Abstract

The aim of the present study was to evaluate the efficacy of different methods of sulphide microencapsulation in terms of inhibiting sulphide oxidation in roofing slate. For this, a preliminary test was carried out with ground pyrite and the methods that provided the best results were applied to samples of roofing slate. Protection against oxidation was measured by the amount of iron released after enforced oxidation with H2O2 in the tests with pyrite, and by thermal cycle alteration, SO2 and saline spray tests (EN 12326-2:2000 and EN 14147:2004) in the tests with the slate samples. The results indicate that treatments with potassium phosphate and potassium silicate, proposed for controlling acid mine drainage, were the most effective at protecting pyrite against oxidation, and that these methods are also effective when applied to slate. © 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mine drainage and remediation techniques · Tailings Management and Properties · Metal Extraction and Bioleaching

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Spanish roofing slate deposits
2. The geology of roofing slate
3. Factores de calidad en la elaboración de placas de pizarra para cubiertas en Galicia y León
4. Drainage waters affected by pyrite oxidation in a coal mine in Galicia (NW Spain): composition and mineral stability10.1016/S0048-9697(98)00149-1 ↗
5. Procesos de oxidación de pirita en medios superficiales: potencial acidificante e interés para la recuperación de suelos de mina
6. Microbial oxidation of piryte: experiments using microorganisms from extreme acidic environment10.2138/am-1998-11-1233 ↗
7. Stumm · 1981
8. Passivation of pyrite due to surface treatment10.1016/0016-2361(90)90209-9 ↗
9. Effect of sodium oleate on inhibiting pyrite oxidation10.1016/S0301-7516(99)00045-9 ↗
10. Pyrite oxidation inhibition by a cross-linked lipid coating10.1186/1467-4866-4-8 ↗
11. Inhibition of pyrite oxidation by a phospholipid in the presence of silicate10.1021/es0352552 ↗
12. Preventing oxidation of iron sulfide minerals by polyethylene polyamines10.1016/j.mineng.2005.04.007 ↗
13. Studies on the oxidation of pyrite in colliery spoil. The inhibition pathway and inhibition of the ferrous–ferric oxidation
14. Passivation of pyrite oxidation with metal cations10.1007/BF01161449 ↗
15. Pyrite oxidation in carbonate-buffered solution 2. Rate control by oxide coatings10.1016/0016-7037(90)90328-I ↗
16. Potential microencapsulation of pyrite by artificial inducement of ferric phosphate coatings10.2134/jeq1995.00472425002400030021x ↗
17. Evangelou · 1995
18. Pyrite microencapsulation technologies: principles and potential field application10.1016/S0925-8574(00)00156-7 ↗
19. Feasibility and cost of creating an iron–phosphate coating on pyrrhotite to prevent oxidation10.1007/s002540050078 ↗
20. X-ray photoelectron spectroscopic analyses of corrosion products formed on rock bolt carbon steel in chloride media with bicarbonate and silicate ions10.1016/j.corsci.2004.03.007 ↗
21. The passivation of iron–carbon alloys in acidic phosphate solution and its relation to stress corrosion cracking10.1016/0010-938X(85)90110-6 ↗
22. Studies of the corrosion of mild steel in alkali-activated slag cement mortars with sodium chloride admixtures by a galvanostatic pulse method10.1016/j.corsci.2005.05.035 ↗
23. Carrier – microencapsulation for preventing pyrite oxidation10.1016/j.minpro.2007.06.003 ↗
24. Protocol for assessing the effectiveness of protective coatings for roofing slate10.3989/mc.2008.v58.i289-290.68 ↗
25. Pyrite oxidation: protection using synthetic resins10.1127/ejm/9/1/0167 ↗
26. Formation of ferric hydroxide–silica coatings on pyrite and its oxidation behavior10.1097/00010694-199801000-00008 ↗
27. Causes of variation in cristal morphology in metamorphogenic pyrite depositsof the Cameros Basin (Spain)10.1002/gj.889 ↗
28. V. Cárdenes, R. de la Horra, C. Monterroso, J. García-Guinea, V. Pais, Depósitos de pizarras para cubiertas en la Península Ibérica. in: VII Congreso Geológico de España, Las Palmas de Gran Canaria, Geotemas, vol. 10, 2008, p. 453..
29. Nuevos datos geológicos y cartográficos sobre el flanco Sur del Sinclinorio de Truchas
30. Revisión Bioestratigráfica de las pizarras del Ordovícico Medio en el Noroeste de España (zonas Cantábrica, Asturoccidental – Leonesa y Centroibérica septentrional)
31. CEN/TC_128, EN 12326-2:2000, Slate and Stone Products for Discontinuous Roofing and Cladding – Part 2: Methods of Test, 2000.
32. CEN/TC_128, EN 14147:2004, Natural Stone Test Methods – Determination of Resistance to Aging by Salt Mist, 2004.
33. Image processing with ImageJ
34. Changes in rainwater pH associated with increasing atmospheric carbon dioxide after the industrial revolution water10.1007/s11270-008-9774-0 ↗