Effects of sulphate deposits on corrosion behaviour of Ni-base alloys in wet CO2 gas at 750 °C
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Research and development of heat-resistant materials for advanced USC power plants with steam temperatures of 700 °C and above10.15302/J-ENG-2015031 ↗
2. Future directions in the field of high-temperature corrosion research10.1007/s11085-017-9719-3 ↗
3. Impact of iron and chromium on coal ash corrosion behavior of Ni-Cr-Co based alloy for advanced ultra-supercritical power plants10.5006/2998 ↗
4. Phenomenological and microstructural analysis of intermediate temperatures creep in a Ni-Fe-based alloy for advanced ultra-supercritical fossil power plants10.1016/j.actamat.2015.09.006 ↗
5. U.S. Program on materials technology for ultra-supercritical coal power plants10.1007/s11665-013-0717-6 ↗
6. Phase investigations under steam oxidation process at 800 °C for 1000 h of advanced steels and Ni-based alloys10.1007/s11085-016-9662-8 ↗
7. Oxidation behaviour of cast Ni-Cr alloys in steam at 800 °C10.1179/1743284712Y.0000000103 ↗
8. Effect of surface condition on steam oxidation of martensitic steels and nickel-based alloys10.5006/1859 ↗
9. Corrosion behavior of candidate heat exchanger materials in oxidizing and reducing gases relevant to oxyfuel power plants10.1080/09603409.2017.1392113 ↗
10. High-temperature performance of ferritic steels in fireside corrosion regimes: temperature and deposits10.1007/s11665-016-2423-7 ↗
11. Microscopy of fireside corrosion on superheater materials for oxy-fired pulverised fuel power plants10.3184/096034012X13323635669332 ↗
12. Mechanism of Na2SO4 induced corrosion at 600°–900°C10.1149/1.2129375 ↗
13. Hot corrosion of metals and alloys10.1007/s11085-011-9254-6 ↗
14. Fireside corrosion of superheaters: Effects of air and oxy-firing of coal and biomass10.1016/j.fuel.2011.03.010 ↗
15. Fireside corrosion degradation of 15Mo3, T22, T23 & T91 in simulated coal-biomass co-fired environment10.1002/maco.201407886 ↗
16. Laboratory-simulated fuel-ash corrosion of superheater tubes in coal-fired ultra-supercritical-boilers10.1002/1521-4176(200011)51:11<786::AID-MACO786>3.0.CO;2-M ↗
17. Fireside corrosion during oxyfuel combustion considering various SO2 contents10.1016/j.egypro.2014.07.015 ↗
18. Effect of coal ash on the performance of alloys in simulated oxy-fuel environments10.1016/j.fuel.2013.09.021 ↗
19. Nickel-base superalloys for ultra-supercritical coal-fired power plants: Fireside corrosion. Laboratory studies and power plant exposures10.1016/j.fuel.2012.11.081 ↗
20. Failure of Alloy 625 tube stub ends - Effect of primary nitrides10.1016/j.engfailanal.2013.03.018 ↗
21. Effects of sulphate deposits on corrosion behaviour of Fe-base alloys in wet CO2 gas at 750 °C
22. Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2-20H2O gas at 700 °C10.1016/j.corsci.2020.108702 ↗
23. Effects of water vapour on the oxidation of a nickel-base 625 alloy between 900 and 1,100 °C10.1007/s10853-011-5544-2 ↗
24. Sub-scale depletion and enrichment processes during high temperature oxidation of the nickel base alloy 625 in the temperature range 900-1000 °C10.1007/s11085-010-9225-3 ↗
25. Microstructure and mechanical properties of Inconel 625 superalloy10.1016/S0022-3115(00)00723-6 ↗
26. Scale formation of alloy 602 CA during isothermal oxidation at 800-1100 °C in different types of water vapor containing atmospheres10.1007/s11085-015-9595-7 ↗
27. Reaktionstypen bei der oxydation von legierungen
28. The transition from internal to external oxidation and the formation of interruption bands in silver-indium alloys10.1016/0001-6160(61)90103-1 ↗
29. Determination of diffusion coefficient of oxygen in α-iron from internal oxidation measurements in Fe-Si alloys10.1007/BF00547959 ↗
30. Tracer diffusion in the chromium-nickel system10.1002/pssa.2210080230 ↗
31. The diffusion and solubility of oxygen in solid nickel10.1007/BF02646220 ↗
32. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
33. Corrosion behaviour of Ni-Cr alloys in wet CO2 atmosphere at 700 and 800 °C10.1016/j.corsci.2018.10.029 ↗
34. Temperature effect on oxidation behavior of Ni-Cr Alloys in CO2 gas atmosphere10.1149/2.1021706jes ↗
35. Impurity diffusion of Al in Ni single crystals studied by secondary ion mass spectrometry (SIMS)10.1002/pssa.2210640120 ↗
36. Growth and microstructure of α-Al2O3 on Ni-Al alloys: internal precipitation and transition to external scale10.1149/1.2129964 ↗
37. Effects of slicon on high temperature corrosion of Fe-Cr and Fe-Cr-Ni alloys in carbon dioxide10.1007/s11085-013-9467-y ↗
38. Effects of silicon and water vapour on corrosion of Fe-20Cr and Fe-20Cr-20Ni alloys in CO2 at 650 °C10.1007/s11085-016-9681-5 ↗
39. Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2 at 700 °C10.1016/j.corsci.2017.11.005 ↗
40. Diffusion of magnesium, silicon, and molybdenum in nickel10.1007/BF03397944 ↗
41. The effect of silicon and manganese on the oxidation mechanism of Ni-20 Cr10.1007/BF00603657 ↗
42. Mechanisms of hot corrosion of pure nickel at 700°C: influence of testing conditions10.1016/j.corsci.2018.06.009 ↗
43. On the hot corrosion of nickel at 700 °C10.1007/s11085-015-9588-6 ↗
44. The high temperature corrosion of metals in sulfidizing-oxidizing environments: a critical review10.1515/HTMP.1989.8.3.149 ↗
45. Na2SO4-deposit-induced corrosion of Mo-containing alloys10.1007/s11085-017-9746-0 ↗
46. Chemical reactions involved in the initiation of hot corrosion of B-1900 and NASA-TRW VIA10.1149/1.2123928 ↗