Abstract The oxidation behaviour of Fe-20Mn-8Al-xC (x = 0.25-0.35 wt. %) duplex light-weight steels at 1000 °C in dry air has been investigated. The results show that the increased carbon content enlarges austenite phase fractions and degrades oxidation resistance to high temperature. The preferential oxidation of manganese at high temperature promotes phase transformation of austenite → ferrite, and offers pathways for aluminium diffusion. Aluminium enriches at the boundary of the austenite internal oxidation layer. A continuous and compact pure Al2O3 layer has been observed between iron and manganese oxides and oxidation-induced ferrite layers. The formed Al2O3 layer can further prevent oxidation of Fe-20Mn-8Al-xC duplex steels.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Analysis of thermo-visco-plastic behaviour of six high strength steels10.1016/j.matdes.2008.07.034 ↗
2. Physical and mechanical properties of iron aluminum-(Mn, Si) lightweight steels10.1051/metal:2000110 ↗
3. An analysis of the deformation characteristics of a dual phase twinning-induced plasticity steel in warm working temperature regime10.1016/j.matdes.2012.04.019 ↗
4. Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes10.2355/isijinternational.43.438 ↗
5. Deformation behaviour of ferrite-austenite duplex lightweight Fe-Mn-Al-C steel10.1016/j.scriptamat.2011.12.026 ↗
6. Microband-induced plasticity in a high Mn-Al-C light steel10.1016/j.msea.2008.05.042 ↗
7. Evolution of microstructure and mechanical properties during thermomechanical processing of a low-density multiphase steel for automotive application10.1016/j.actamat.2014.04.031 ↗
8. Effects of ferrite volume fraction on the tensile deformation characteristics of dual phase twinning induced plasticity steel10.1016/j.matdes.2013.06.033 ↗
9. Effects of Al addition on high strain rate deformation of fully austenitic high Mn steels10.1016/j.msea.2011.06.020 ↗
10. Temperature dependence of the flow stress of Fe-18Mn–0.6C-xAl twinning-induced plasticity steel10.1016/j.actamat.2013.07.042 ↗
11. Effect of annealing temperature on microstructural modification and tensile properties in 0.35C–3.5Mn-5.8Al lightweight steel10.1016/j.actamat.2013.04.038 ↗
12. Microstructure and tensile behaviour of duplex low-density steel containing 5 mass % aluminum10.1016/j.scriptamat.2012.09.030 ↗
13. Tensile deformation of low density duplex Fe-Mn-Al-C steel10.1016/j.matdes.2015.03.043 ↗
14. Factors influencing the tensile behaviour of a Fe-28Mn-9Al-0.8C steel10.1016/j.msea.2008.12.055 ↗
15. Tensile deformation of a duplex Fe-20Mn-9Al-0.6C steel having the reduced specific weight10.1016/j.msea.2011.03.045 ↗
16. A model for heat conduction through the oxide layer of steel during hot rolling10.1016/S0924-0136(00)00569-0 ↗
17. Cracking and deformation of surface scale during hot rolling of steel10.1179/026708301225000761 ↗
18. The effect of scaling on interfacial friction in hot rolling of steels10.1016/S0924-0136(98)00392-6 ↗
19. Formation and growth morphology of nodules in the high-temperature oxidation of Fe-Mn-Al-C alloy10.1016/S0254-0584(02)00134-7 ↗
20. Oxidation induced phase transformation of duplex stainless steel 25Cr-10Mn-2Ni-3Mo-0.8W-0.8Cu-.5N10.1016/j.corsci.2011.10.024 ↗
21. NaCl-induced hot corrosion of Fe-Mn-Al-C alloys10.1016/S0254-0584(01)00515-6 ↗
22. Improved oxidation resistance of 15wt.% Cr ferritic stainless steels containing 0.08–2.45wt.% Alat 1000°C in air10.1016/j.corsci.2015.08.007 ↗
23. High temperature oxidation of Fe-Al and Fe-Cr-Al alloys: the role of Cr as a chemically active element10.1016/j.corsci.2010.06.019 ↗
24. The effects of Cr and Al concentrations on the oxidation behaviour of oxide dispersion strengthened ferritic alloys10.1016/j.corsci.2013.07.004 ↗
25. Criteria for the formation of protective Al2O3 scales on Fe-Al and Fe-Cr-Al alloys10.1016/j.corsci.2005.01.012 ↗
26. A study of the oxidation of FeCrAl alloy in pressurized water and high-temperature steam environment10.1016/j.corsci.2015.02.027 ↗
27. High temperature oxidation of iron-manganese-aluminum based alloys10.1007/BF00741468 ↗
28. Microstructural development in the oxidation-induced phase transformation of Fe-Al-Cr-Mn-C alloys10.1007/BF01111928 ↗
29. Formation and growth morphology of oxidation-induced ferrite layer in Fe-Mn-AI-Cr-C alloys10.1007/BF01045765 ↗
30. Nitrogen-induced selective high-temperature internal oxidation behaviour in duplex stainless steels 19Cr-10Mn-0.3Ni-xN10.1016/j.corsci.2015.06.013 ↗
31. GB/T228-2010 · 2010
32. The Thermo-Calc databank system10.1016/0364-5916(85)90021-5 ↗
33. 1999
34. Thermodynamic calculation on the stability of (Fe, Mn)3AlC carbide in high aluminum steels10.1016/j.jallcom.2010.06.032 ↗
35. Glass coating on stainless steels for high temperature oxidation protection: mechanisms10.1016/j.corsci.2014.01.033 ↗
36. Oxidation behaviour of chromium nitride films10.1016/j.tsf.2006.06.039 ↗
37. High-temperature oxidation of duplex stainless steels S32101 and S32304 in air and simulated industrial reheating atmosphere10.1016/j.corsci.2010.04.033 ↗
38. Effect of carbon on cavity formation during the high-temperature oxidation of Ni10.1007/BF00603786 ↗
39. The high temperature oxidation of metals forming cation-diffusing scales10.1007/BF02644552 ↗
40. Influence of the alloy grain size on the oxidation behaviour of PM2000 alloy10.1016/S0010-938X(01)00182-2 ↗
41. Raman spectroscopy of thin corrosion films on iron at 100 to 150C in Air10.5006/1.3583054 ↗
42. Raman spectra of possible corrosion products of iron10.1366/000370278774330739 ↗
43. The air oxidation of an austenitic Fe-Mn-Cr stainless steel for fusion-reactor applications10.1007/BF00655899 ↗
44. Re-investigating the CO oxidation mechanism over unsupported MnO, Mn2O3 and MnO2 catalysts10.1016/j.cattod.2007.10.061 ↗
45. Controlled synthesis of Mn3O4 and MnCO3 in a solvothermal system10.1016/j.materresbull.2009.03.004 ↗
46. Thin film of aluminum oxide through pulsed laser deposition: a micro-Raman study10.1016/S0921-5107(00)00554-7 ↗
47. Enhance methane combustion over NiAl2O4-interface-promoted Pd/γ-Al2O310.1016/j.jcat.2015.12.031 ↗