journal article·2020-07

The effect of Gd addition on the cyclic oxidation behavior and creep life of alumina-forming Ni-based superalloy

Dae Won Yun, Seong Moon Seo, Hi Won Jeong, Young Soo Yoo

Corrosion Science· Volume 170
Publisher page

Abstract

Abstract The oxidation resistance and creep property of alumina-forming Ni-based superalloys with varying amounts of Gd are studied at 1100 ℃ in ambient air. Regardless of the Gd content, from the outermost surface inwards, a typical oxide scale consists primarily of NiO, spinel, spinel with oxide particles containing refractory elements, and Al2O3. However, spallation and abnormal growth of the scale are observed in alloys without Gd, and Gd addition significantly improves oxidation resistance. The creep rupture life is almost identical for the alloys with 0.04 wt.% Gd and those without Gd. The addition of Gd improves alloy oxidation resistance without compromising creep property.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. The role of Cr and Si in affecting high-temperature oxidation behaviour of minor Dy doped NiAl alloys10.1016/j.corsci.2013.08.020 ↗
2. The effects of the minor alloying elements Al, Si and Mn on the cyclic oxidation of Ni–Cr–W–Mo alloys10.1016/j.corsci.2014.02.015 ↗
3. Effects of Al and Ta on the high temperature oxidation of Ni-based superalloys10.1016/j.corsci.2014.10.025 ↗
4. Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2 at 700 °C10.1016/j.corsci.2017.11.005 ↗
5. The oxidation behavior of Ni–15Cr–5Al–xSi (x = 0, 1, 3, 5 wt%) alloys in air at 1100 °C10.1007/s11085-019-09922-0 ↗
6. Effect of Cr on microstructural evolution of aluminized fourth generation Ni-base single crystal superalloys10.1016/j.surfcoat.2011.11.029 ↗
7. On the creep and phase stability of advanced Ni-base single crystal superalloys10.1016/j.msea.2008.02.008 ↗
8. The precipitation of topologically close-packed phases in rhenium-containing superalloys10.1016/S1359-6454(01)00265-8 ↗
9. Developing an advanced Si-bearing DS Ni-base superalloy10.1016/j.jallcom.2013.09.193 ↗
10. The physical metallurgy of a silicon-containing low expansion superalloy, Superalloys 1988
11. Development of Si-bearing 4th generation Ni-base single-crystal superalloys, Superalloys 2008
12. The effect of reactive element additions on the selective oxidation, growth and adhesion of chromia scales10.1016/0921-5093(95)09798-8 ↗
13. Improvements in high temperature oxidation resistance by additions of reactive elements or oxide dispersions10.1098/rsta.1980.0124 ↗
14. Microstructure, adhesion and growth kinetics of protective scales on metals and alloys10.1007/BF00656571 ↗
15. The high-temperature oxidation of nickel-20 wt. % chromium alloys containing dispersed oxide phases10.1007/BF00614617 ↗
16. Experimental observations in support of the dynamic-segregation theory to explain the reactive-element effect10.1007/BF01046818 ↗
17. Characterization of alumina scales grown on a 2nd generation single crystal Ni superalloy during isothermal oxidation at 1050, 1100 and 1150 °C10.1007/s11085-014-9487-2 ↗
18. Segregation studies of oxidized Y and Zr doped NiAl10.1002/maco.19950460405 ↗
19. Chromia scale growth in alloy oxidation and the reactive element effect10.1149/1.2220920 ↗
20. Effects of rare-earth dopants on the thermally grown Al2O3/Ni(Al) interface: the first-principles prediction10.1007/s10853-013-7968-3 ↗
21. Interfacial segregation, pore formation, and scale adhesion on NiAl alloys10.1007/s11085-005-1954-3 ↗
22. The oxidation behavior of Y2O3-dispersed β-NiAl10.1023/B:OXID.0000025335.62402.79 ↗
23. The oxidation behavior of oxide-dispersed β-NiAl: I. Short-term performance at 1200°C10.1023/A:1018894711276 ↗
24. High temperature oxidation resistance of Ni-(5∼13)Co-(10∼16)Cr-(5∼9)W-5Al-(1∼1.5)Ti-(3∼6)Ta alloys10.1007/s12540-016-6305-1 ↗
25. Cyclic oxidation of β-NiAl with various reactive element dopants at 1200 °C10.1016/j.corsci.2012.09.010 ↗
26. The development of Cr2O3 scales on iron-chromium alloys containing reactive elements10.1016/0010-938X(89)90057-7 ↗
27. Cyclic oxidation behaviour of rare earth oxide coated Fe–20Cr alloys10.1179/174329406X122847 ↗
28. Effect of surface deposited rare earth oxide gel characteristics on cyclic oxidation behavior of Fe20-Cr alloys10.1590/S1516-14392006000200016 ↗
29. Effect of rare earth oxide dispersion on the oxidation of Ni-15Cr sintered alloy10.2320/matertrans1960.24.839 ↗
30. Effect of Sm, Gd, Yb, Sc and Nd as reactive elements on oxidation behaviour of β-NiAl at 1200 °C10.1016/j.corsci.2013.10.021 ↗
31. The role of rare earths and reactive elements in high-temperature oxidation behavior of Fe–20Cr alloy10.2320/matertrans1960.20.299 ↗
32. Improving the oxidation resistance and electrical properties of ferritic stainless steels for application in SOFC interconnects10.1007/s11085-015-9605-9 ↗
33. Role of rare-earth elements on high temperature oxidation behavior of Fe-Cr, Ni-Cr and Ni-Cr-Al alloys10.1016/0010-938X(93)90303-X ↗
34. Effect of refractory elements and Al on the high temperature oxidation of Ni-base superalloys and modelling of their oxidation resistance10.1016/j.jallcom.2017.03.179 ↗
35. A 5th Generation SC superalloy with balanced high temperature properties and processability
36. Grain boundary segregation of cation dopants in α-Al2O3 scales10.1149/1.1838563 ↗
37. Creep of CMSX-4 single crystals of different orientations in tension and compression10.1016/0921-5093(95)10052-0 ↗
38. Process and alloy optimization for CMSX-4 superalloy single crystal airfoils