journal article·2015-11Open access

Oxidation model for construction materials in supercritical water—Estimation of kinetic and transport parameters

Sami Penttilä, Iva Betova, Martin Bojinov, Petri Kinnunen, Aki Toivonen

Corrosion Science· Volume 100

Abstract

An upgraded model was employed to obtain estimates of kinetic parameters of oxidation of stainless steel Sanicro 28 (UNS N08028) and nickel-based alloy 690 (UNS N06690) in supercritical water at 650 °C/25 MPa up to 2000 h. In the present approach, it is assumed that the growth of the outer layer is governed by the transport of cations through the inner layer via an interstitialcy mechanism. The model is able to reproduce quantitatively the depth profiles of constituent elements oxide layer, as well as in the transition layer situated between the inner layer and the bulk alloy.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Material performance in supercritical water
2. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
3. Corrosion behavior of alloy 800H (Fe–21Cr–32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
4. Corrosion of ferritic–martensitic steel HT9 in supercritical water10.1016/j.jnucmat.2006.07.010 ↗
5. Influence of dissolved oxygen content on corrosion of the ferritic–martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
6. Pourbaix diagrams for the nickel-water system extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.007 ↗
7. Corrosion behavior of Ni-base alloys for advanced high temperature water-cooled nuclear plants10.1016/j.corsci.2008.08.024 ↗
8. Supercritical water oxidation: an environmentally safe method for the disposal of organic wastes
9. Corrosion behavior of ferritic/martensitic steel P92 in supercritical water10.1016/j.supflu.2009.06.019 ↗
10. Corrosion behavior of Hastelloy C-276 in supercritical water10.1016/j.corsci.2009.05.041 ↗
11. Alloying design of oxide dispersion strengthened ferritic steel for long life FBRs core materials10.1016/0022-3115(93)90200-I ↗
12. Tube manufacturing and mechanical properties of oxide dispersion strengthened ferritic steel10.1016/0022-3115(93)90201-9 ↗
13. Corrosion resistance of high-Cr oxide dispersion strengthened ferritic steels in super-critical pressurized water10.1016/j.jnucmat.2007.03.211 ↗
14. High temperature oxidation behavior of ODS steels10.1016/j.jnucmat.2004.04.203 ↗
15. Improvement of compatibility of advanced ferritic steels with super critical pressurized water toward a higher thermally efficient water-cooled blanket system10.1016/j.fusengdes.2005.09.056 ↗
16. Corrosion properties of oxide dispersion strengthened steels in supercritical water environment10.1016/j.jnucmat.2004.04.040 ↗
17. Influence of alloy composition and temperature on corrosion behavior of ODS ferritic steels10.1016/j.jnucmat.2010.12.279 ↗
18. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
19. Composition, structure, and properties of corrosion layers on ferritic and austenitic steels in ultrasupercritical water10.1149/1.2337166 ↗
20. Surface film electrochemistry of austenitic stainless steel and its main constituents in supercritical water10.1016/j.supflu.2007.06.005 ↗
21. Estimation of kinetic parameters of the corrosion layer constituents on steels in supercritical water coolant conditions10.1016/j.corsci.2011.08.029 ↗
22. Stress corrosion cracking susceptibility of austenitic stainless steels in supercritical water conditions10.1016/j.jnucmat.2010.09.018 ↗
23. High Cr ODS steels performance under supercritical water environment10.1016/j.supflu.2013.04.014 ↗
24. A mixed-conduction model for the oxidation of stainless steel in a high-temperature electrolyte. Estimation of kinetic parameters of oxide layer growth and restructuring10.1149/1.1931447 ↗
25. Estimation of the parameters of oxide film growth on nickel-based alloys in high-temperature water electrolytes10.1016/j.electacta.2007.06.002 ↗
26. Mixed-conduction model for stainless steel in a high-temperature electrolyte: estimation of kinetic parameters of inner layer constituents10.1149/1.2818774 ↗
27. Influence of Zn on the oxide layer on AISI 316L(NG) stainless steel in simulated pressurized water reactor coolant10.1016/j.electacta.2008.08.040 ↗
28. Effect of water chemistry on the oxide film on Alloy 690 during simulated hot functional testing of a pressurized water reactor10.1016/j.corsci.2012.01.002 ↗
29. Growth mechanism of anodic tantalum pentoxide formed in phosphoric acid10.1016/j.electacta.2012.08.014 ↗
30. Enhanced oxidation of the 9% Cr steel P91 in water vapor containing environments10.1016/j.corsci.2006.02.002 ↗
31. Microstructural characteristics of oxide scales grown on stainless steel exposed to supercritical water10.1016/j.scriptamat.2009.08.013 ↗
32. Challenges in the theory of electron transfer at passive interfaces10.1016/j.corsci.2005.06.016 ↗
33. Electrochemical behavior of nickel–chromium alloys in a high-temperature aqueous electrolyte10.5006/1.3277550 ↗
34. Effect of pre-oxidation and corrosion potential on electronic properties of passive films on Ni–Cr–Fe alloys in pure water at 288°C10.1023/B:JMSC.0000012938.61636.4e ↗
35. Einfluss von wasserdampf und kohlendioxyd auf die oxydation von eisen in sauerstoff bei hohen temperaturen10.1016/S0010-938X(65)90500-7 ↗
36. Role of water vapor in chromia-scale growth at low oxygen partial pressure10.1023/A:1023040010859 ↗
37. Protective and non-protective scale formation of Ni–Cr alloys in water vapor containing high- and low-pO2 gases10.1016/j.corsci.2008.03.001 ↗
38. Water vapor effects on Fe–Cr alloy oxidation10.1007/s11085-009-9183-9 ↗
39. The effects of water vapor and hydrogen on the high-temperature oxidation of alloys10.1007/s11085-012-9349-8 ↗
40. Marcus · 2012
41. Diffusion currents in large electric fields for discrete lattices10.1063/1.1709721 ↗
42. The passive state in our reactive metals-based civilization10.1007/s13369-012-0281-7 ↗
43. A practical method for numerical evaluation of solutions of partial differential equations of the heat conduction type10.1017/S0305004100023197 ↗
44. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
45. Oxidation of ferritic-martensitic alloys T91HCM12A and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
46. Corrosion behaviour of 9–12% Cr ferritic–martensitic steels in supercritical water10.1016/j.corsci.2009.12.032 ↗
47. Oxide film growth kinetics on metals and alloys part I10.1149/2.036306jes ↗
48. Oxide film growth kinetics on metals and alloys part II10.1149/2.037306jes ↗
49. On the mechanism of radiation-induced segregation in austenitic Fe–Cr–Ni alloys10.1016/S0022-3115(98)00010-5 ↗
50. A multicomponent model of radiation-induced segregation for commercial stainless steels10.1080/18811248.2007.9711581 ↗
51. S. Penttilä, A. Toivonen, P. Auerkari, R. Novotny, Characterization of high performance austenitic and ODS alloys for SCWR conditions, Proceedings of ICAPP’ 2012, paper 12,051.
52. Shreir’s corrosion
53. A kinetic model of the oxide growth and restructuring on structural materials in nuclear power plants
54. Corrosion mechanisms of candidate structural materials for supercritical water-cooled reactor10.1007/s11708-009-0024-y ↗