Abstract

The dense Cr/GLC multilayer coatings were fabricated by high power impulse magnetron sputtering (HiPIMS) with various duty cycles. HiPIMS-deposited GLC coatings with high density displayed the lower corrosion current density by five times than DC- deposited GLC, due to the higher C + ionization rate and larger incident ions energy. Noted that, after 425 h immersion with 15 MPa, though a laminar-like spallation occurred in the Cr/GLC interfaces instead of the coating/substrate interfaces, the lower galvanic corrosion current density was particularly achieved at 2.04 × 10 −9 A·cm −2 for the HiPIMS-coatings with reduced porosity, emulating an excellent tolerance of long-term corrosion resistance for deep-sea.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. A review of studies on corrosion of metals and alloys in deep-sea environment10.1016/j.oceaneng.2014.05.003 ↗
2. Studies of impedance models and water transport behaviours of epoxy coating at hydrostatic pressure of seawater10.1016/j.porgcoat.2013.03.006 ↗
3. Accelerated deterioration mechanism of 316L stainless steel in NaCl solution under the intermittent tribocorrosion process10.1016/j.jmst.2022.01.011 ↗
4. Influence of nickel additions on the corrosion behaviour of low nitrogen 22% Cr series duplex stainless steels10.1016/j.corsci.2008.05.023 ↗
5. Influence of Cu and Sn content in the corrosion of AISI 304 and 316 stainless steels in H2SO410.1016/j.corsci.2005.05.002 ↗
6. The effect of carbon on hydrogen embrittlement in stable Cr-Ni-Mn-N austenitic stainless steels10.1016/j.corsci.2017.05.004 ↗
7. Failure behavior of nano-SiO2 fillers epoxy coating under hydrostatic pressure10.1016/j.electacta.2011.11.067 ↗
8. Study of the failure mechanism of an epoxy coating system under high hydrostatic pressure10.1016/j.corsci.2013.04.012 ↗
9. Diamond-like amorphous carbon10.1016/S0927-796X(02)00005-0 ↗
10. Insights on high temperature friction mechanism of multilayer ta-C films10.1016/j.jmst.2021.04.028 ↗
11. Tailoring the tribocorrosion and antifouling performance of (Cr, Cu)-GLC coatings for marine application10.1021/acsami.8b12359 ↗
12. An analysis of tribological performance on Cr/GLC film coupling with Si3N4, SiC, WC, Al2O3 and ZrO2 in seawater10.1016/j.triboint.2015.12.010 ↗
13. Growth defects in PVD hard coatings10.1016/j.vacuum.2009.05.018 ↗
14. Structural design of Cr/GLC films for high tribological performance in artificial seawater: Cr/GLC ratio and multilayer structure10.1016/j.jmst.2017.12.002 ↗
15. Controllable defect engineering to enhance the corrosion resistance of Cr/GLC multilayered coating for deep-sea applications10.1016/j.corsci.2022.110175 ↗
16. High power impulse magnetron sputtering of diamond-like carbon coatings10.1116/6.0000070 ↗
17. A review comparing cathodic arcs and high power impulse magnetron sputtering (HiPIMS)10.1016/j.surfcoat.2014.08.043 ↗
18. Fabrication and mechanical properties of Cr2AlC MAX phase coatings on TiBw/Ti6Al4V composite prepared by HiPIMS10.3390/ma14040826 ↗
19. HiPIMS induced high-purity Ti3AlC2 MAX phase coating at low-temperature of 700 °C10.1016/j.jeurceramsoc.2023.03.059 ↗
20. Effects of HiPIMS pulse-length on plasma discharge and on the properties of WC-DLC coatings10.1016/j.apsusc.2019.05.046 ↗
21. Effect of substrate bias on microstructure and mechanical properties of WC-DLC coatings deposited by HiPIMS10.1016/j.surfcoat.2018.07.088 ↗
22. Cr/GLC multilayered coating in simulated deep-sea environment: Corrosion behavior and growth defect evolution10.1016/j.corsci.2021.109528 ↗
23. Ab initio study of interfacial structure transformation of amorphous carbon catalyzed by Ti, Cr, and W transition layers10.1021/acsami.7b12179 ↗
24. Enhanced tribocorrosion performance of Cr/GLC multilayered films for marine protective application10.1021/acsami.8b00628 ↗
25. Quantitative NEXAFS and solid-state NMR studies of sp 3/ (sp2 + sp3) ratio in the hydrogenated DLC films10.1016/j.diamond.2016.09.026 ↗
26. In situ infrared reflection spectroscopy studies of the initial atmospheric corrosion of Zn–Al–Mg coated steel10.1016/j.corsci.2013.03.005 ↗
27. Diamond-like carbon thin films with high density and low internal stress deposited by coupling DC/RF magnetron sputtering10.1016/j.diamond.2016.10.004 ↗
28. Corrosion resistance of amorphous carbon film in 3.5 wt% NaCl solution for marine application10.1016/j.electacta.2020.136282 ↗
29. Effect of uniaxial stress on the Raman spectra of graphite fibers10.1063/1.340975 ↗
30. Nanoindentation data analysis of loading curve performed on DLC thin films: Effect of residual stress on the elasto-plastic properties10.1063/1.5009756 ↗
31. Interface-induced degradation of amorphous carbon films/stainless steel bipolar plates in proton exchange membrane fuel cells10.1016/j.jpowsour.2020.228269 ↗
32. Probing inhomogeneities in nanoscale organic semiconductor films: Depth profiling using slow positron beam and X-ray reflectivity techniques10.1016/j.ssc.2014.09.001 ↗
33. The correlation between optical and mechanical properties of amorphous diamond-like carbon films prepared by pulsed filtered cathodic vacuum arc deposition10.1016/j.tsf.2018.03.053 ↗
34. Phase tailoring of tantalum thin films deposited in deep oscillation magnetron sputtering mode10.1016/j.surfcoat.2016.08.017 ↗
35. Electrochemical polarization: I. a theoretical analysis of the shape of polarization curves10.1149/1.2428653 ↗
36. One- and two-dimensional polymer films of modified alkanethiol monolayers for preventing iron from corrosion10.1016/S0010-938X(98)00048-1 ↗
37. Comparison of corrosion behaviour of zinc in NaCl and in NaOH solutions; Part II: Electrochemical analyses10.1016/j.corsci.2010.08.018 ↗
38. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
39. Concerning the conversion of the constant phase element parameter Y0 into a capacitance10.5006/1.3280607 ↗
40. Passive films on stainless steels—chemistry, structure and growth10.1016/S0013-4686(02)00841-1 ↗
41. Tailoring hardness and electrochemical performance of TC4 coated Cu/a-C thin coating with introducing second metal Zr10.1016/j.corsci.2020.108713 ↗
42. Determination of coating deterioration with EIS: I. basic relationships
43. Study on the mechanism of hydrostatic pressure promoting electrochemical corrosion of pure iron in 3.5% NaCl solution10.1016/j.actamat.2020.11.009 ↗
44. The effect law of different hydrostatic pressures on the failure of multilayer Cr/GLC coatings in 3.5.wt% NaCl solution10.1016/j.corsci.2023.111120 ↗
45. Galvanic corrosion of type 316L stainless steel and graphite in molten fluoride salt10.1016/j.corsci.2020.108677 ↗
46. A methodology for characterizing the electrochemical stability of DLC coated interlayers and interfaces10.1016/j.surfcoat.2019.07.055 ↗
47. Structural properties and growth evolution of diamond-like carbon films with different incident energies: a molecular dynamics study10.1016/j.apsusc.2013.02.108 ↗