The characterization of oxide scales formed on ferritic-martensitic steel in supercritical water with dissolved oxygen
Source abstract
Abstract
Abstract The oxidation behaviour of ferritic-martensitic steel in supercritical water has been studied at 600−700 °C and 25 MPa. Exposure tests as functions of temperature, time and distance from the leading edge of the specimen provide evidence that hydrogen influence the surface morphology and oxide phase. Hematite is apt to develop on the top of the magnetite at a lower temperature, prolonged time, and smaller distance from the leading edge of the specimen. By the consideration of convective mass transfer, diffusive mass transport and oxidation rate, a model has been proposed to calculate the partial pressure of hydrogen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Influence of temperature on the oxidation behaviour of a ferritic-martensitic steel in supercritical water10.1016/j.corsci.2016.10.020 ↗
2. Ferritic/martensitic steels for next-generation reactors10.1016/j.jnucmat.2007.05.005 ↗
3. Corrosion behavior of ferritic/martensitic steel P92 in supercritical water10.1016/j.supflu.2009.06.019 ↗
4. Corrosion behavior of ferritic-martensitic steel T91 in supercritical water10.1016/j.corsci.2005.08.021 ↗
5. Oxidation behaviour of ferritic-martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
6. Corrosion behavior of a ferritic/martensitic steel HCM12A exposed to harsh environments10.1016/j.jnucmat.2007.05.001 ↗
7. Temperature dependence of oxidation behaviour of a ferritic-martensitic steel in supercritical water at 600-700° C10.1007/s11085-016-9647-7 ↗
8. The role of dissolved oxygen in supercritical water in the oxidation of ferritic-martensitic steel10.1016/j.supflu.2015.10.017 ↗
9. Oxidation of ferritic and ferritic-martensitic steels in flowing and static supercritical water10.1016/j.corsci.2015.10.017 ↗
10. Corrosion behavior of 9-12% Cr ferritic-martensitic steels in supercritical water10.1016/j.corsci.2009.12.032 ↗
11. Investigation on early formation and evolution of oxide scales on ferritic-martensitic steels in supercritical water10.1016/j.corsci.2018.02.036 ↗
12. Oxidation of austenitic and ferritic/martensitic alloys in supercritical water10.1016/j.supflu.2013.03.014 ↗
13. Corrosion of ferritic-martensitic steels in steam and supercritical water10.1016/j.jnucmat.2012.09.037 ↗
14. Effect of ultrasonic impact peening on the corrosion of ferritic-martensitic steels in supercritical water10.1016/j.jnucmat.2014.11.028 ↗
15. Role of dissolved oxygen in iron oxidation in supercritical water: insights from reactive dynamics simulations10.1021/acs.jpcc.9b01936 ↗
16. Effect of steam flow rate and sample orientation on steam oxidation of ferritic and austenitic steels at 650 and 700 C10.1007/s11085-013-9358-2 ↗
17. Hydrogen effects on oxidation behaviors of Haynes 230 in high temperature steam environments10.1016/j.ssi.2013.04.010 ↗
18. Improvement in steam oxidation resistance of Fe-10% Cr-0.08% C steel by suppressing hydrogen dissolution10.1016/j.corsci.2006.01.008 ↗
19. The effects of water vapor and hydrogen on the high-temperature oxidation of alloys10.1007/s11085-012-9349-8 ↗
20. The location of hydrogen in the kinetics of oxidation of ferrous alloys by superheated steam10.1007/BF00656353 ↗
21. Corrosion and carburization behavior of heat-resistant steels in a high-temperature supercritical carbon dioxide environment10.1007/s11085-019-09917-x ↗
22. Hydrogen emission during the steam oxidation of ferritic steels: kinetics and mechanism10.1016/0010-938X(89)90086-3 ↗
23. Quantification of aluminum outward diffusion during oxidation of FeCrAl alloys10.1007/s11085-005-4391-4 ↗
24. The role of oxide microstructure and growth stresses in the high-temperature scaling of nickel
25. Effects of exposure temperature and time on corrosion behavior of a ferritic-martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
26. The effect of water-vapor content and gas flow rate on the oxidation mechanism of a 10% Cr-ferritic steel in Ar-H2O mixtures10.1007/s11085-005-4394-1 ↗
27. Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water10.1016/j.supflu.2006.12.020 ↗
28. Hydrogen transport during steam oxidation of iron and nickel alloys
29. The characteristic of oxide scales on T91 tube after long-term service in an ultra-supercritical coal power plant10.1016/j.supflu.2012.08.015 ↗
30. Mayer · 1983 · 368
31. Hydrogen transport in stainless steels10.1016/0022-3115(84)90304-0 ↗
32. Hydrogen transport in austenitic stainless steel10.1016/0010-938X(75)90022-0 ↗
33. Effect of gas flow rate on oxidation behaviour of alloy 625 in wet air in the temperature range 900-1000 °C10.1002/maco.201608831 ↗
34. Short-time oxidation behavior of low-carbon, low-silicon steel in air at 850-1180 °C: II. Linear to parabolic transition determined using existing gas-phase transport and solid-phase diffusion theories10.1007/s11085-009-9180-z ↗