Equivalence in evaluating hydrogen-assisted fracture strength of slow strain rate tensile and constant load tensile for three precipitation-hardened martensitic stainless steels: Effect of large-sized particles
Source abstract
Abstract
This study investigated the equivalence in evaluating hydrogen-assisted fracture strength undergoing slow strain rate tensile (SSRT) and constant load tensile (CLT) for three precipitation-hardened martensitic stainless steels containing second-phase particles of different sizes. For both PH13–8Mo and 17–4PH with nano-sized precipitates, the fracture strength was higher for SSRT than for CLT. However, for 15–6PH with both nano-sized precipitates and large-sized carbides, cracks at the larger-sized carbide/matrix interface led to the lower fracture strength for SSRT. Furthermore, we concluded that the hydrogen-assisted threshold fracture strength of CLT could be estimated by using SSRT if no large-sized particles were in high-strength steels.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. The potential role of hydrogen as a sustainable transportation fuel to combat global warming10.1016/j.ijhydene.2018.10.149 ↗
2. Energy system analysis of the implications of hydrogen fuel cell vehicles in the Swedish road transport system10.1016/j.ijhydene.2015.04.160 ↗
3. Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance10.1016/j.corsci.2020.108428 ↗
4. Effect of hydrogen trapping on hydrogen permeation in a 2205 duplex stainless steel: Role of austenite–ferrite interface10.1016/j.corsci.2022.110332 ↗
5. Influence of microstructure on hydrogen embrittlement in hot-rolled medium Mn steels10.1016/j.msea.2020.139147 ↗
6. Effect of strain rate on hydrogen embrittlement in low-carbon martensitic steel10.1016/j.ijhydene.2016.09.188 ↗
7. Stress-induced hydrogen redistribution and corresponding fracture behavior of Q960E steel at different hydrogen content10.1016/j.msea.2020.138963 ↗
8. Hydrogen redistribution under stress-induced diffusion and corresponding fracture behaviour of a structural steel10.1080/02670836.2017.1325562 ↗
9. Method of evaluating delayed fracture susceptibility of tempered martensitic steel showing quasi-cleavage fracture10.1007/s11661-016-3885-9 ↗
10. Method of evaluating hydrogen embrittlement susceptibility of tempered martensitic steel showing intergranular fracture10.1007/s11661-017-4435-9 ↗
11. Crosshead speed dependence of the notch tensile strength of a high strength steel in the presence of hydrogen10.1016/j.scriptamat.2005.05.014 ↗
12. Dependence of hydrogen-induced lattice defects and hydrogen embrittlement of cold-drawn pearlitic steels on hydrogen trap state, temperature, strain rate and hydrogen content10.1016/j.actamat.2014.07.008 ↗
13. Effect of vanadium content on hydrogen embrittlement of 1400 MPa grade high strength bolt steels10.1016/j.ijhydene.2021.08.060 ↗
14. Microstructure effect on hydrogen-induced cracking in TM210 maraging steel10.1016/j.msea.2013.07.097 ↗
15. Study of correlation between hydrogen-induced stress and hydrogen embrittlement10.1016/S0921-5093(02)00600-7 ↗
16. Comparison of constant load, SSRT and CSRT methods for hydrogen embrittlement evaluation using round bar specimens of high strength steels10.2355/isijinternational.ISIJINT-2015-565 ↗
17. Hydrogen-induced cracking and service safety evaluation for precipitation strengthened austenitic stainless steel as hydrogen storage tank10.1016/j.ijhydene.2014.08.143 ↗
18. Effect of nickel on hydrogen embrittlement behavior of medium-carbon high strength steels10.1016/j.msea.2016.08.028 ↗
19. Effect of uniform distribution of fine cementite on hydrogen embrittlement of low carbon martensitic steel plates10.2355/isijinternational.52.213 ↗
20. Delayed fracture and hydrogen absorption of 1.3GPa grade high strength bolt steel10.2355/tetsutohagane1955.82.4_297 ↗
21. The mechanism of hydrogen evolution on iron in acid solutions by determination of permeation rates10.1149/1.2426195 ↗
22. The adsorption and diffusion of electrolytic hydrogen in palladium
23. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
24. Hydrogen embrittlement assessment of ultra-high strength steel 30CrMnSiNi210.1016/j.corsci.2013.08.013 ↗
25. Crank · 1979
26. Effects of Ti alloying on resistance to hydrogen embrittlement in (Nb+Mo)-alloyed ultra-high-strength hot-stamping steels10.1016/j.msea.2020.139763 ↗
27. Effect of Nb on hydrogen-induced delayed fracture in high strength hot stamping steels10.1016/j.msea.2014.12.051 ↗
28. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
29. Precise determination of the activation energy for desorption of hydrogen in two Ti-added steels by a single thermal-desorption spectrum10.1007/s11663-004-0057-x ↗
30. Combined thermal desorption spectroscopy, differential scanning calorimetry, scanning electron microscopy and X-ray diffraction study of hydrogen trapping in cold deformed TRIP steel10.1016/j.actamat.2012.01.026 ↗
31. Origin of hydrogen trapping site in vanadium carbide precipitation strengthening steel10.1016/j.actamat.2018.05.003 ↗
32. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
33. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
34. Effect of aging treatment on apparent hydrogen solubility and trapping in a new generation maraging steel10.1016/j.scriptamat.2020.03.013 ↗
35. The solubility and diffusivity of hydrogen in well-annealed and deformed iron
36. Hydrogen trapping and desorption of dual precipitates in tempered low-carbon martensitic steel10.1016/j.actamat.2020.06.046 ↗
37. Enhanced hydrogen concentrations ahead of rounded notches and cracks—competition between plastic strain and hydrostatic stress10.1016/S1359-6454(97)00364-9 ↗
38. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
39. Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel10.1016/j.msea.2005.03.008 ↗
40. Determination of the critical hydrogen concentration for delayed fracture of high strength steel by constant load test and numerical calculation10.1016/j.corsci.2005.07.010 ↗
41. Some surprising features of the plastic deformation of body-centered cubic metals and alloys10.1007/BF02664806 ↗
42. Hydrogen solubility, diffusivity and trapping in a tempered Fe–C–Cr martensitic steel under various mechanical stress states10.1016/j.msea.2011.11.084 ↗
43. Hydrogen behavior in high strength steels during various stress applications corresponding to different hydrogen embrittlement testing methods10.1016/j.msea.2018.08.002 ↗
44. Effects of lamellar structure on tensile properties and resistance to hydrogen embrittlement of pearlitic steel10.1016/j.actamat.2019.04.040 ↗
45. Permeation measurements of hydrogen trapping in 1045 steel10.1007/BF02670691 ↗
46. Hydrogen in trapping states innocuous to environmental degradation of high-strength steels10.2355/isijinternational.43.520 ↗
47. The effect of second tempering on hydrogen embrittlement of ultra-high-strength steel10.1007/s11661-020-05749-6 ↗
48. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
49. Aging condition and trapped hydrogen effects on the mechanical behavior of a precipitation hardened martensitic stainless steel10.1016/j.jallcom.2019.07.112 ↗
50. The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel10.1016/j.actamat.2017.08.011 ↗
51. Effect of aging treatment on hydrogen embrittlement of PH 13-8 Mo martensite stainless steel10.1016/j.msea.2015.09.116 ↗
52. The role of delta ferrite in hydrogen embrittlement fracture of 17-4 PH stainless steel10.1016/j.ijhydene.2022.07.257 ↗
53. Ferrite effects on the hydrogen embrittlement of 17-4PH stainless steel10.1108/ACMM-03-2022-2615 ↗
54. Crack and blister initiation and growth in purified iron due to hydrogen loading10.1016/j.actamat.2016.05.034 ↗
55. Comparative study of non-metallic inclusions on the critical size for HIC initiation and its influence on hydrogen trapping10.1016/j.ijhydene.2020.02.131 ↗
56. Effect of hydrogen content and strain rate on hydrogen-induced delay cracking for hot-stamped steel10.3390/met9070798 ↗
57. Reduction of delayed fracture susceptibility of tempered martensitic steel through increased si content and surface softening10.2355/isijinternational.53.714 ↗
58. Evaluation method of delayed fracture property of high strength steels10.2355/tetsutohagane1955.83.7_454 ↗
59. Twinning and martensite in a 304 austenitic stainless steel10.1016/j.msea.2012.05.080 ↗
60. First principles study the stability and mechanical properties of MC (M=Ti, V, Zr, Nb, Hf and Ta) compounds10.1016/j.jallcom.2013.08.045 ↗