and composites from 3Y-TZP/α-Al2O3 system10.1016/j.acme.2017.06.008 ↗
22. Chromium sesquioxide (Cr2O3): thermal expansion, density, melting point
23. Metallic interconnects for solid oxide fuel cells10.1016/j.msea.2005.02.047 ↗
24. Temperature dependence of corrosion of ferritic stainless steel in dual atmosphere at 600–800 ºC10.1016/j.jpowsour.2018.04.088 ↗
25. Growth and characterization of α-Fe2O3 nanowires10.1063/1.2776222 ↗
26. Rapid formation of the sigma phase in 304 stainless steel during friction stir welding10.1016/j.scriptamat.2003.08.022 ↗
27. High temperature oxidation behaviour of ferritic stainless steel SUS 430 in humid air10.1007/s12540-015-4168-5 ↗
28. Simultaneous oxidation and sigma-phase formation in a stainless steel10.1007/s11661-999-0324-1 ↗
29. Cracking and spalling of protective oxide layers10.1016/0921-5093(89)90731-4 ↗
30. Chromium vaporization of bare and of coated iron–chromium alloys at 1073 K10.1016/j.ssi.2006.12.010 ↗
31. The effect of temperature on chromium vaporization and oxide scale growth on interconnect steels for solid oxide fuel cells10.1016/j.jpowsour.2015.04.040 ↗
32. Equilibrium oxygen pressure of (Co3O4 + CoO) from 1173 to 1228 K10.1016/0021-9614(86)90095-9 ↗
33. Standard enthalpy of reaction for the reduction of Co3O4 to CoO10.1016/j.tca.2017.03.011 ↗
34. Patnaik · 2001
35. The sigma phase