journal article·2020-07

Pitting of 2024 alloys prepared by spark plasma sintering using powders with different sizes

Yanbing Meng, Songmei Li, Jianhua Liu, Mei Yu, Wenming Tian, Mengjia Chen

Corrosion Science· Volume 170
Publisher page

Abstract

Abstract Correlation in microstructures of bulks and powders, pitting resistance and grain sizes for spark plasma sintered 2024 aluminum alloys has been studied. Results reveal the microstructures of bulk are resemble to powders. While the average grain sizes of bulks, which increase with raising powder size, are much smaller due to recrystallization. Corrosion in electrochemical tests increase with increasing grain size, suggesting a decreasing pitting resistance. Microscopy observation indicates pits initiate at intermetallic particles and the biggest depths range from 3.2 to 24.7 μm for A5 and A80. Mechanism analysis proves the stronger passivity of fine-grained samples enhances the corrosion resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Effect of processing on grain size and corrosion of AA2024-T310.5006/1.3647762 ↗
2. Impact of ultrafine-grained microstructure on the corrosion of aluminium alloy AA202410.1016/j.corsci.2011.12.016 ↗
3. Surface modifications of a cold rolled 2024 Al alloy by high current pulsed electron beams
4. Novel fabrication of bulk fine-grained Al-Cu-Mg alloy with superior mechanical properties10.1002/adem.201500450 ↗
5. Effect of grain size on corrosion of high purity aluminium10.1016/j.electacta.2010.09.023 ↗
6. A comparison of the corrosion behavior of nanocrystalline and conventional Al 5083 samples10.5006/1.3278260 ↗
7. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
8. Correlations between intergranular stress corrosion cracking, grain-boundary microchemistry, and grain-boundary electrochemistry for Al–Zn–Mg–Cu alloys10.1016/j.corsci.2010.08.024 ↗
9. Corrigendum to “Spreading of intergranular corrosion on the surface of sensitized Al-4.4 Mg alloys_ A general finding”10.1016/j.corsci.2012.02.018 ↗
10. Corrosion behaviour and mechanism of new aerospace Al–Zn–Mg alloy friction stir welded joints and the effects of secondary Al 3 Sc x Zr 1− x nanoparticles10.1016/j.corsci.2014.10.036 ↗
11. Intergranular corrosion of spark plasma sintering assembled bimodal grain sized AA7075 aluminum alloys10.1016/j.corsci.2016.02.034 ↗
12. Pitting corrosion of naturally aged AA 7075 aluminum alloys with bimodal grain size10.1016/j.corsci.2016.09.013 ↗
13. How complex is the microstructure of AA2024-T3?10.1016/j.corsci.2009.05.001 ↗
14. Investigation of the initiation of localized corrosion on aluminum alloys by using fluorescence microscopy10.1016/S0010-938X(00)00020-2 ↗
15. Role of intermetallic phases in localized corrosion of AA508310.1016/j.electacta.2006.12.072 ↗
16. Development of gradient microstructure in mild steel and grain size dependence of its electrochemical response10.1016/j.corsci.2018.04.009 ↗
17. Intergranular corrosion of cryorolled and aged D16 aluminum alloy10.1134/S2070205117060144 ↗
18. Intergranular corrosion resistance of Zn modified 5××× series Al alloy during retrogression and re-aging treatment10.1016/j.matchar.2018.07.008 ↗
19. Electrochemical study of the surface metal matrix composite developed on AA 2024-T351 by the friction stir process10.1080/1478422X.2019.1661569 ↗
20. Improving corrosion resistance of pure Al through ECAP10.1179/147842209X12559428167562 ↗
21. Effects of grain size on the corrosion resistance of pure magnesium by cooling rate-controlled solidification10.1007/s11706-015-0299-3 ↗
22. Effect of different grain sizes and textures on the corrosion behaviour of aluminum alloy AA608210.1002/mawe.201100829 ↗
23. Effects of secondary phase and grain size on the corrosion of biodegradable Mg-Zn-Ca alloys10.1016/j.msec.2014.12.049 ↗
24. Influence of grain size on the electrochemical behavior of pure copper10.1007/s10853-016-0445-z ↗
25. Enhanced corrosion resistance of 5083 aluminum alloy by refining with nano-CeB6/Al inoculant10.1016/j.apsusc.2019.03.283 ↗
26. Effect of laser shock peening on the microstructure and corrosion resistance in the surface of weld nugget zone and heat-affected zone of FSW joints of 7050 Al alloy10.1016/j.optlastec.2018.10.054 ↗
27. Interfacial microstructural and corrosion characterizations of friction stir welded AA6061-T6 and AISI304 materials10.1007/s12540-018-00222-x ↗
28. Comparative effect of grain size and texture on the corrosion behaviour of commercially pure titanium processed by equal channel angular pressing10.1016/j.corsci.2009.08.017 ↗
29. Corrosion behavior of ultra-fine grained industrial pure Al fabricated by ECAP10.1016/S1003-6326(08)60407-0 ↗
30. Influence of crystallographic texture and grain size on the corrosion behaviour of as-extruded Mg alloy AZ31 sheets10.1016/j.corsci.2017.08.004 ↗
31. Effect of surface passivation on corrosion resistance and antibacterial properties of Cu-bearing 316L stainless steel10.1016/j.apsusc.2016.06.036 ↗
32. Discharge and densification in the spark plasma sintering of quasicrystal particles10.1007/s10853-019-03489-6 ↗
33. Field-assisted sintering technology/spark plasma sintering: mechanisms, materials, and technology developments10.1002/adem.201300409 ↗
34. Structure and strength of aluminum with sub-micrometer/micrometer grain size prepared by spark plasma sintering10.1016/j.matdes.2013.01.018 ↗
35. Dynamic evolution of new grains in magnesium alloy AZ31 during hot deformation
36. Review grain and subgrain characterisation by electron backscatter diffraction10.1023/A:1017973432592 ↗
37. Field-assisted sintering technology / spark plasma sintering: mechanisms, materials, and technology development10.1002/adem.201300409 ↗
38. Localised corrosion initiation and microstructural characterisation of an Al 2024 alloy with a higher Cu to Mg ratio10.1016/j.corsci.2011.10.035 ↗
39. Role of intermetallic phases in localized corrosion of AA508310.1149/1.1764780 ↗
40. Corrosion of AA2024-T3 Part I: Localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
41. E. M · 2010
42. Cyclic polarization analysis of corrosion behavior of ceramic coating on 6061 Al/SiCp composite for marine applications10.1134/S2070205116050117 ↗
43. Interpretation of cyclic potentiodynamic polarization test results for study of corrosion behavior of metals: a review10.1134/S207020511805026X ↗
44. Passivity breakdown, pit initiation and propagation of pits in metallic materials – review10.1016/j.corsci.2014.10.006 ↗
45. Polyethyleneimine as a corrosion inhibitor for ASTM 420 stainless steel in near-neutral saline media10.1016/j.corsci.2008.12.006 ↗
46. Electrochemical and XPS study of polyethyleneimines of different molecular sizes as corrosion inhibitors for AISI 430 stainless steel in near-neutral chloride media10.1016/j.matchemphys.2009.03.010 ↗
47. Effects of applied potential on stable pitting of 304 stainless steel10.1016/j.corsci.2015.01.034 ↗
48. Investigation of pitting corrosion by potentiostatic polarization measurements
49. Pitting corrosion of Al2024-T3 in sodium chloride solution
50. A study of the corrosion of aluminum alloy 2024-T3 under thin electrolyte layers10.1016/j.corsci.2003.10.005 ↗
51. An impedance investigation of the mechanism of pure magnesium corrosion in sodium sulfate solutions10.1149/1.2401056 ↗
52. Influence of Mg and Ti on the microstructure and electrochemical performance of aluminum alloy sacrificial anodes10.1007/s12598-009-0037-z ↗
53. Characterization of pitting corrosion of 7A60 aluminum alloy by EN and EIS techniques10.1016/S1003-6326(14)63550-0 ↗
54. Corrosion mechanism of Al, Al–Zn and Al–Zn–Sn alloys in 3 wt.% NaCl solution10.1016/j.corsci.2014.07.018 ↗
55. Anodizing of 2024-T3 aluminum alloy in sulfuric-boric-phosphoric acids and its corrosion behavior10.1016/S1003-6326(13)62767-3 ↗
56. Enhanced graphical representation of electrochemical10.1149/1.2168377 ↗
57. The evaluation of experimental dielectric data of barrier coatings by means of different models10.1016/S0013-4686(01)00644-2 ↗
58. Impedance spectroscopy at interfaces of metals and aqueous solutions — surface roughness, CPE and related issues10.1016/j.ssi.2004.06.023 ↗
59. Impedance of porous Au based electrodes10.1016/j.jelechem.2004.01.008 ↗
60. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
61. The electrochemistry of intermetallic compounds: a mini-review10.1016/j.elecom.2017.05.008 ↗
62. Mechanism of pit nucleation by electrical breakdown of the passive film10.1016/S0010-938X(01)00113-5 ↗
63. Multi-state Markov modeling of pitting corrosion in stainless steel exposed to chloride-containing environment10.1016/j.ress.2017.12.015 ↗
64. In situ X-ray tomography of intergranular corrosion of 2024 and 7050 aluminium alloys10.1016/j.corsci.2010.08.026 ↗
65. Fatigue life of the strain hardened austenitic stainless steel in simulated pressurized water reactor primary water10.1115/1.4026521 ↗
66. Passive films on iron_ the mechanism of breakdown in chloride containing solutions10.1149/1.2115795 ↗
67. Intermetallic phases in aluminum alloys and their roles in localized corrosion10.1149/2.0931811jes ↗
68. Electrochemical behavior and localized corrosion associated with Al7Cu2Fe particles in aluminum alloy 7075-T65110.1016/j.corsci.2006.02.007 ↗
69. Self-regulation of the cathodic reaction kinetics during corrosion of AlCu alloys10.1149/1.1432669 ↗
70. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
71. Corrosion of AA2024-T3 Part II: Co-operative corrosion10.1016/j.corsci.2010.09.030 ↗
72. Effect of friction stir processing on pitting corrosion and intergranular attack of 7075 aluminum alloy10.1016/j.jmst.2016.07.008 ↗
73. Role of chemical composition in corrosion of aluminum alloys10.3390/met8080581 ↗