Abstract

To improve fracture toughness and oxidation resistance of SiC coating, we designed and prepared a SiC/PyC laminated coating with biomimetic laminated structure on carbon/carbon (C/C) composites by chemical vapor deposition (CVD) method. The microstructure, mechanical properties and oxidation resistance of the coating were investigated. The results showed that the laminated structure could effectively improve the toughness of SiC coating and avoid the formation of penetrating cracks, thus improved the oxidation resistance of coating. The weight loss of laminated SiC/PyC coated sample decreased 75.2 % compared with that of single SiC coated sample after oxidation at 1773 K. The good oxidation resistance and mechanical properties of SiC/PyC laminated coating were attributed to the toughening effect of laminated structure including crack deflection and interface debonding. Our work could bring beneficial enlightenment to improve the toughness of ceramic coating.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
2. Improved ablation resistance of C/C composites using zirconium diboride and boron carbide10.1016/j.jeurceramsoc.2010.02.025 ↗
3. Quéau, Structural modifications of carbon-carbon composites under high temperature and ion irradiation10.1016/j.apsusc.2004.09.106 ↗
4. Mo-Si-Al-C multiphase oxidation protective coating for carbon/carbon composites10.1016/j.apsusc.2013.03.050 ↗
5. TaB2-SiC-Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2013.06.028 ↗
6. Preparation of ZrB2-MoSi2 high oxygen resistant coating using nonequilibrium state powders by self-propagating high-temperature synthesis10.1007/s40145-021-0485-y ↗
7. Ultra-High temperature ceramic coatings for oxidation protection of carbon-carbon composites10.1111/j.1551-2916.2008.02331.x ↗
8. B2O3 modified SiC-MoSi2 oxidation resistant coating for carbon/carbon composites by a two-step pack cementation10.1016/j.corsci.2009.06.033 ↗
9. Influence of MoSi2 on oxidation protective ability of TaB2-SiC coating in oxygen-containing environments within a broad temperature range10.1007/s40145-020-0406-5 ↗
10. Oxidation through coating cracks of SiC-protected carbon/carbon10.1016/j.surfcoat.2008.09.013 ↗
11. Oxidation and erosion resistance of MoSi2-CrSi2-Si/SiC coated C/C composites in static and aerodynamic oxidation environment10.1016/j.carbon.2010.01.005 ↗
12. Mullite based oxidation protection for SiC-C/C composites in air at temperatures up to 1900 K10.1016/S0955-2219(98)00242-8 ↗
13. Microstructural evolution of SiC coating on C/C composites exposed to 1500 °C in ambient air10.1016/j.ceramint.2018.09.255 ↗
14. Effect of residual silicon on the oxidation resistance of bilayer Yb2Si2O7/SiC coated C/SiC composites at high temperature10.1016/j.corsci.2020.108676 ↗
15. Si-W-Mo coating for SiC coated carbon/carbon composites against oxidation10.1016/j.surfcoat.2007.04.062 ↗
16. Microstructure and anti-oxidation properties of multi-composition ceramic coatings for carbon/carbon composites10.1016/j.ceramint.2010.08.027 ↗
17. CNT-PyC-SiC/SiC double-layer oxidation-protection coating on C/C composite10.1016/j.carbon.2008.07.014 ↗
18. SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites10.1016/j.carbon.2005.09.026 ↗
19. Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 °C10.1016/j.corsci.2011.05.046 ↗
20. Investigation of structure and mechanical properties of magnetron sputtered monolayer and multilayer coatings in the ternary system Si-B-C10.1016/j.surfcoat.2006.07.130 ↗
21. Oxidation behavior of C/SiC composites with a SiC/Mo-Si multilayer coating10.1016/j.carbon.2010.03.054 ↗
22. Magnetron sputtering preparation and properties of SiC/MoSi2 oxidation protective coating for carbon/carbon composites prepared10.1016/S1875-5372(17)30031-0 ↗
23. Long-time ablation behavior of the multilayer alternating CVD-(SiC/HfC)3 coating for carbon/carbon composites10.1016/j.corsci.2021.109586 ↗
24. Design and preparation of multilayer TaC/HfC coating: ablation behavior under oxyacetylene flame with different heat flux10.1016/j.corsci.2022.110385 ↗
25. Ultra-high temperature oxidation behavior of micro-laminated ZrC/MoSi2 coating on C/C composite10.1016/j.corsci.2017.12.034 ↗
26. Microstructure and self-healing properties of multi-layered NiCoCrAlY/TAZ/YSZ thermal barrier coatings fabricated by atmospheric plasma spraying10.1016/j.apsusc.2019.05.268 ↗
27. Microstructure and electrical conductivity of laminated Cu/CNT/Cu10.1016/j.jallcom.2017.05.074 ↗
28. Impact-resistant nacre-like transparent materials10.1126/science.aaw8988 ↗
29. Mechanical and oxidation protective properties of SiC nanowires-toughened SiC coating prepared in-situ by a CVD process on C/C composites10.1016/j.surfcoat.2016.08.072 ↗
30. Multi-length scale Monte Carlo simulation of the growth process of SiC film by chemical vapor deposition10.1016/j.apsusc.2008.09.051 ↗
31. Crystallinity control of SiC grown on Si by sputtering method10.1016/j.jcrysgro.2017.01.042 ↗
32. Toward hard yet tough ceramic coatings10.1016/j.surfcoat.2014.07.007 ↗
33. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
34. Microstructure and mechanical properties of CVD TiN/TiBN multilayer coatings10.1016/j.surfcoat.2019.04.086 ↗
35. Toughness of hard nanostructured ceramic thin films10.1016/j.surfcoat.2006.07.020 ↗
36. A carbon nanotube–enhanced SiC coating for the oxidation protection of C/C composite materials10.1016/j.compositesb.2011.05.012 ↗
37. Comparison of the oxidation behaviors of SiC coatings on C/C composites prepared by pack cementation and chemical vapor deposition10.1016/j.surfcoat.2016.05.071 ↗
38. Influence of boron ion implantation on the oxidation behavior of CVD-SiC coated carbon-carbon composites10.1016/S0008-6223(99)00126-8 ↗
39. Preparation of an oxidation protection coating for c/c composites by low pressure chemical vapor deposition10.1016/S0008-6223(00)00086-5 ↗
40. Oxidation behavior of oxidation protective coatings for PIP–C/SiC composites at 1500°C10.1016/j.ceramint.2011.06.063 ↗
41. Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites10.1016/S0008-6223(02)00103-3 ↗
42. The improvement in oxidation resistance of carbon by a graded SiC/SiO2 coating10.1016/S0955-2219(03)00098-0 ↗
43. Improvement of the bonding strength and the oxidation resistance of SiC coating on C/C composites by pre-oxidation treatment10.1016/j.surfcoat.2014.05.042 ↗
44. Influence of grain size on high temperature oxidation behavior of Cr2AlC ceramics10.1016/j.ceramint.2012.09.039 ↗
45. Effect of grain‐boundary oxidation on fracture toughness of SiC10.1111/j.1151-2916.1987.tb05703.x ↗
46. A multi-layered SiC coating to protect graphite spheres from high temperature oxidation in static air10.1016/j.corsci.2021.109325 ↗