journal article·2022-02

Unlocking the cavitation erosion-corrosion resistance of a TiCN nanocrystalline coating with an equiaxed grain structure

Shuang Peng, Jiang Xu, Shuyun Jiang, Zong-Han Xie, Paul Munroe

Corrosion Science· Volume 195
Publisher page

Abstract

Abstract To alleviate cavitation erosion damage in hydraulic machines operating, a TiCN coating was prepared on to a TC11 substrate using a double-cathode glow discharge technique. The TiCN coating consist of equiaxed nanocrystals with the grain size of about 10 nm. Under cavitation condition, the TiCN coated sample showed higher corrosion resistant, lower local corrosion tendency and less weight loss than the substrate. The excellent cavitation erosion resistance of the TiCN coating was ascribed to its nanoscale equiaxed grain structure and the good self-healing capability of the passive film, which was confirmed through both subsurface cross-sectional observation and electrochemical measurements.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. Cavitation erosion mechanisms in stainless steels and in composite metal–ceramic HVOF coatings10.1016/j.wear.2016.07.015 ↗
2. Ultrasonic cavitation erosion mechanism and mathematical model of HVOF sprayed Fe-based amorphous/nanocrystalline coatings10.1016/j.ultsonch.2018.11.010 ↗
3. Different methods of measuring synergy between cavitation erosion and corrosion for nickel aluminium bronze in 3.5% NaCl solution
4. Synergistic effect of cavitation erosion and corrosion of various engineering alloys in 3.5% NaCl solution10.1016/S0921-5093(00)00899-6 ↗
5. The synergistic effect of cavitation erosion and corrosion of nickel-aluminum copper surface layer on nickel-aluminum bronze alloy10.1016/j.jallcom.2018.03.103 ↗
6. Cavitation resistance of TiN nanocrystalline coatings with various thickness
7. Cavitation erosion of monolayer PVD coatings – An influence of deposition technique on the degradation process
8. Cavitation erosion and sliding wear mechanisms of AlTiN and TiAlN films deposited on stainless steel substrate10.3390/coatings9050340 ↗
9. Corrosion resistance of multi-layered plasma-assisted physical vapour deposition TiN and CrN coatings10.1016/S0257-8972(01)01267-1 ↗
10. V. Vasyliev, A. Luchaninov, E. Reshetnyak, V. Strel’nitskij, Structure and Properties of Periodic Multilayer Metal/nitride Coatings Deposited from Filtered Vacuum-arc Plasma Using Ti-Al-Y Cathode, 2020 IEEE 10th International Conference Nanomaterials: Applications & Properties (NAP) Sumy, Ukraine, 2020, pp. 01TFC26–01-01TFC26–05.10.1109/NAP51477.2020.9309561 ↗
11. Cavitation erosion resistance parameter of hard CAVD coatings10.1016/j.porgcoat.2010.11.013 ↗
12. Micro-and nanostructured diamond films under wear charging in cavitation test10.1016/S0257-8972(03)00658-3 ↗
13. The influence of semiconducting properties of passive films on the cavitation erosion resistance of a NbN nanoceramic coating10.1016/j.ultsonch.2020.105406 ↗
14. Advanced damage resistance monitoring procedure on the composite materials’ surface-exposed to cavitation testing
15. Analysis of mechanical and chemical mechanisms on cavitation erosion-corrosion of steels in salt water using electrochemical methods10.1016/j.triboint.2018.04.012 ↗
16. Instantaneous impedance monitoring of synergistic effect between cavitation erosion and corrosion processes10.1016/j.electacta.2016.01.216 ↗
17. Application of electrochemical noise (EN) technology to evaluate the passivation performances of adsorption and film-forming type corrosion inhibitors10.1016/j.jelechem.2019.113584 ↗
18. Review—electrochemical probes and sensors designed for time-dependent atmospheric corrosion monitoring: fundamentals, progress, and challenges10.1149/2.0132003JES ↗
19. Sources of electrochemical noise in corroding systems10.1134/S1023193506050077 ↗
20. Electrochemical noise (EN) technique: review of recent practical applications to corrosion electrochemistry research10.1080/01694243.2019.1587224 ↗
21. Oxidation resistance of Mo(Si1-xAlx)2 nanocrystalline films and characterization of their oxide scales by electrochemical impedance spectroscopy10.1039/C4RA10570B ↗
22. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
23. Cavitation erosion mechanisms in stainless steels and in composite metal–ceramic HVOF coatings10.1016/0257-8972(93)90200-8 ↗
24. Electrochemical noise—guidance for improving measurements and data analysis10.5006/3211 ↗
25. Formation mechanism and corrosion performance of phosphate conversion coatings on AZ91 and Mg-Gd-Y-Zr alloy10.1149/2.0221810jes ↗
26. Review—electrochemical noise applied in corrosion science: theoretical and mathematical models towards quantitative analysis10.1149/1945-7111/ab8de3 ↗
27. Effect of atmospheric plasma sprayed TiO2-10% NiAl cermet coating thickness on cavitation erosion, sliding and abrasive wear resistance10.12693/APhysPolA.136.335 ↗
28. Composite cavitation resistant PVD coatings based on NiTi thin films10.1016/j.matdes.2016.08.054 ↗
29. Cavitation protection by low temperature TiCN coatings10.1016/0257-8972(95)08265-4 ↗
30. Structure–property relationships in single- and dual-phase nanocrystalline hard coatings10.1016/S0257-8972(03)00576-0 ↗
31. Particle bombardment effects on thin‐film deposition: A review10.1116/1.576238 ↗
32. Comparison of the cavitation erosion and slurry erosion behavior of cobalt-based and nickel-based coatings10.1016/j.wear.2019.03.022 ↗
33. Cavitation erosion resistance enhancement of martensitic stainless steel via low-temperature plasma carburizing
34. Analysis of morphological, microstructural, electrochemical and nano mechanical characteristics of TiCN coatings prepared under N2 gas flow rate by chemical vapour deposition (CVD) process at higher temperature10.1016/j.ceramint.2020.01.023 ↗
35. Effects of spray distance on the microstructure and mechanical properties of reactive plasma sprayed TiCN coatings10.1016/j.ceramint.2018.06.181 ↗
36. Structure and wear characteristics of TiCN nanocomposite coatings fabricated by reactive plasma spraying10.1016/j.surfcoat.2018.02.108 ↗
37. Tribological behaviours of PVD TiN and TiCN coatings in artificial seawater10.1016/j.surfcoat.2013.03.034 ↗
38. The influence of TiN coatings properties on cavitation erosion resistance10.1016/j.surfcoat.2009.07.014 ↗
39. An investigation on cavitation-corrosion behavior of Ni/β-SiC nanocomposite coatings under ultrasonic field10.1016/j.ultsonch.2019.04.022 ↗
40. Reactive sputter deposition of alumina films on magnesium alloy by double cathode glow-discharge plasma technique10.1016/j.matchar.2009.12.007 ↗
41. The relationship between the formation process of corrosion scales and the electrochemical mechanism of carbon steel in high pressure CO2-containing formation water10.1149/2.030209jes ↗
42. Evaluation of naphthenic acidity number and temperature on the corrosion behavior of stainless steels by using Electrochemical Noise technique10.1016/j.electacta.2013.08.090 ↗
43. Transient analysis through Hilbert spectra of electrochemical noise signals for the identification of localized corrosion of stainless steel10.1016/j.electacta.2013.04.085 ↗
44. Quasiperiodicity and Chaos during an electrochemical reaction10.1021/j100344a009 ↗
45. Dynamics of stainless steel corrosion based on the theory of phase space reconstruction and chaos10.1108/ACMM-11-2015-1613 ↗
46. The significance of correlation dimension obtained from electrochemical noise10.5796/electrochemistry.80.907 ↗
47. Electrochemical Noise Study on the Corrosion Behavior of 304NG Stainless Steel in High Temperature Water10.5796/electrochemistry.82.647 ↗
48. Chaotic analysis of electrochemical noise measured on stainless steel10.1149/1.2044205 ↗
49. Identifying corrosion forms on synthetic electrochemical noise signals by the Hilbert–Huang transform method10.1080/1478422X.2018.1505804 ↗
50. Laboratory investigation of microbiologically influenced corrosion of 2205 duplex stainless steel by marine Pseudomonas aeruginosa biofilm using electrochemical noise10.1016/j.corsci.2018.08.018 ↗
51. In situ monitoring of the localized corrosion of 304 stainless steel in FeCl 3 solution using a joint electrochemical noise and scanning reference electrode technique10.1016/j.elecom.2018.03.002 ↗
52. Novel time–frequency characterization of electrochemical noise data in corrosion studies using Hilbert spectra10.1016/j.corsci.2012.09.007 ↗
53. The role of passive potential in ultrasonic cavitation erosion of titanium in 1 M HCl solution10.1016/j.ultsonch.2015.09.018 ↗
54. Enhancement of cavitation erosion resistance of 316 L stainless steel by adding molybdenum10.1016/j.ultsonch.2016.10.015 ↗
55. Evaluation of cavitation erosion resistance of arc-sprayed Fe-based amorphous/nanocrystalline coatings in NaCl solution10.1016/j.rinp.2018.12.007 ↗
56. Microwave-assisted post-processing of detonation gun-sprayed coatings for better slurry and cavitation erosion resistance10.1007/s11666-019-00914-9 ↗
57. Water irradiation by high-frequency ultrasonic wave: effects on properties of passive film formed on stainless steel10.1016/j.ultsonch.2011.04.003 ↗
58. Cavitation erosion behavior of HVOF sprayed WC-10Co4Cr cermet coatings in simulated sea water10.1016/j.oceaneng.2019.106449 ↗
59. Nanoindentation induced plastic deformation in nanocrystalline ZrN coating10.1016/j.matlet.2015.10.091 ↗
60. Nanohardness of nanocrystalline TiN thin films10.1016/j.surfcoat.2004.10.098 ↗
61. Deformation in nanocrystalline ceramics: a microstructural study of MgAl2O410.1016/j.actamat.2019.11.015 ↗
62. Correlation between microstructural characteristics and cavitation resistance of Stellite-6 coatings on 17-4 PH stainless steel prepared with supersonic laser deposition and laser cladding10.1016/j.jallcom.2020.158417 ↗
63. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting