Abstract

This work investigated the effect of shearing prestrain on hydrogen embrittlement. The strength and ductility values were similar to those in air for hydrogen precharging before tensile testing, but the ductility decreased significantly for tensile testing with in-situ hydrogen charging due to intergranular fracture initiation at the specimen surface. In contrast, there was a significant decrease in ductility for the hydrogen precharged steel after prestrain. The hydrogen-facilitated fracture was transgranular. The hydrogen fracture grew by fracture tip blunting, new fracture initiation, and coalescence, consistent with a hydrogen enhanced localized plasticity (HELP) mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (78)

Show source-provided references
1. WorldAutoSteel, Advanced High-Strength Steels Application Guidelines V6.0, in, 2017.
2. Martensitic automotive steel sheet-fundamentals and metallurgical optimization strategies
3. A review of hydrogen embrittlement of martensitic advanced high-strength steels10.1515/corrrev-2016-0006 ↗
4. Evaluation of automobile service performance using laboratory testing10.1080/02670836.2018.1495903 ↗
5. A review of the influence of hydrogen on the mechanical properties of DP, TRIP, and TWIP advanced high-strength steels for auto construction10.1515/corrrev-2015-0083 ↗
6. Further study of the hydrogen embrittlement of martensitic advanced high-strength steel in simulated auto service conditions10.1016/j.corsci.2018.02.037 ↗
7. Hydrogen embrittlement of an automotive 1700 MPa martensitic advanced high-strength steel10.1016/j.corsci.2020.108726 ↗
8. The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test10.1016/j.corsci.2015.06.038 ↗
9. Correlation between the microstructure and hydrogen embrittlement resistance in a precipitation-hardened martensitic stainless steel10.1016/j.corsci.2021.109260 ↗
10. Hydrogen embrittlement of a quenching and partitioning steel during corrosion and zinc electroplating10.1016/j.msea.2018.12.022 ↗
11. Microstructural evaluation of hydrogen embrittlement and successive recovery in advanced high strength steel10.1016/j.jmatprotec.2018.09.039 ↗
12. Mechanical properties and fracture behavior of hydrogen charged AHSS/UHSS grades at high- and low strain rate tests10.1016/j.msea.2013.10.044 ↗
13. Influence of hydrogen on steel components for clean energy10.3390/cmd1010002 ↗
14. Hydrogen influence on some advanced high-strength steels10.1016/j.corsci.2017.06.012 ↗
15. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel10.1016/j.ijhydene.2014.06.079 ↗
16. Evaluation of the hydrogen embrittlement susceptibility in DP steel under static and dynamic tensile conditions10.1016/j.ijimpeng.2018.10.002 ↗
17. Influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels in simulated service conditions10.1016/j.corsci.2016.05.040 ↗
18. Warm pre-strain: strengthening the metastable 304l austenitic stainless steel without compromising its hydrogen embrittlement resistance10.3390/ma10111331 ↗
19. Combined effects of prior plastic deformation and sensitization on hydrogen embrittlement of 304 austenitic stainless steel10.1016/j.ijhydene.2019.01.122 ↗
20. Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: Effect of plastic pre-strain10.1016/j.ijhydene.2014.04.122 ↗
21. Effect of pre-strain on hydrogen embrittlement of high strength steels10.1016/j.msea.2014.07.085 ↗
22. Effect of cathodic hydrogen-charging current density on mechanical properties of prestrained high strength steels10.1016/j.msea.2015.06.003 ↗
23. Effect of plastic strain damage on the hydrogen embrittlement of a dual-phase (DP) and a quenching and partitioning (Q&P) advanced high-strength steel
24. Hydrogen-induced delayed fracture of a 1180 MPa martensitic advanced high-strength steel under U-bend loading
25. Hydrogen fracture maps for sheared-edge-controlled hydrogen-delayed fracture of 1180 MPa advanced high-strength steels10.1016/j.corsci.2021.109360 ↗
26. The role of the microstructure on the influence of hydrogen on some advanced high-strength steels10.1016/j.msea.2017.12.079 ↗
27. Evaluation of the influence of hydrogen on some commercial DP, Q&P and TWIP advanced high-strength steels during automobile service10.1016/j.engfailanal.2018.08.011 ↗
28. MPa class automotive martensitic advanced high-strength steel
29. The influence of microstructure on the hydrogen embrittlement susceptibility of martensitic advanced high strength steels10.1016/j.mtcomm.2018.07.011 ↗
30. Dependence of hydrogen embrittlement mechanisms on microstructure-driven hydrogen distribution in medium Mn steels10.1016/j.actamat.2019.11.029 ↗
31. Study of the hydrogen uptake in deformed steel using the microcapillary cell technique10.1016/j.corsci.2019.04.029 ↗
32. Characterization of mechanically sheared edges of dual phase steels10.1016/j.jmatprotec.2012.01.006 ↗
33. Hydrogen trapping in some advanced high strength steels10.1016/j.corsci.2016.05.046 ↗
34. Hydrogen concentration in dual-phase (DP) and quenched and partitioned (Q&P) advanced high-strength steels (AHSS) under simulated service conditions compared with cathodic charging conditions10.1002/adem.201600217 ↗
35. Equivalent hydrogen fugacity during electrochemical charging of some martensitic advanced high-strength steels10.1016/j.corsci.2017.08.011 ↗
36. Equivalent hydrogen fugacity during electrochemical charging of 980DP steel determined by thermal desorption spectroscopy10.1002/adem.201700469 ↗
37. Hydrogen trapping in some automotive martensitic advanced high-strength steels10.1002/adem.201700468 ↗
38. Standard Test Methods for Tension Testing of Metallic Materials, in: ASTM E8, 2016.
39. Determining Volume Fraction by Systematic Manual Point Count, in: ASTM E562, 2011.
40. EBSD as a tool to identify and quantify bainite and ferrite in low‐alloyed Al‐TRIP steels10.1111/j.1365-2818.2008.02010.x ↗
41. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
42. Kernel average misorientation confidence index correlation from FIB sliced Ni-Fe-Cr alloy surface10.1017/S1431927611002996 ↗
43. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
44. Identifying slip systems around indentations in FCC metals10.1016/j.scriptamat.2003.08.021 ↗
45. Formation of slip steps and growth of extrusions within persistent slip bands in cyclically deformed polycrystals10.1016/j.msea.2007.06.044 ↗
46. On the effect of plastic pre-straining on the corrosion behaviour of a duplex stainless steel and how the emergence of slip steps affects the hydrogen evolution reaction kinetics10.1016/j.corsci.2020.109167 ↗
47. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
48. Hydrogen microprint analysis on the effect of dislocations on grain boundary hydrogen distribution in steels10.2355/isijinternational.ISIJINT-2015-329 ↗
49. Observation of trapping sites of hydrogen and deuterium in high-strength steels by using secondary ion mass spectrometry10.2320/matertrans1989.36.1134 ↗
50. The influence of microstructure on the trapping and diffusion of hydrogen in a low carbon steel10.1016/0010-938X(91)90097-9 ↗
51. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
52. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
53. Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
54. Fracture elongation of brittle/ductile multilayered steel composites with a strong interface10.1016/j.scriptamat.2008.07.020 ↗
55. Dislocation substructures in mild steel deformed in simple shear10.1016/0921-5093(89)90331-6 ↗
56. Structure and properties of ultrafine-grained materials produced by severe plastic deformation10.1016/0921-5093(93)90717-S ↗
57. Deformation induced vacancies with severe plastic deformation: measurements and modelling10.4028/www.scientific.net/MSF.503-504.57 ↗
58. The development of vacancies during severe plastic deformation10.2320/matertrans.MF201937 ↗
59. Thermodynamic parameters evolution versus plastic strain during HER on nickel in sulphuric acid10.1016/j.electacta.2006.11.029 ↗
60. Influence of plastic strain on the hydrogen evolution reaction on nickel (100) single crystal surfaces to improve hydrogen embrittlement10.1016/j.msea.2013.04.052 ↗
61. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
62. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
63. Hydrogen trapping in alloys studied by thermal desorption spectrometry10.1016/j.jallcom.2018.03.066 ↗
64. Effects of prior cold work on hydrogen trapping and diffusion in API X-70 line pipe steel during electrochemical charging10.5006/0990 ↗
65. Trap theory of hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
66. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(99)00094-6 ↗
67. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
68. Hydrogen embrittlement (HE) phenomena and mechanisms
69. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)10.1007/BF02642048 ↗
70. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
71. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
72. Electrochemical and Mechanical Aspects of Hydrogen Embrittlement Evaluation of Martensitic Steels, in: Reference Module in Chemistry
73. T. Yasutomi, T. Matsuno, S. Yonemura, T. Yoshida, Shearing method, in, Google Patents, 2018.
74. FE simulations and experimental analysis of the blade angle effect on sheared surface in trimming process of advanced high-strength steel sheet
75. H.-C. Shih, C. Chiriac, M.F. Shi, The effects of ahss shear edge conditions on edge fracture, in: ASME 2010 international manufacturing science and engineering conference, American Society of Mechanical Engineers, 2010, pp. 599–608.10.1115/MSEC2010-34062 ↗
76. Delayed fracture in cold blanking of ultra-high strength steel sheets10.1016/j.cirp.2019.04.111 ↗
77. Warm and hot punching of ultra high strength steel sheet10.1016/j.cirp.2008.03.125 ↗
78. Blanking method with aid of scrap to reduce tensile residual stress on sheared edge