The behaviour of iron-containing intermetallic particles in aluminium alloys in alkaline solution
Source abstract
Abstract
The behaviour of Fe-containing particles during alkaline etching and desmutting of AA5052 aluminium alloy is investigated by quasi in situ monitoring of the compositional and morphological evolution of the particles. In alkaline solution, multi-layered oxide/hydroxide films are rapidly formed on the particles, rendering them electrochemically inactive. The particles are inactive in nitric acid due to formation of thin alumina layer. The treatment doesn’t significantly change the total population of Fe-containing particles with the population of Al3Fe being reduced and that of Al(Fe,Mn,Cr)Si remaining almost unchanged. Further, relevance of the observed behaviour to localized corrosion of aluminium alloys is also discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Anodic Oxide Films and Nanostructures · Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Mondolfo · 1976 · 806
2. Polmear · 2005
3. Sheasby · 1987
4. Discontinuities in the porous anodic film formed on AA2099-T8 aluminium alloy10.1016/j.corsci.2011.08.023 ↗
5. The behaviour of second phase particles during anodizing of aluminium alloys10.1016/j.corsci.2010.03.029 ↗
6. Effect of iron-containing intermetallic particles on film structure and corrosion resistance of anodized AA2099 alloy10.1149/2.1361809jes ↗
7. In situ and operando AFM and EIS studies of anodization of Al 6060: influence of intermetallic particles10.1149/2.0061610jes ↗
8. Anodizing of multiphase aluminium alloys in sulfuric acid: insitu electrochemical behaviour and oxide properties10.1016/j.electacta.2016.06.131 ↗
9. Effect of alkaline-etch pretreatment on the pitting corrosion of wrought aluminum10.5006/1.3583956 ↗
10. Electrochemical behavior of aluminum-base intermetallics containing iron10.1149/1.2086441 ↗
11. Surface morphological changes of aluminium alloys in alkaline solution10.1016/S0010-938X(98)00188-7 ↗
12. Reaction rates of second-phase constituents in aluminium during etching, brightening and oxalic Acid anodizing processes10.1080/00202967.1968.11870048 ↗
13. Reaction of second-phase constituents in aluminium during etching in sodium hydroxide based solutions10.1080/00202967.1969.11870081 ↗
14. The effect of different aluminum alloy surface compositions on barrier anodic film formation10.1149/1.2115230 ↗
15. Surface texture formed on AA2099 Al-Li-Cu alloy during alkaline etching10.1016/j.corsci.2012.09.032 ↗
16. Alkaline etching and desmutting of aluminium alloys: the behaviour of Mg2Si particles10.1016/j.jallcom.2020.155834 ↗
17. Influence of pre-treatments on the surface condition of 2024-T3 aluminium alloy10.1080/00202967.2000.11871334 ↗
18. Nanoscale enrichments of substrate elements in the growth of thin oxide films10.1016/S0010-938X(97)89339-0 ↗
19. Electrolytic dissolution of binary alloys containinga noble metal10.1149/1.2426709 ↗
20. Computer simulations of corrosion: selective dissolution of binary alloys10.1080/01418618908209817 ↗
21. Curvature effects in alloy dissolution10.1149/1.2220924 ↗
22. Relationship between the parting limit for de-alloying and a particular geometric high-density site percolation threshold10.1080/14786430903025708 ↗
23. Mechanisms and morphology evolution in dealloying10.1149/2.064306jes ↗
24. Investigation of the de-alloying behaviour of θ-phase (Al2Cu) in AA2024-T351 aluminium alloy10.1016/j.corsci.2016.03.003 ↗
25. Investigation of dealloying of S phase (Al2CuMg) in AA 2024-T3 aluminium alloy using high resolution 2D and 3D electron imaging10.1016/j.corsci.2015.11.013 ↗
26. Dealloying of Al2CuMg in alkaline media10.1149/1.1393896 ↗