journal article·2019-07Open access

Study of the hydrogen uptake in deformed steel using the microcapillary cell technique

Berk Ozdirik, Thomas Suter, Ulrik Hans, Tom Depover, Kim Verbeken, Patrik Schmutz, Lars P.H. Jeurgens, Herman Terryn, Iris De Graeve

Corrosion Science· Volume 155

Abstract

Abstract The microcapillary cell electrochemical method is capable of evaluating hydrogen (H) uptake in steel with respect to deformation, which is induced by various mechanical methods (cold rolling, bending and punching). A clear relation between the deformation degree and the local H-content is established for dual phase (DP600) steel. The magnitude of the deformation nearby a punched edge is quantitatively determined using electron backscatter diffraction technique. A shear-affected zone is identified at the edge of the punched hole. The dedicated local electrochemical measurements confirm the presence of high concentrations of local-H in this shear affected zone, which is likely detrimental for H-embrittlement.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (78)

Show source-provided references
1. Hydrogen embrittlement of automotive advanced high-strength steels10.1007/s11661-012-1280-8 ↗
2. Equivalent hydrogen fugacity during electrochemical charging of 980DP steel determined by thermal desorption spectroscopy
3. Fractographic analysis of the role of hydrogen diffusion on the hydrogen embrittlement susceptibility of DP steel10.1016/j.msea.2015.09.124 ↗
4. Observation of hydrogen distribution in high-strength steel10.1023/A:1017568706014 ↗
5. Perspectives on hydrogen uptake, diffusion and trapping10.1016/j.ijhydene.2015.06.147 ↗
6. Hydrogen interaction with multiple traps: Can it be used to mitigate embrittlement10.1016/j.ijhydene.2011.05.027 ↗
7. Effect of hydrogen on the fracture behaviour of high strength 372 steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
8. Effect of hydrogen content on the embrittlement in a Fe-Mn-374 C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
9. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
10. Trap-governed hydrogen diffusivity and uptake capacity in ultrahigh-strength AERMET 100 steel10.1007/s11661-002-0032-6 ↗
11. The effect of straining on the transport of hydrogen in Iron, nickel, and stainless steel10.5006/1.3583831 ↗
12. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
13. Petit · 2003 · Vol. 6 · 65
14. Deep trapping states for hydrogen in deformed iron10.1016/0001-6160(80)90038-3 ↗
15. The detrimental effect of hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-C-X alloys: an experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
16. Spatially resolved localization of trapped hydrogen in zero to three dimensional defects inside ferritic steel10.1016/j.actamat.2017.10.066 ↗
17. Bulk forming of sheet metal10.1016/j.cirp.2012.05.007 ↗
18. Hydrogen embrittlement resistance evaluation of ultra-high strength steel sheets for automobiles”10.2355/isijinternational.52.316 ↗
19. The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys10.1016/j.corsci.2016.07.013 ↗
20. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗
21. Hydrogen trapping and hydrogen induced mechanical degradation in lab cast Fe-C-Cr alloys10.1016/j.msea.2016.05.018 ↗
22. Evaluation of the role of Mo2C in hydrogen induced ductility loss in Q&T Fe-C-Mo alloys10.1016/j.ijhydene.2016.05.176 ↗
23. Effect of Ti, Mo and Cr based precipitates on the hydrogen trapping and embrittlement of Fe-C-X Q&T alloys10.1016/j.ijhydene.2015.06.157 ↗
24. Influence of experimental parameters on thermal desorption spectroscopy measurements during evaluation of hydrogen trapping10.1016/j.jnucmat.2013.07.006 ↗
25. Spatially and kinetically resolved mapping of hydrogen in a twinning induced plasticity steel by use of scanning kelvin probe force microscopy10.1149/2.0131512jes ↗
26. Evaluation of hydrogen entry into high strength steel under atmospheric corrosion10.1016/j.corsci.2009.11.046 ↗
27. On the synergy of diffusible hydrogen content and hydrogen diffusivity in the mechanical degradation of laboratory cast Fe-C alloys10.1016/j.msea.2016.03.107 ↗
28. Influence of experimental parameters on thermal desorption spectroscopy measurements during evaluation of hydrogen trapping10.1016/j.jnucmat.2013.07.006 ↗
29. The adsorption and diffusion of electrolytic hydrogen in Palladium
30. Hydrogen trapping in high-strength steels
31. Hydrogen embrittlement susceptibility and permeability of two high strength steels10.1016/j.corsci.2005.05.042 ↗
32. Measurement of lattice and apparent diffusion coefficient of hydrogen in X65 and F22 pipeline steels10.1016/j.ijhydene.2012.11.059 ↗
33. Hydrogen permeation through deformed and heat-treated Armco pure iron10.1080/02670836.2017.1342015 ↗
34. Study on hydrogen absorption of pipeline steel under cathodic charging10.1016/j.corsci.2005.01.011 ↗
35. Comparative assessment of electrochemical hydrogen absorption by pipeline steels with different strength10.1016/j.corsci.2010.02.011 ↗
36. Electrochemical determination of hydrogen in steel
37. Development of an electrochemical procedure for monitoring hydrogen sorption/desorption in steel10.1149/2.0521713jes ↗
38. Analyses of hydrogen distribution around fatigue crack on type 304 stainless steel using secondary ion mass spectrometry10.1016/j.ijhydene.2011.03.111 ↗
39. Recent progress in microstructural hydrogen mapping in steels: quantification, kinetic analysis, and multi-scale characterization10.1080/02670836.2017.1299276 ↗
40. Houston TXProceedings of the 12th International Corrosion CongressVol. 3A1993
41. Electrochemical methods in corrosion research v
42. Microtechniques and nanotechniques to study localized corrosion10.1016/0013-4686(95)00072-M ↗
43. Microelectrodes for corrosion studies in microsystems10.1016/S0013-4686(01)00551-5 ↗
44. The use of the electrochemical micro-cell for the investigation of corrosion phenomena10.1016/j.electacta.2016.01.099 ↗
45. Neue Methoden Zur Analyse Von Diffusiblem Wasserstoff in hochfesten stählen10.3139/120.110483 ↗
46. Development of an in-situ measuring Cell to non-destructive, local measurement of diffusible hydrogen content in steels
47. Local dissolution of MnS inclusion and microstructural distribution of absorbed hydrogen in carbon steel10.1149/1.3611405 ↗
48. Hydrogen permeation into a carbon steel sheet observed by a micro-capillary combined with a devanathan-stachurski cell10.2355/isijinternational.ISIJINT-2015-191 ↗
49. Hydrogen embrittlement associated with strain localization in a precipitation-hardened FeMnAlC light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
50. Hydrogen environment embrittlement of stable austenitic steels
51. A review of strain analysis using electron backscatter diffraction10.1017/S1431927611000055 ↗
52. A review of advances and challenges in EBSD strain mapping
53. Mapping and assessing plastic deformation using EBSD
54. Quantification of large deformation with punching in dual phase steel and change of its microstructure –part 2: Local strain mapping of dual phase steel by a combination technique of electron backscatter diffraction and digital image correlation methods10.2355/isijinternational.ISIJINT-2016-310 ↗
55. Dislocation substructure as a function of strain in a dual-phase steel”10.1007/BF02644716 ↗
56. Microstructural and micromechanical effects of cold roll-forming on high strength dual phase steels10.1590/1516-1439.000314 ↗
57. ’A micro-level strain analysis of a high-strength dual-phase steel10.3139/146.110522 ↗
58. Influence of sheared edge on hydrogen embrittlement resistance in an ultra-high strength steel sheet10.2355/isijinternational.54.1416 ↗
59. Characterization of mechanically sheared edges of dual phase steels10.1016/j.jmatprotec.2012.01.006 ↗
60. Quantification of large deformation with punching in dual phase steel and change of its microstructure –part 1: proposal of quantification technique of the punching damage of the dual phase steel10.2355/isijinternational.ISIJINT-2016-312 ↗
61. Hydrogen embrittlement of DP-1000 flat steel sheet: influence of mechanical properties, specimen geometry, pre-damaging and electrolytically zinc galvanizing
62. Hydrogen embrittlement of high strength steel under in situ corrosive charging conditions and tensile load
63. Fractographic analysis of the role of hydrogen diffusion on the hydrogen embrittlement susceptibility of DP steel10.1016/j.msea.2015.09.124 ↗
64. Comparison of electrochemical and thermal evaluation of hydrogen uptake in steel alloys having different microstructures10.1149/2.0891811jes ↗
65. Application of the electrochemical microcapillary technique to study intergranular stress corrosion cracking of austenitic stainless steel on the micrometer scale10.1016/j.corsci.2011.10.011 ↗
66. International Standard, ISO 15724 · 2001
67. DeLuccia · 1981 · 256
68. Mansfeld. “Electrochemical cell for measuring hydrogen in metal”. United States Patent, pp. 1–4, (1982).
69. An electrochemical method for determining hydrogen concentrations in metals and some applications
70. Effect of mechanical deformation on permeation of hydrogen in iron10.2355/isijinternational.43.548 ↗
71. Hydrogen embrittlement interactions in cold-worked steel10.5006/1.3293573 ↗
72. Hydrogen absorption and diffusion in Cr-Mo low alloy steels undergoing tensile straining
73. An example of the effect of hydrogen trapping on hydrogen embrittlement10.1007/BF02648348 ↗
74. The interaction of hydrogen with dislocation in iron10.1016/0001-6160(84)90217-7 ↗
75. SKPFM measured Volta potential correlated with strain localization in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel10.1016/j.corsci.2015.06.035 ↗
76. Hydrogen absorption, embrittlement and fracture of steel10.5006/0010-9312-13.7.33 ↗
77. The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test10.1016/j.corsci.2015.06.038 ↗
78. Effect of hydrogen content on the embrittlement in a Fe-Mn-C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗