journal article·2023-11

Temperature-dependent oxidation kinetics and mechanical properties degradation of Cf/ZrB2-SiC composites

Zhangwen Wang, Bing Wang, Sai Li, Xiangyu Jin, Xinghong Zhang, Songhe Meng, Guodong Fang

Corrosion Science· Volume 224
Publisher page

Abstract

The oxidation kinetics and microstructures evolution of C f/ZrB 2 -SiC composites are investigated by experimental characterizations. An empirical model containing multi-reaction systems is further established for predicting the specimen mass evolution during isothermal oxidantion. Based on the morphological observations and in-situ tensile responses, three oxidation mechanisms of carbon phase controlled by reaction and diffusion kinetic are categorized as uniform, non-uniform and superficial oxidation. The relationship between fracture modes and internal fibers microstructures indicates that the structural origin of the fracture mode transition is the toughening mechanism transition of fibers on the ceramics matrix induced by oxidative damage.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Material property requirements for analysis and design of UHTC components in hypersonic applications[J]10.1016/j.jeurceramsoc.2010.01.026 ↗
2. preparation and properties of carbon fiber reinforced ultra-high temperature ceramic composites for aerospace applications: a review[J]10.1016/j.jmst.2016.08.004 ↗
3. Achieving the synergy of superior damage tolerance and oxidation resistance of 2D Cf/ZrB2-SiC composites via fiber heat treatment [J]10.1016/j.apsusc.2021.149807 ↗
4. Continuous carbon fiber reinforced ZrB2-SiC composites fabricated by direct ink writing combined with low-temperature hot-pressing [J]10.1016/j.jeurceramsoc.2022.03.045 ↗
5. In situ studies of oxidation of ZrB2 and ZrB2-SiC composites at high temperatures[J]10.1016/j.jeurceramsoc.2010.03.009 ↗
6. Thermophysical properties of ZrB2 and ZrB2-SiC ceramics[J]10.1111/j.1551-2916.2008.02268.x ↗
7. Effect of carbon nanotube on processing, microstructural, mechanical and ablation behavior of ZrB2-20SiC based ultra-high temperature ceramic composites[J]10.1016/j.carbon.2016.10.002 ↗
8. Inhomogeneous oxidation of ZrB2-SiC ultra-high-temperature ceramic particulate composites and its mitigation[J]10.1016/j.actamat.2017.02.076 ↗
9. Influence of silicon carbide particle size on the microstructure and mechanical properties of zirconium diboride-silicon carbide ceramics[J]10.1016/j.jeurceramsoc.2006.07.003 ↗
10. Temperature-dependent fracture strength and the effect of oxidation for ZrB2-SiC ceramics[J]10.1016/j.jeurceramsoc.2017.12.021 ↗
11. Improved microstructure and fracture properties of short carbon fiber-toughened ZrB2-based UHTC composites via colloidal process[J]10.1016/j.ijrmhm.2016.07.010 ↗
12. Synergistic reinforcement effects of ZrB2 on the ultra-high temperature stability of Cf/SiC composite fabricated by liquid silicon infiltration[J]10.1016/j.jeurceramsoc.2023.02.048 ↗
13. Influence of pressure on the oxidation resistance of carbon fiber reinforced ZrB2/SiC composites at 2000 and 2200 ̊C[J]10.1016/j.corsci.2021.109377 ↗
14. Influence of Y2O3 addition on the mechanical and oxidation behaviour of carbon fibre reinforced ZrB2/SiC composites[J]10.1016/j.jeurceramsoc.2020.06.043 ↗
15. Efficacy of a ZrB2-SiC matrix in protecting C fibres from oxidation in novel UHTCMC materials[J]10.1016/j.matdes.2016.09.104 ↗
16. Oxidation behavior and ablation mechanism of Cf/ZrB2-SiC composite fabricated by vibration-assisted slurry impregnation combined with low-temperature hot pressing [J]10.1016/j.corsci.2019.108181 ↗
17. Oxidation behaviour of a continuous carbon fibre reinforced ZrB2-SiC composite[J]10.1016/j.corsci.2017.04.012 ↗
18. Real-time quantitative imaging of failure events in materials under load at temperatures above 1,600 ̊C[J]10.1038/nmat3497 ↗
19. Oxidation degradation and mechanical reduction on C/SiC composites with artificial notch defects[J]10.1016/j.ceramint.2018.04.234 ↗
20. Simplified approach to study oxidative damage of C/SiC composites induced from notch defects[J]10.1016/j.ceramint.2019.07.267 ↗
21. Tensile behavior and microstructural evolution of a carbon/silicon carbide composite in simulated re-entry environments[J]
22. Tensile properties of two-dimensional carbon fiber reinforced silicon carbide composites at temperatures up to 1800° C in air[J]10.1016/j.eml.2019.100546 ↗
23. Oxidation effects on the mechanical properties of 2D woven C/SiC composites[J]10.1016/0955-2219(94)90105-8 ↗
24. Oxidation behavior of C/SiC-SiBCN composites at high temperature[J]10.1016/j.jeurceramsoc.2019.04.025 ↗
25. Oxidation of carbon fiber-reinforced silicon carbide matrix composites at reduced oxygen partial pressures[J]10.1111/j.1551-2916.2010.04376.x ↗
26. Modeling the effects of thermal and mechanical load cycling on a C/SiC composite in oxygen/argon mixtures[J]10.1016/j.carbon.2007.06.051 ↗
27. Effect of oxidation and residual stress on mechanical properties of SiC seal coated C/SiC composite[J]10.1016/j.ceramint.2017.10.085 ↗
28. Oxidation effects on in-plane and interlaminar shear strengths of two-dimensional carbon fiber reinforced silicon carbide composites[J]10.1016/j.carbon.2015.10.091 ↗
29. Crack opening behavior in ceramic matrix composites[J]10.1111/jace.14976 ↗
30. Influence of SiC content on the oxidation of carbon fibre reinforced ZrB2/SiC composites at 1500 and 1650 ̊C in air[J]10.1016/j.jeurceramsoc.2018.04.064 ↗
31. Effect of carbon fiber preform structures on the mechanical properties of Cf@PyC/SiC composites[J]10.1016/j.jallcom.2022.167400 ↗
32. Significant improvement of ultra-high temperature oxidation resistance of C/SiC composites upon matrix modification by SiHfBCN ceramics[J]10.1016/j.compositesb.2023.110553 ↗
33. Microstructure and mechanical behaviors of 2D-Cf/ZrB2-SiC composites at elevated temperatures[J]10.1016/j.jeurceramsoc.2022.05.063 ↗
34. Effect of PyC interphase thickness on mechanical behaviors of SiBC matrix modified C/SiC composites fabricated by reactive melt infiltration[J]10.1016/j.carbon.2014.05.092 ↗
35. Evaluation of the effect of PyC coating thickness on the mechanical properties of T700 carbon fiber tows[J]10.1016/j.apsusc.2018.08.195 ↗
36. Characterization and mechanical properties of Cf /ZrB2-SiC composites fabricated by a hybrid technique based on slurry impregnation, polymer infiltration and pyrolysis and low-temperature hot pressing [J]10.1016/j.ceramint.2018.12.001 ↗
37. Ceramic matrix composite corrosion models [J]10.1016/j.jeurceramsoc.2004.12.010 ↗
38. Oxidation kinetics and stress effects for the oxidation of continuous carbon fibers within a microcracked C/SiC ceramic matrix composite[J]10.1111/j.1551-2916.2007.02170.x ↗
39. Study on toughening mechanisms of pyrolytic carbon interface layer in Cf/ZrB2-SiC composites using in-situ tensile experimental and numerical methods[J]10.1016/j.jeurceramsoc.2021.04.028 ↗
40. Improved mechanical properties and fracture mechanism of C/C composites with salt treatment monitored by synchrotron-based in-situ tensile XRD[J]10.1016/j.compositesb.2020.108274 ↗
41. Experimental results on the elevated temperature tensile response of SiC/SiC ceramic matrix notched composites[J]. Composites Part B: Engineering
42. Advanced structural ceramics in aerospace propulsion[J]10.1038/nmat4687 ↗
43. Impact of residual stress on thermal damage accumulation, and Young's modulus of fiber-reinforced ultra-high temperature ceramics[J]10.1016/j.matdes.2018.10.019 ↗
44. Oxidation of carbon fiber-reinforced silicon carbide matrix composites at reduced oxygen partial pressures[J]10.1111/j.1551-2916.2010.04376.x ↗
45. Oxidation microstructure studies of reinforced carbon/carbon[J]10.1016/j.carbon.2005.11.013 ↗
46. Microscale characterization of damage accumulation in CMCs[J]10.1016/j.jeurceramsoc.2020.05.077 ↗
47. Effects of temperature and stress on the oxidation behavior of a 3D C/SiC composite in a combustion wind tunnel[J]10.1016/j.compscitech.2009.12.025 ↗
48. Unified tensile model for unidirectional ceramic matrix composites with degraded fibers and interface[J]10.1016/j.jeurceramsoc.2018.09.006 ↗
49. Toughening materials: enhancing resistance to fracture[J]10.1098/rsta.2020.0437 ↗
50. Multiscale investigation on fatigue properties and damage of a 3D braided SiC/SiC+ PyC/SiC composites in the full stress range at 1300° C[J]10.1016/j.jeurceramsoc.2021.11.045 ↗