Abstract

The long-term corrosion behavior of three FeCrAl(Si) alloys has been investigated in two environments (K2CO3 and KCl+H2O) at 600 °C. The FeCrAl alloy experienced breakaway oxidation in both environments but displayed a higher corrosion rate in KCl+H2O. The FeCrAlSi alloys retained the primary protection in the presence of K2CO3 but underwent breakaway oxidation in the presence of KCl+H2O. The FeCrAlSi alloys displayed considerably reduced corrosion rates, suggested to be an effect of the prevention of internal oxidation and the formation of non-continuous corundum-type oxide dispersed within the inward-growing scale.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (72)

Show source-provided references
1. Characterization of pack cemented Ni2Al3 coating exposed to KCl(s) induced corrosion at 600 °C
2. High temperature corrosion behavior of FeCrAlSi model alloys in the presence of water vapor and KCl at 600 °C – The influence of Cr content10.1016/j.corsci.2022.110114 ↗
3. The influence of small amounts of KCl(s) on the high temperature corrosion of a Fe-2.25Cr-1Mo steel at 400 and 500°C
4. High temperature oxidation and chlorination of FeCrAl alloys, in, Chalmers University of Technology
5. KCl-Induced Corrosion of an FeCrAl Alloy at 600 °C in O2 + H2O Environment: The Effect of Pre-oxidation10.1007/s11085-014-9507-2 ↗
6. KCl-Induced Corrosion of the FeCrAl Alloy Kanthal ® AF at 600 °C and the Effect of H2O10.1007/s11085-014-9506-3 ↗
7. and Kinetic Investigation of the KCl-Induced Corrosion of an FeCrAl Alloy at 600 °C10.1007/s11085-015-9546-3 ↗
8. T. Jonsson, N. Folkeson, J.-E. Svensson, L.-G. Johansson, M.J.C.S. Halvarsson, An ESEM in situ investigation of initial stages of the KCl induced high temperature corrosion of a Fe–2.25 Cr–1Mo steel at 400C, 53, 2011; 2233–2246.10.1016/j.corsci.2011.03.007 ↗
9. Alkali induced high temperature corrosion of stainless steel: the influence of NaCl, KCl and CaCl210.1007/s11085-012-9293-7 ↗
10. KCl‐induced high temperature corrosion of selected commercial alloys10.1002/maco.201408215 ↗
11. KCl-induced high temperature corrosion of selected commercial alloys10.1002/maco.201408215 ↗
12. High temperature corrosion of superheater steels by KCl and K2CO3 under dry and wet conditions10.1016/j.fuproc.2012.05.020 ↗
13. High temperature interaction of Al/Si-modified Fe–Cr alloys with KCl10.1016/j.corsci.2006.10.019 ↗
14. Effect of Al/Si addition on KCl induced corrosion of 9% Cr steel10.1016/j.matlet.2004.06.068 ↗
15. Effect of service exposure on KCl corrosion attack of AISI 347H FG steel10.1007/s10853-019-03863-4 ↗
16. Effect of microstructure on KCl corrosion attack of modified AISI 310 steel10.1080/09603409.2017.1389381 ↗
17. Oxidation of Fe-2.25Cr-1Mo in presence of KCl(s) at 400 °C – Crack formation and its influence on oxidation kinetics10.1016/j.corsci.2019.108234 ↗
18. The Influence of Small Amounts of KCl(s) on the Initial Stages of the Corrosion of Alloy Sanicro 28 at 600 °C10.1007/s11085-008-9118-x ↗
19. KCl Induced Corrosion of a 304-type Austenitic Stainless Steel at 600°C; The Role of Potassium10.1007/s11085-005-5704-3 ↗
20. The Effects of KCl, K2SO4 and K2CO3 on the High Temperature Corrosion of a 304-Type Austenitic Stainless Steel10.1007/s11085-011-9240-z ↗
21. Alkali Induced Corrosion of 304-type Austenitic Stainless Steel at 600 degrees C; Comparison between KCl, K2CO3 and K2SO4
22. Continuous KCl addition in high temperature exposures of 304 L - A way to mimic a boiler environment10.1016/j.corsci.2020.108511 ↗
23. Initial oxidation mechanisms of stainless steel Sanicro 28 (35Fe27Cr31Ni) exposed to KCl, NaCl, and K2CO3 under dry and humid conditions at 535 °C10.1016/j.corsci.2019.04.010 ↗
24. The Effects of KCl, NaCl and K2CO3 on the High-Temperature Oxidation Onset of Sanicro 28 Steel10.1007/s11085-016-9613-4 ↗
25. Enhanced internal oxidation as reason for breakdown of protective chromia scales on FeCr-alloys in water vapour containing gases10.4028/www.scientific.net/MSF.595-598.699 ↗
26. The Kinetic Behaviour of Metals in Water Vapour at High Temperatures: Can General Rules Be Proposed?10.4028/www.scientific.net/MSF.369-372.231 ↗
27. The Effect of Water Vapor on the Initial Stages of Oxidation of the FeCrAl Alloy Kanthal AF at 900 °C10.1007/s11085-007-9055-0 ↗
28. Effect of water vapour on the oxidation of Fe–13Cr–5Ni martensitic alloy at 973 K10.1016/j.corsci.2012.04.008 ↗
29. p. trans tech, Oxidation of stainless steel in H2O/O-2 environments - Role of chromium evaporation
30. Evidence for Chromium Evaporation Influencing the Oxidation of 304L: The Effect of Temperature and Flow Rate10.1023/A:1014877600235 ↗
31. Effective Reduction of Chromium-oxy-hydroxide Evaporation from Ni-Base Alloy 69010.1007/s11085-019-09935-9 ↗
32. A surface analytical approach to the high temperature chlorination behaviour of inconel 600 at 700C10.1016/S0010-938X(96)00112-6 ↗
33. Einfluß von HCl und Cl2 auf die Hochtemperaturkorrosion des 2 1/4 Cr 1 Mo‐Stahls in Atmosphären mit hohen Sauerstoffdrücken, Materials and Corrosion
34. Chlorine Induced Corrosion in Biomass and Waste Fired Boilers: Laboratory and Field Investigations
35. Secondary corrosion protection of FeCr(Al) model alloys at 600 °C – The influence of Cr and Al after breakaway corrosion10.1016/j.corsci.2021.109584 ↗
36. Beyond Breakaway Corrosion - Influence of Chromium, Nickel and Aluminium on Corrosion of Iron-based Alloys at 600 ∘C10.1016/j.corsci.2020.108961 ↗
37. Effect of alloy grain size and silicon content on the oxidation of austenitic Fe-Cr-Ni-Mn-Si alloys in pure O210.1007/BF00662967 ↗
38. J. Dunning, D. Alman, J.J.Oo.M. Rawers, Influence of silicon and aluminum additions on the oxidation resistance of a lean-chromium stainless steel, 57, 2002: 409–425.10.1023/A:1015344220073 ↗
39. The influence of silicon on the corrosion properties of FeCrAl model alloys in oxidizing environments at 600 °C10.1016/j.corsci.2018.09.004 ↗
40. The effect of silicon addition on the high temperature oxidation of a Fe-Cr alloy
41. Effects of Silicon on High Temperature Corrosion of Fe–Cr and Fe–Cr–Ni Alloys in Carbon Dioxide10.1007/s11085-013-9467-y ↗
42. Effects of Silicon and Water Vapour on Corrosion of Fe–20Cr and Fe–20Cr–20Ni Alloys in CO2 at 650 °C10.1007/s11085-016-9681-5 ↗
43. science, technology
44. Effect of silicon on high temperature oxidation of stainless steels10.5006/0010-9312-15.11.73 ↗
45. Exploring the Effect of Silicon on the High Temperature Corrosion of Lean FeCrAl Alloys in Humid Air10.1007/s11085-020-10019-2 ↗
46. Oxygen and Water Vapour Oxidation of 15Cr Ferritic Stainless Steels with Different Silicon Contents10.4028/www.scientific.net/MSF.461-464.839 ↗
47. The influence of Si on the primary protection of lean FeCrAl model alloys in O2 and O2+H2O at 600 °C—A microstructural investigation10.1016/j.corsci.2020.109155 ↗
48. Rates of Evaporation. VI. The Vapour Pressure and Rate of Evaporation of Potassium Chloride
49. High temperature corrosion resistance of FeCr(Ni, Al) alloys as bulk/overlay weld coatings in the presence of KCl at 600 °C10.1016/j.corsci.2022.110896 ↗
50. Corrosion of FeCrAl Alloys in Biomass-And Waste-Fired Boilers-The Influence of Alloying Elements in Prediction and Mitigation of Corrosion in Harsh Environments
51. Comparison of potassium chloride and potassium carbonate with respect to their tendency to cause high temperature corrosion of stainless 304L steel10.1016/j.fuproc.2011.12.016 ↗
52. Oxidation After Breakdown of the Chromium-Rich Scale on Stainless Steels at High Temperature: Internal Oxidation10.1007/s11085-016-9610-7 ↗
53. High-Temperature Oxidation of FeCr(Ni) Alloys: The Behaviour After Breakaway10.1007/s11085-017-9731-7 ↗
54. The Influence of Oxide-Scale Microstructure on KCl(s)-Induced Corrosion of Low-Alloyed Steel at 400 °C10.1007/s11085-018-9881-2 ↗
55. The Influence of KCl and HCl on the High-Temperature Oxidation of a Fe-2.25Cr-1Mo Steel at 400 °C10.1007/s11085-019-09943-9 ↗
56. The influence of H2O on iron oxidation at 600C: a microstructural study10.4028/www.scientific.net/MSF.595-598.1005 ↗
57. Oxidation of iron at 400–600°C in dry and wet O210.1016/j.corsci.2010.01.002 ↗
58. Oxidation of Binary FeCr Alloys (Fe–2.25Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2 + H2O Environment at 600 °C10.1007/s11085-010-9229-z ↗
59. Oxidation of Fe–10Cr in O2 and in O2+H2O environment at 600°C: A microstructural investigation10.1016/j.corsci.2013.06.016 ↗
60. J. Eklund, M.D. Paz, B. Jönsson, J. Liske, J.-E. Svensson, T. Jonsson, Field exposure of FeCrAl model alloys in a waste-fired boiler at 600°C: The influence of Cr and Si on the corrosion behaviour, 70, 2019: 1476–1485.10.1002/maco.201810618 ↗
61. Y. Inoue, N. Hiraide, K. Ushioda, Effect of Si Addition on Oxidation Behavior of Nb containing Ferritic Stainless Steel, Tetsu-to-Hagane, advpub, 2016.10.2355/tetsutohagane.TETSU-2016-023 ↗
62. Microstructural Investigation of the Effect of Water Vapour on the Oxidation of the Si-Containing FeCrNi Steel 353MA at 900 (Degree Sign) C in Oxygen10.1149/MA2006-02/18/949 ↗
63. Effect of Si on high temperature oxidation of 30Cr13 stainless steel10.1016/S1006-706X(17)30084-5 ↗
64. Effects of si on oxidation behaviors in Cr-Mn-Ni austenitic stainless steels10.4028/www.scientific.net/MSF.539-543.4897 ↗
65. Healing layer formation in Fe–Cr–Si ferritic steels10.1179/mst.1989.5.8.741 ↗
66. High-temperature oxidation and aqueous corrosion performance of ferritic, vacuum-sintered stainless steels prealloyed with Si10.1016/j.corsci.2008.09.035 ↗
67. The influence of Si on the primary protection of lean FeCrAl model alloys in O2 and O2+H2O at 600 °C – A microstructural investigation
68. Microstructural investigation of the effect of water vapour on the oxidation of alloy 353 MA in oxygen at 700 and 900°C10.3184/096034005782744461 ↗
69. Mechanism of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide
70. Kinetics of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗
71. M. Mantel, Breakaway oxidation of austenitic stainless steels induced by alloyed sulphur10.1016/j.corsci.2015.01.007 ↗
72. Oxidation of a Fe–18Cr–8Ni austenitic stainless steel at 850°C in O2: Microstructure evolution during breakaway oxidation10.1016/j.corsci.2016.10.029 ↗