Abstract Fe-9Cr, Fe-9Cr-1Mo and Fe-9Cr-0.5Mo-0.5Ni (wt%) alloys have been prepared for studying the effect of (Mo, Mo/Ni) on carbide precipitation, oxidation behavior and high-temperature tensile property of Fe-9Cr alloy. Rod-shaped Cr23C6 precipitates in Fe-9Cr alloy were refined and spheroidized by Mo addition, while Mo/Ni addition had no impact on Cr23C6 precipitates. Adding (Mo, Mo/Ni) to Fe-9Cr alloy reduced inward oxygen diffusion and the growth rate of an inner Cr-rich layer, thereby accelerating chromia formation and improving the oxidation resistance. High-temperature strength of Fe-9Cr alloy was also enhanced by alloying elements (Mo, Mo/Ni).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Combustion assisted gravity drainage- Experimental and simulation results of a promising in-situ combustion technology to recover extra-heavy oil10.1016/j.petrol.2017.01.044 ↗
2. Investigation of the combustion characteristics of Bati Raman oil with sand10.1016/j.petrol.2017.08.006 ↗
3. Mechanical performance of casing in in-situ combustion thermal recovery10.1016/j.petrol.2018.04.068 ↗
4. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe-Cr and Fe-Cr-X alloys10.1007/s11085-010-9215-5 ↗
5. A ferrite stainless steel Cr27Mo6Al3Cu with oxidation resistance10.1016/j.matdes.2012.04.006 ↗
6. Corrosion behavior of seamless pipeline C-Mn steel by on-line controlled cooling technique10.2355/isijinternational.ISIJINT-2017-523 ↗
7. Influence of molybdenum on tribo-corrosion behavior of 316L stainless steel in artificial saliva10.1007/s40735-015-0014-z ↗
8. Effect of Mo addition on strength of fire-resistant steel at elevated temperature10.1007/s11665-014-1051-3 ↗
9. Influence of Mo on high-temperature oxidation behavior of La- and Zr-added 20 mass %Cr–6 mass %Al ferritic stainless steels10.1007/s11085-016-9660-x ↗
10. Molybdenum effect on oxidation resistance and electric conduction of ferritic stainless steel for SOFC interconnect10.1016/j.ijhydene.2012.04.013 ↗
11. Oxidation of iron-molybdenum and nickel-molybdenum alloys10.1149/1.2429990 ↗
12. Catastrophic oxidation of some molybdenum-containing alloys10.1149/1.2429980 ↗
13. High temperature corrosion protection of austenitic AISI 304 stainless steel by Si, Mo and Ce ion implantation10.1016/S0257-8972(98)00685-9 ↗
14. Effects of Cr, W, and Mo on the high temperature oxidation of Ni-based superalloys10.3390/ma12182934 ↗
15. Role of molybdenum on the AISI 316L oxidation at 900℃10.1007/s10853-008-2965-7 ↗
16. Effect of Ni-Mo addition on cyclic and isothermal oxidation resistance and electrical behavior of ferritic stainless steel for SOFCs interconnect10.1016/j.ijhydene.2014.05.122 ↗
17. MoSi2/(Mo, Ti)Si2 dual-phase composite coating for oxidation protection of molybdenum alloy10.1016/j.jallcom.2017.08.173 ↗
18. Effect of Ni addition on the fracture behavior of a cast ferritic stainless steel10.1016/0167-577X(96)00006-7 ↗
19. High temperature oxidation mechanism of a 3%Ni cast stainless steel10.1179/147842204X2907 ↗
20. Kubaschewski · 1953
21. High-temperature oxidation of Cu-30 wt.% Ni-15 wt.% Fe10.1016/S0010-938X(00)00080-9 ↗
22. Oxidation or nitridation behavior of pure chromium and chromium alloys containing 10 mass % Ni or Fe in atmospheric heating10.2320/matertrans.47.2540 ↗
23. Modelling the effects of alloying elements on precipitation in ferritic steels10.1016/S0921-5093(02)00418-5 ↗
24. Influence of martensitic structure and carbide precipitation behavior on mechanical properties of 25CrMoNbB alloy steels with Mo contents of 0.25 and 0.5 Pct
25. Influence of Mo on precipitation hardening in hot rolled HSLA steels containing Nb10.1016/S1359-6462(00)00411-5 ↗
26. Carbide precipitation and high-temperature strength of hot-rolled high-strength, low-alloy steels containing Nb and Mo10.1007/s11661-002-0178-2 ↗
27. Coarsening kinetics of multicomponent MC-type carbides in high-strength low-alloy steels10.1007/s11661-003-0303-x ↗
28. Influence of Mo on growth and coarsening of nanometer-sized carbides in low-alloy ferritic steels containing Ti10.1016/S1006-706X(14)60156-4 ↗
29. Water vapor effects on the oxidation behavior of Fe-Cr and Ni-Cr alloys in atmospheres relevant to oxy-fuel combustion10.1007/s11085-012-9302-x ↗
30. Self-healing metal-enamel composite coating and its protection for TiAl alloy against oxidation under thermal shock in NaCl solution10.1016/j.corsci.2020.108526 ↗
31. Oxidation behavior of Ni–Mo–Si alloy coatings fabricated on carbon steel by laser cladding10.1016/j.surfcoat.2019.08.001 ↗
32. A new insight into high-temperature oxidation mechanism of superaustenitic stainless steel S32654 in air10.1016/j.jallcom.2016.06.023 ↗
33. Structural and morphological studies of the growth of MoO3 scales during high-temperature oxidation of molybdenum10.1007/BF00665191 ↗
34. High-temperature oxidation behavior of 2 14 Cr-1Mo steel in air—Part 1: Gain of mass kinetics and characterization of the oxide scale10.1115/1.1335499 ↗
35. Reactive element effects on the ionic transport processes in Cr2O3 scales10.1016/S0167-2738(98)00101-5 ↗
36. Phase equilibria and thermodynamic properties in the system Ni-Mo-O10.1007/BF01132018 ↗
37. Na2SO4 and NaCl-induced hot corrosion of six nickel-base superalloys10.1007/BF00603857 ↗
38. Electrocatalytic properties of new spinel-type MMoO4 (M=Fe, Co and Ni) electrodes for oxygen evolution in alkaline solution10.1016/j.ijhydene.2008.06.008 ↗
39. High temperature corrosion of Fe-Cr-(Mn/Si) alloys in CO2-H2O-SO2 gases10.1016/j.corsci.2016.07.026 ↗