journal article·2021-07

The high temperature wetting and corrosion mechanism analysis of Nb by TiAl alloy melt

Xianjun Lei, Xiaopeng Wang, Fantao Kong, Yuyong Chen

Corrosion Science· Volume 186
Publisher page

Abstract

Abstract High temperature corrosion behavior of Nb containing a TiAl melt is studied connecting with grain boundary wetting (GBW). Three intermetallic compounds (IMC) layers are formed and corroded step by step via the TiAl melt. The interfacial morphology and wetting angle evolution are investigated theoretically and experimentally. The morphology of the grooves controlled by interfacial tension, while nonzero wetting angles θd controlled by surface diffusion are established at the roots. By quantitative assessment, when θd is more than 140°, the grooves terminating on a thin sheet, which is responsible for the effective inhibition of further wetting and corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · nanoparticles nucleation surface interactions · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (90)

Show source-provided references
1. Impurity effects on the intergranular liquid bismuth penetration in polycrystalline nickel10.1016/j.actamat.2011.09.034 ↗
2. Grain boundary penetration of nickel by liquid bismuth as a film of nanometric thickness10.1016/S1359-6462(00)00518-2 ↗
3. Improvement of oxidation resistance of γ-TiAl at 900 and 1000 °C through hot-dip aluminizing10.1007/s11085-009-9187-5 ↗
4. Adhesive bonding in microelectronics and photonics10.1063/1.1467950 ↗
5. Effect of CuO content on the wetting behavior and mechanical properties of a Ag-CuO braze for ceramic joining10.1111/j.1551-2916.2005.00492.x ↗
6. Extremely rapid grain growth in scallop-type Cu6Sn5 during solid-liquid interdiffusion reactions in micro-bump solder joints10.1016/j.scriptamat.2020.01.005 ↗
7. Crystal-melt interfaces and solidification morphologies in metals and alloys10.1557/mrs2004.263 ↗
8. The influence of order on the nucleation barrier10.1557/mrs2004.264 ↗
9. Interfacial phenomena and microstructure evolution during solidification of binary and ternary Al-Mg-Si alloys cast with titanium carbonitride10.1016/S0921-5093(01)01485-X ↗
10. Synthesis of Al2O3-Al composites by reactive metal penetration10.1111/j.1151-2916.1996.tb07876.x ↗
11. The wetting and spontaneous infiltration of ceramics by molten copper10.1023/A:1004714407371 ↗
12. Microstructure and mechanical properties of chromium and chromium/nickel particulate reinforced alumina ceramics10.1023/A:1021000318894 ↗
13. Interface interaction in the (B4C+TiB2)/Cu system10.1007/s10853-006-0436-6 ↗
14. Interpenetrating Al2O3-TiAl3 alloys produced by reactive infiltration10.1016/S0955-2219(99)00133-8 ↗
15. Synthesis of damage-tolerant Cu-matrix composites with nacre-inspired laminate-reticular hierarchical architecture via tuning compositional wettability10.1016/j.scriptamat.2020.05.029 ↗
16. Hot corrosion behavior and wettability of calcium-magnesium-alumina-silicate (CMAS) on LaTi2Al9O19 ceramic10.1016/j.corsci.2019.108199 ↗
17. Slag corrosion-resistance mechanism of lightweight magnesia-based refractories under a static magnetic field10.1016/j.corsci.2020.108517 ↗
18. Analytical Solution on the transient corrosion/precipitation in non-isothermal liquid lead bismuth eutectic flow loops10.5006/1.3287739 ↗
19. Corrosion mechanisms of steel and cast Iron by molten aluminum10.1007/s11661-010-0306-3 ↗
20. Reactive wetting in metal/metal systems: dissolutive versus compound-forming systems10.1016/j.msea.2007.11.097 ↗
21. A diffuse-interface model of reactive wetting with intermetallic formation10.1016/j.actamat.2012.03.047 ↗
22. Kinetics of reactive wetting10.1016/S1359-6462(00)00298-0 ↗
23. Diffusion-limited reactive wetting: study of spreading kinetics of Cu-Cr alloys on carbon substrates10.1016/S1359-6454(99)00008-7 ↗
24. Kinetics of diffusion-limited spreading of sessile drops in reactive wetting10.1016/S1359-6462(96)00431-9 ↗
25. Grain boundary diffusion and wetting in the analysis of intergranular penetration10.1016/j.msea.2007.10.107 ↗
26. Discontinuous penetration of liquid Ga into grain boundaries of Al polycrystals10.1016/j.actamat.2003.09.017 ↗
27. The role of a bilayer interfacial phase on liquid metal embrittlement10.1126/science.1208774 ↗
28. Mechanism of liquid Bi penetration along Cu grain boundaries10.1016/S1359-6462(00)00351-1 ↗
29. Wetting: statics and dynamics10.1016/S1359-0294(97)80039-8 ↗
30. Dissolutive wetting in the Bi-Sn system10.1016/j.actamat.2006.03.032 ↗
31. Wetting and spreading in the Cu-Ag system10.1016/0001-6160(81)90128-0 ↗
32. Rapid penetration of liquid Bi along Cu grain boundaries10.1016/S1359-6462(98)00230-9 ↗
33. The role of liquid-substrate interactions on wetting in metallic embedded atom method systems10.1016/S1359-6454(00)00274-3 ↗
34. The flow of liquid metals on metal surfaces and its relation to soldering, brazing, and hot-dip coating
35. Wetting under chemical equilibrium and nonequilibrium conditions10.1021/j100605a009 ↗
36. The wettability of solids by liquid metals10.1016/B978-0-12-571814-1.50011-7 ↗
37. Nakae · 1997 · 29
38. Dynamics of wetting in reactive metal/ceramic systems: linear spreading10.1016/S1359-6454(96)00052-3 ↗
39. Wetting in the Au-Sn system10.1016/j.actamat.2004.02.033 ↗
40. Phase-field modeling of reactive wetting and growth of the intermetallic Al2Au phase in the Al-Au system10.1016/j.actamat.2017.12.015 ↗
41. The role of intermetallics in wetting in metallic systems10.1016/S1359-6462(01)01181-2 ↗
42. Dynamics of wetting in reactive metal/ceramic systems
43. Theory of thermal grooving10.1063/1.1722742 ↗
44. Instability of grain boundary grooves due to equilibrium grain boundary diffusion10.1016/0956-7151(91)90132-K ↗
45. On the kinetic mechanism of grain boundary wetting in metals10.1063/1.369659 ↗
46. The Al-B-Nb-Ti system: IV. Experimental study and thermodynamic re-evaluation of the binary Al-Nb and ternary Al-Nb-Ti systems10.1016/j.jallcom.2008.05.008 ↗
47. Thermodynamic description of the systems Co-Nb, Al-Nb and Co-Al-Nb10.1016/j.jallcom.2015.02.182 ↗
48. Direct synthesis of Nb-Al intermetallic nanoparticles by sodiothermic homogeneous reduction in molten salts10.1016/j.intermet.2013.07.005 ↗
49. Synthesis and characterization of mechanically alloyed Nb3Al-base alloys10.1016/S0921-5093(97)00624-2 ↗
50. Microstructure evolution and mechanical properties of diffusion bonding high Nb containing TiAl alloy to Ti2AlNb alloy10.1016/j.vacuum.2019.03.010 ↗
51. Synthesis of TiAl/Nb composites with concurrently enhanced strength and plasticity by powder metallurgy10.1016/j.msea.2020.139997 ↗
52. Evaluation of refractory intermetallics with A15 structure for high temperature structural applications10.1016/0921-5093(92)90228-S ↗
53. The wetting transition in high and low energy grain boundaries in the Cu(In) system10.1016/0956-7151(92)90070-U ↗
54. Interfacial reaction in Cu/Sn/Cu system during the transient liquid phase soldering process10.1016/j.actamat.2010.10.053 ↗
55. Direct evidence for a Cu-enriched region at the boundary between Cu6Sn5 and Cu3Sn during Cu/Sn reaction10.1016/j.scriptamat.2010.04.011 ↗
56. Early stages of intermetallic compound formation and growth during lead-free soldering10.1016/j.actamat.2010.05.028 ↗
57. Three-dimensional simulation of intermetallic compound layer growth in a binary alloy system10.1016/j.actamat.2008.11.006 ↗
58. Phase field simulations of morphological evolution and growth kinetics of solder reaction products10.1007/s11664-006-0184-z ↗
59. Phase field simulations of intermetallic compound growth during soldering reactions10.1007/s11664-004-0118-6 ↗
60. Premelting transition on 38°〈100〉 tilt grain boundaries in (Fe-10at.%Si)-Zn alloys10.1016/0956-7151(92)90021-6 ↗
61. Wetting transition on grain boundaries in Al contacting with a Sn-rich melt10.1007/BF00207014 ↗
62. Pressure influence on the grain boundary wetting phase transition in Fe-Si alloys10.1016/S1359-6454(96)00332-1 ↗
63. Diffusion-induced grain boundary porosity in NiAl10.1016/S1359-6462(00)00324-9 ↗
64. II-Mean Curvature and Weighted Mean Curvature10.1016/0956-7151(92)90091-R ↗
65. Role of the solid/liquid interface faceting in rapid penetration of a liquid phase along grain boundaries10.1016/S1359-6454(01)00039-8 ↗
66. The kinetics of cellular segregation reactions10.1016/0001-6160(59)90164-6 ↗
67. Equilibrium shapes of FCC metallic crystals in liquid alloys10.1016/0036-9748(80)90213-6 ↗
68. Penetration of tin and zinc along tilt grain boundaries 43° [100] in Fe-5at.%Si alloy: Premelting phase transition?10.1016/0956-7151(91)90131-J ↗
69. Grain boundary transitions in binary alloys10.1103/PhysRevLett.97.075502 ↗
70. On the mechanism of the binary Cu/Sn solder reaction10.1063/1.1852724 ↗
71. Initial rapid wetting in metallic systems10.1016/j.actamat.2013.05.026 ↗
72. The relation between wetting and interfacial chemistry in the CuAgTi/alumina system10.1016/j.actamat.2005.11.048 ↗
73. Fundamental issues of reactive wetting by liquid metals10.1007/s10853-009-4128-x ↗
74. Surface tensions in the system solid copper-molten lead10.1088/0370-1301/63/5/306 ↗
75. Kinetics of high-temperature spreading10.1016/j.cossms.2006.04.005 ↗
76. Triple line ridging and attachment in high-temperature wetting10.1016/S1359-6462(00)00549-2 ↗
77. Coherency strain energy as a driving force for liquid grooving at grain boundaries10.1016/S1359-6462(98)00229-2 ↗
78. In-Situ TEM observation of aluminum embrittlement by liquid gallium10.1016/S1359-6462(97)00464-8 ↗
79. Liquid grooving at grain boundaries10.1016/0921-5093(95)09830-5 ↗
80. Crack-like grain-boundary diffusion wedges in thin metal films10.1016/S1359-6454(99)00178-0 ↗
81. Spreading of Sn-Ag solders on FeNi alloys10.1016/S1359-6454(03)00140-X ↗
82. Wetting under chemical equilibrium and non-equilibrium conditions10.1021/j100605a009 ↗
83. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation: II. Experimental evidence and consequences10.1016/j.actamat.2007.05.033 ↗
84. Measurements of Adsorption at the air-water interface by the microtome method
85. Defay · 1966
86. The shape of intergranular creep cracks growing by surface diffusion10.1016/0001-6160(73)90105-3 ↗
87. High temperature strength of niobium aluminide intermetallics10.1016/0921-5093(92)90227-R ↗
88. In situ investigation of liquid Ga penetration in Al bicrystal grain boundaries: grain boundary wetting or liquid metal embrittlement?10.1016/j.actamat.2004.09.012 ↗
89. Atomic dynamics and Marangoni films during liquid-metal spreading10.1038/nmat1252 ↗
90. Stability of a planar interface during solidification of dilute binary alloy10.1063/1.1713333 ↗