Microstructural understanding of general and localized corrosion of Fe13Cr4Al2Mo1.2Nb alloy in high temperature aerated water and superheated steam
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (74)
Show source-provided references
1. Current state and prospect on the development of advanced nuclear fuel system materials: a review
2. K.G. Field, Y. Yamamoto, B.A. Pint, M.N. Gussev, K.A. Terrani, Accident tolerant FeCrAl fuel cladding: current status towards commercialization, in: Proceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors, Portland, Oregon, USA, August 13–17, 2017, pp. 1381–1389.10.1007/978-3-030-04639-2_91 ↗
3. Material selection for accident tolerant fuel cladding
4. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
5. Recent studies on potential accident-tolerant fuel-cladding systems in light water reactors
6. Development and property evaluation of nuclear grade wrought FeCrAl fuel cladding for light water reactors10.1016/j.jnucmat.2015.10.019 ↗
7. The development of cladding materials for the accident tolerant fuel system from the Materials Genome Initiative10.1016/j.scriptamat.2017.07.030 ↗
8. Effects of Nb-doping on the mechanical properties and high-temperature steam oxidation of annealing FeCrAl fuel cladding alloys10.1016/j.msea.2020.140500 ↗
9. Study on high temperature creep behavior of the accident-resistant cladding Fe–13Cr–4Al-1.85Mo-0.85Nb alloy10.1016/j.msea.2020.140688 ↗
10. Microstructural control of FeCrAl alloys using Mo and Nb additions10.1016/j.matchar.2017.08.008 ↗
11. Accident tolerant nuclear fuels and cladding materials10.1007/s11837-017-2701-3 ↗
12. Performance of FeCrAl for accident-tolerant fuel cladding in high-temperature steam10.1515/corrrev-2016-0067 ↗
13. Versatile oxide films protect FeCrAl alloys under normal operation and accident conditions in light water power reactors10.1007/s11837-017-2705-z ↗
14. Corrosion of FeCrAl alloys used as fuel cladding in nuclear reactors10.1016/j.jallcom.2021.159235 ↗
15. An investigation of FeCrAl cladding behavior under normal operating and loss of coolant conditions10.1016/j.jnucmat.2017.04.039 ↗
16. Water-vapor-effect on the oxidation of Fe-21.5 wt%Cr-5.6 wt%A1 at 1000 °C10.1007/BF02134786 ↗
17. Formation and stability of oxide layer in FeCrAl fuel cladding material under high-temperature steam10.1016/j.jallcom.2016.05.145 ↗
18. Oxidation of FeCrAl alloy: influence of temperature and atmosphere on scale growth rate and mechanism10.1016/S0257-8972(00)00989-0 ↗
19. Oxidation kinetics of ferritic alloys in high-temperature steam environments10.1007/s11837-017-2639-5 ↗
20. B.A. Pint, K.A. Terrani, R.B. Rebak, Steam oxidation behavior of FeCrAl cladding, in: Proceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors, Portland, Oregon, USA, August 13–17, 2017, pp. 1451–1460.10.1007/978-3-030-04639-2_96 ↗
21. Oxidation characteristics of two FeCrAl alloys in air and steam from 800 °C to 1300 °C10.1007/s11837-018-2979-9 ↗
22. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
23. Alumina volatility in water vapor at elevated temperatures10.1111/j.1551-2916.2004.01701.x ↗
24. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
25. Effect of Al and Cr content on air and steam oxidation of FeCrAl alloys and commercial APMT alloy10.1007/s11085-017-9745-1 ↗
26. Uniform corrosion of FeCrAl alloys in LWR coolant environments10.1016/j.jnucmat.2016.06.047 ↗
27. Iron-chrome-aluminum alloy cladding for increasing safety in nuclear power plants10.1051/epjn/2017029 ↗
28. A study of the oxidation of FeCrAl alloy in pressurized water and high-temperature steam environment10.1016/j.corsci.2015.02.027 ↗
29. Uniform corrosion behavior of FeCrAl alloys in borated and lithiated high temperature water10.1016/j.jmst.2020.07.026 ↗
30. Characterization of oxides formed on iron-chromium-aluminum alloy in simulated light water reactor environments10.1515/corrrev-2017-0011 ↗
31. Early corrosion behaviour of irradiated FeCrAl alloy in a simulated pressurized water reactor environment10.1016/j.corsci.2020.108824 ↗
32. Microstructural characteristics of the oxide scale formed on 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.07.015 ↗
33. Corrosion of phase and phase boundary in proton-irradiated 308L stainless steel weld metal in simulated PWR primary water10.1016/j.corsci.2019.108401 ↗
34. Analysis of oxide film formed on type 304 stainless steel in 288 °C water containing oxygen, hydrogen, and hydrogen peroxide10.5006/1.3283969 ↗
35. Effects of hydrogen peroxide on corrosion of stainless steel, (V) Characterization of oxide film with multilateral surface analyses10.1080/18811248.2006.9711173 ↗
36. Effect of dissolved hydrogen on corrosion of 316NG stainless steel in high temperature water10.1016/j.nucengdes.2015.08.030 ↗
37. Experimental evaluation of cold spray FeCrAl alloys coated zirconium-alloy for potential accident tolerant fuel cladding
38. Some thoughts on the mechanisms of in-reactor corrosion of zirconium alloys10.1016/j.jnucmat.2004.09.029 ↗
39. A novel mechanism for nodular corrosion of Zircaloy-4 corroded in 773 K superheated steam10.1016/j.corsci.2017.06.007 ↗
40. Intermediate temperature corrosion behaviour of Fe-12Cr-6Al-2Mo-0.2Si-0.03Y alloy (C26M) at 300-600 °C10.1016/j.corsci.2019.05.029 ↗
41. ASTM G2/G2M-19: Standard test method for corrosion testing of products of zirconium, hafnium, and their alloys in water at 680 °F (360 °C) or in steam at 750 °F (400 °C), ASTM International, West Conshohocken, 2019, pp. 1–8.
42. Out-reactor nodular corrosion behavior of zircaloys10.1016/0022-3115(83)90197-6 ↗
43. Effect of additives on the susceptibility of zirconium alloys to nodular corrosion10.1016/j.jnucmat.2009.04.003 ↗
44. Strengthening mechanism of Nb addition in Fe-13Cr-4.5Al-2Mo alloys assessed by internal friction measurement10.1016/j.jnucmat.2020.152461 ↗
45. Theory of steady-state passive films10.1149/1.2086949 ↗
46. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
47. Oxide film growth kinetics on metals and alloys10.1149/2.036306jes ↗
48. The mechanism and kinetics of corrosion product release from stainless-steel in lithiated high-temperature water10.1016/0010-938X(87)90068-0 ↗
49. Corrosion of nickel-base alloys in primary medium of pressurized water reactors: new insights on the oxide growth mechanisms and kinetic modelling10.1016/j.corsci.2015.09.001 ↗
50. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
51. Properties of oxide films formed on 316l SS and model alloys with modified Ni, Cr and Si contents in high temperature water10.1016/j.corsci.2016.02.001 ↗
52. The evolution of electrochemical behaviour and oxide film properties of 304 stainless steel in high temperature aqueous environment10.1016/j.electacta.2012.03.148 ↗
53. Effects of Mn on the mechanical properties and high temperature oxidation of 9Cr2WVTa steel10.1016/j.jnucmat.2017.07.024 ↗
54. Effects of dissolved hydrogen on general corrosion behavior and oxide films of alloy 690TT in PWT primary water10.1016/j.jnucmat.2016.12.020 ↗
55. Representation of mixed reactive gases on free energy (Ellingham-Richardson) diagrams10.1007/BF02915078 ↗
56. Revised pourbaix diagrams for iron at 25–300 °C10.1016/S0010-938X(96)00067-4 ↗
57. Uniform corrosion of FeCrAl cladding tubing for accident tolerant fuels in light water reactors10.1016/j.jnucmat.2021.153090 ↗
58. New insights into the oxidation mechanisms of a ferritic-martensitic steel in high-temperature steam10.1016/j.actamat.2020.05.052 ↗
59. Microstructure evolution during steam oxidation of a Nb stabilized austenitic stainless steel10.1007/s11085-009-9182-x ↗
60. Microstructural understanding of the oxidation of an austenitic stainless steel in high-temperature steam through advanced characterization10.1016/j.actamat.2020.05.010 ↗
61. Evolution of nanoporosity in dealloying10.1038/35068529 ↗
62. A preliminary correlation between the accelerated corrosion of zircaloy in BWR's and in high temperature, high pressure steam10.1016/0022-3115(76)90289-0 ↗
63. D. Charquet, R. Tricot, J.-F. Wadier, Heterogeneous scale growth during steam corrosion of Zr-4 and 500 °C, in: Proceedings of Zirconium in the Nuclear Industry: 8th International Symposium, San Diego, CA, June 19–23, 1988, pp. 374–391.10.1520/STP18876S ↗
64. B.X. Zhou, J.C. Peng, M.Y. Yao, Q. Li, S. Xia, C.X. Du, G. Xu, Study of the initial stage and anisotropic growth of oxide layers formed on Zr-4, in: Proceedings of Zirconium in the Nuclear Industry: 16th International Symposium, Chengdu, China, May 9–13, 2010, pp. 620–648.10.1520/STP49277T ↗
65. Mechanism of zircaloy nodular corrosion10.1016/0022-3115(83)90199-X ↗
66. Microstructural investigation of the nodular corrosion of 304NG stainless steel in supercritical water10.1016/j.corsci.2020.108652 ↗
67. Nodular corrosion inside the crevice of alloy 690 in deaerated high-temperature chloride solution10.1016/j.corsci.2021.109442 ↗
68. The effect of grain boundary structure on the intergranular degradation behavior of solution annealed alloy 690 in high temperature, hydrogenated water10.1016/j.actamat.2019.10.041 ↗
69. Intergranular oxidation of 316L stainless steel in the PWR primary water environment10.1016/j.corsci.2017.06.023 ↗
70. Effect of irradiation on corrosion of 304 nuclear grade stainless steel in simulated PWR primary water10.1016/j.corsci.2017.08.010 ↗
71. Nanoscale characterisation of grain boundary oxidation in cold-worked stainless steels10.1016/j.corsci.2012.06.030 ↗
72. Atom probe tomography of stress corrosion crack tips in SUS316 stainless steels10.1016/j.corsci.2015.06.008 ↗
73. Transmission electron microscopy examination of oxide layers formed on Zr alloys10.1016/j.jnucmat.2005.10.012 ↗
74. Effect of Zr2+ irradiation on microstructure and corrosion behavior of 90Nb-10Zr binary alloy in 360 °C lithiated water10.1016/j.corsci.2021.109620 ↗