journal article·2022-12

Improvement mechanism of the oxidation resistance of Al-doped Ti(C,N)-based cermets: Influence of enriched Al in the subsurface oxide layer

A.Q. Li, N. Lin, L.W. Xu, W.J. Zhang, X.C. Zhang, Z.Y. Wang, C. Ma

Corrosion Science· Volume 209
Publisher page

Abstract

The effects of Al doping on the oxidation kinetics and oxidation mechanism of Ti(C,N)-based cermets were investigated systematically. During the preparation process, Al derived from decomposed AlN powders promoted the precipitation of (Ni,Co) 3 Al nanoparticles in the binder phase of the cermets. The formation of (Ni,Co)(W,Mo)O 4 and Co 2NiO 4 oxides provided essential oxidation resistance for the cermets. The presence of (Ni,Co) 3 Al nanoparticles was found to promote oxidation resistance by forming a continuous (Ni,Co)(Ti,Al)O 3 layer within subsurface oxide layers. After 20 h of oxidation at 800 ℃, the weight gain of cermets containing 2.0 wt% AlN was only 67.49 % of that of the pure cermets.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. The evaluation of tribo-corrosion synergy for WC–Co hardmetals in low stress abrasion10.1016/j.wear.2003.04.001 ↗
2. Mechanism of the early stages of oxidation of WC-Co cemented carbides10.1016/j.corsci.2015.11.007 ↗
3. Enhanced oxidation resistance of Ti(C,N)- based cermets containing Ta10.1016/j.corsci.2014.03.007 ↗
4. Oxidation of WC-Co, WC-Ni and WC-Co-Ni hard metals in the temperature range 500–800°C10.1016/0263-4368(96)00009-1 ↗
5. Strength degradation of a tungsten carbide-cobalt composite at elevated temperatures10.1016/S1044-5803(98)00056-4 ↗
6. Toughened ultra-fine (Ti,W)(C,N)–Ni cermets10.1016/j.scriptamat.2004.09.017 ↗
7. Effects of secondary carbides on the microstructure, mechanical properties and erosive wear of Ti(C, N)-based cermets10.1016/j.ceramint.2016.10.024 ↗
8. Study on the formation of core-rim structure in Ti(CN)-based cermets10.1016/j.ijrmhm.2012.03.012 ↗
9. Fabrication and cutting performance of Ti(C,N)-based cermet tools used for machining of high-strength steels10.1016/j.ceramint.2017.02.034 ↗
10. Effect of WC Addition and Cooling Rate on Microstructure, Magnetic and Mechanical Properties of Ti(C0.6,N0.4)-WC-Mo-Ni Cermets10.1016/j.ijrmhm.2019.105001 ↗
11. The Effects of Mo2C Additions on the Microstructure and Sliding Wear of TiC0.3N0.7-Ni3Al Cermets10.1016/j.ijrmhm.2015.01.013 ↗
12. Effects of Cr3C2 addition on the corrosion behavior of Ti(C, N)-based cermets10.1016/j.ijrmhm.2011.10.013 ↗
13. Effect of AlN content on microstructure and properties of Ti(C,N)-Based cermet
14. Early high temperature oxidation behaviour of Ti(C,N)-based cermets in air10.1016/j.corsci.2010.05.028 ↗
15. High temperature oxidation resistance of (Ti,Ta)(C,N)-based cermets10.1016/j.corsci.2015.10.001 ↗
16. Oxidation-abrasion of TiC-based cermets in SiC medium10.1016/j.wear.2011.05.005 ↗
17. Kinetics of high-temperature oxidation of (Ti,Ta)(C,N)-based cermets10.1016/j.corsci.2015.10.006 ↗
18. Microstructure and oxidation behavior of Ti(C,N)-based cermets with in situ synthesized Ni3Al phase10.1016/j.ijrmhm.2018.02.008 ↗
19. High temperature oxidation behaviors of Ni3Al-bonded cermets10.1016/j.jallcom.2017.02.034 ↗
20. Improvement in wear and corrosion resistance of Ti(C,N)-based cermets via Aluminum nitride additions10.1016/j.vacuum.2019.108849 ↗
21. Characterization of oxide scales to evaluate high temperature oxidation behavior of Ti(C,N)-based cermets in static air10.1016/j.jallcom.2010.07.031 ↗
22. High-temperature oxidation resistance, mechanical and wear resistance properties of Ti(C,N)-based cermets with Al0.3CoCrFeNi high-entropy alloy as a metal binder10.1016/j.jallcom.2019.152486 ↗
23. Investigation of the oxidation behavior and high oxidation-resistant mechanism of Ti(C,N)-based cermets10.1016/j.corsci.2020.108959 ↗
24. Influence of ZrC addition on the microstructure, mechanical properties and oxidation resistance of Ti(C,N)-based cermets10.1016/j.ceramint.2018.03.131 ↗
25. Thermodynamic modeling of Al–Co–Cr, Al–Co–Ni, Co–Cr–Ni ternary systems towards a description for Al–Co–Cr–Ni10.1016/j.calphad.2015.12.007 ↗
26. Effect of TiB2/WC addition on the oxidation behavior of Ti(C,N)-304ss cermets during the early oxidation stage10.1016/j.corsci.2019.108118 ↗
27. Kubaschewski · 1993
28. Driving force and growth mechanism for spontaneous oxide nanowire formation during the thermal oxidation of metals10.1016/j.actamat.2010.12.052 ↗
29. On the mechanisms of grain boundary migration10.1016/S1359-6454(01)00343-3 ↗
30. Isothermal oxidation behavior characteristics of a second generation Ni-base single crystal superalloy in Air at 1000 and 1100°C10.1016/S1452-3981(23)18000-X ↗
31. Plasma electrolytic deposition of α-Al2O3 on TiNb fibres and their mechanical properties10.1016/j.ceramint.2021.08.190 ↗
32. Crack generation in blast furnace slag bearing high titanium by microwave cyclic heating10.2355/isijinternational.47.193 ↗
33. Sintering behavior and microwave dielectric properties of (Ca, La)(Ti, Al)O3 ceramics10.1143/JJAP.38.6821 ↗
34. Insights into the performance of CoxNi1−xTiO3 solid solutions as photocatalysts for sun-driven water oxidation10.1021/acsami.7b12994 ↗