Hot corrosion behavior of NiCr-Cr3C2-CaF2/BaF2 composite coating with NiAl bond coating in molten NaCl-KCl and NaCl-Na2SO4 at 800 ℃

J.H. Wang, D.G. Li, T.M. Shao

Corrosion Science· Volume 206
Publisher page

Abstract

The NiCr-Cr 3C 2-CaF 2/BaF 2 coating with the NiAl bond coating was sprayed on a Ni16Cr13Co4Mo(wt%) alloy by detonation-gun spray, and hot corrosion behaviors were studied by electrochemical measurements. In molten NaCl-KCl, the corrosion products were mainly Cr 2O 3. Gas phases such as Cl 2 led to spallations and cracks on the coating surface. In molten NaCl-Na 2SO 4, Na 2SO 4 decomposed and reacted with the coating. Mixed oxides formed a continuous corrosion layer, and Al diffused outward from bond coating to be oxidized. Some liquid phases existed in the corrosion layer and promoted hot corrosion. The detailed hot corrosion mechanisms in two molten salts were discussed.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Influence of molten salt with or without V2O5 on hot corrosion and high-temperature tribological performance of HVOF-sprayed Ni-based self-lubricating composite coating10.1016/j.surfcoat.2021.127210 ↗
2. Enamel coating for protection of the 316 stainless steel against tribo-corrosion in molten zinc alloy at 460 °C10.1016/j.jmst.2020.04.079 ↗
3. High temperature corrosion and wear behavior of HVOF-sprayed coating of Al2O3-NiAl on AISI 304 stainless steel10.1016/j.surfcoat.2018.12.047 ↗
4. Oxidation and hot corrosion behaviors of Mo-doped NiMoAlY alloys at 750 °C10.1016/j.corsci.2022.110262 ↗
5. High-temperature wear and cyclic oxidation behavior of (Ti, W)C reinforced stainless steel coating deposited by PTA on a plain carbon steel10.1016/j.surfcoat.2021.127736 ↗
6. Hot corrosion behaviors of directed energy deposited Inconel 718/Haynes 25 functionally graded material at 700 °C and 900 °C10.1016/j.corsci.2021.110040 ↗
7. Influence of molten salt with or without V2O5 on hot corrosion and high-temperature tribological performance of HVOF-sprayed Ni-based self-lubricating composite coating10.1016/j.surfcoat.2021.127210 ↗
8. Preparation of linseed oil-loaded porous glass bubble/wax microcapsules for corrosion- and wear-resistant difunctional coatings10.1016/j.cej.2022.135403 ↗
9. High temperature wear performance of HVOF-sprayed Cr3C2-WC-NiCoCrMo and Cr3C2-NiCr hardmetal coatings10.1016/j.apsusc.2017.04.132 ↗
10. Microstructure and wear properties of atmospheric plasma-sprayed Cr3C2-NiCr composite coatings10.1016/j.surfcoat.2021.127904 ↗
11. The effects of post-treatment on the hot corrosion behavior of the HVOF-sprayed Cr3C2–NiCr coating10.1016/j.surfcoat.2012.04.026 ↗
12. Effects of solid lubricant content on the microstructure and properties of NiCr/Cr3C2–BaF2·CaF210.1016/j.jallcom.2009.01.062 ↗
13. Derby · 2015
14. Microstructure of HVOF-sprayed Ag–BaF2⋅CaF2–Cr3C2–NiCr coating and its tribological behavior in a wide temperature range (25 °C to 800 °C)10.1016/j.ceramint.2020.08.199 ↗
15. Hot corrosion behavior of Pt+Hf co-modified NiAl coating in the mixed salt of Na2SO4-NaCl at 900 °C10.1016/j.corsci.2020.108527 ↗
16. Hot corrosion behaviour of thermally sprayed CoCrAlY coating irradiated by high-current pulsed electron beam10.1016/j.jallcom.2019.01.071 ↗
17. Hot corrosion behavior of solution precursor and atmospheric plasma sprayed thermal barrier coatings10.1016/j.corsci.2015.05.034 ↗
18. Corrosion behavior of Fe-Ni alloys in molten KF-AlF3-Al2O3 salts at 700 °C10.1016/j.corsci.2019.05.012 ↗
19. Hot corrosion behaviour of Fe–Al based intermetallic in molten NaVO3 salt10.1016/j.corsci.2009.03.028 ↗
20. Corrosion evaluation by electrochemical real-time tracking of VM12 martensitic steel in a ternary molten salt mixture with lithium nitrates for CSP plants10.1016/j.solmat.2021.111302 ↗
21. Effect of Li and Cu addition on corrosion of Fe–40at% Al intermetallics in molten LiCl–KCl eutectic salt10.1016/j.corsci.2012.02.020 ↗
22. An improved technique for molten salt corrosion sample preparation10.1016/j.solmat.2021.111057 ↗
23. ASTM G1–03, Standard Practice for Preparing, Cleaning and Evaluating Corrosion Test Specimens, West Conshohocken, PA, 2017.
24. Hot corrosion of Inconel 625 wrought alloy and weld overlay on carbon steel by gas metal arc welding in 47 PbSO4-23 ZnO-13 Pb3O4-7 PbCl2-5 CdO-5 Fe2O3 molten salt mixture10.1016/j.corsci.2021.109348 ↗
25. A review of advances in high-temperature corrosion10.1016/0921-5093(89)90712-0 ↗
26. Hot corrosion of some superalloys and role of high-velocity oxy-fuel spray coatings—a review10.1016/j.surfcoat.2004.10.056 ↗
27. Oxidation and hot corrosion of superalloys
28. Electrochemical study on the hot corrosion behavior of Ni16Cr13Co4Mo alloy in molten NaCl-KCl and NaCl-KCl-Na2SO4
29. Performance of protective oxide films on Fe–Ni alloy anodes in molten KF–AlF3–Al2O3 salts at 700 °C10.1016/j.electacta.2020.136275 ↗
30. Rearrangement of oxide scale on Ni-11Fe-10Cu alloy under anodic polarization in molten Na2CO3-K2CO310.1016/j.corsci.2018.07.014 ↗
31. Corrosion monitoring of 321H in contact with a quaternary molten salt for parabolic trough CSP plants10.1016/j.corsci.2020.109070 ↗
32. Effects of the oxidants H2O and CrF3 on the corrosion of pure metals in molten (Li,Na,K)F10.1016/j.corsci.2015.11.032 ↗
33. Electrochemical impedance models for molten salt corrosion10.1016/S0010-938X(00)00108-6 ↗
34. Electrochemical impedance of two-phase Ni–Ti alloys during corrosion in eutectic (0.62Li, 0.38K)2CO3 at 650 °C10.1016/j.electacta.2003.12.050 ↗
35. Comparative interaction of cold-worked versus annealed inconel 601 with molten carbonate salt at 450°C10.1016/j.corsci.2017.01.004 ↗
36. Evolution of corrosion on microstructure of ceramic coating produced by plasma electrolytic oxidation in molten salt10.1016/j.ceramint.2021.12.318 ↗
37. Interfacial impedance and roughness of solid electrodes; gold in perchloric acid10.1016/0013-4686(70)90008-3 ↗
38. High temperature corrosion and electrochemical behavior of INCONEL 625 weld overlay in PbSO4–Pb3O4–PbCl2–CdO–ZnO molten salt medium10.1016/j.corsci.2014.03.034 ↗
39. High temperature oxidation behaviour of combustion flame sprayed CoNiCrAlY coatings10.1016/j.surfcoat.2020.125431 ↗
40. CRC Handbook of Chemistry and Physics
41. A comparative study on the high temperature corrosion of TP347H stainless steel, C22 alloy and laser-cladding C22 coating in molten chloride salts10.1016/j.corsci.2014.03.012 ↗
42. Corrosion of steel alloys in molten NaCl + Na2SO4 at 700°C for thermal energy storage10.1016/j.solmat.2017.11.017 ↗
43. Corrosion of super-heater steel materials under alkali salt deposits. Part 2: SEM analyses of different steel materials10.1016/j.corsci.2009.11.026 ↗
44. Hot corrosion behavior of electrodeposited SiO2 coating on TiAl alloy10.1016/j.corsci.2020.108827 ↗
45. Improving hot corrosion resistance of aluminized TiAl alloy by anodization and pre-oxidation10.1016/S1003-6326(20)65487-5 ↗
46. A study on hot corrosion performance of high velocity arc-sprayed FeCrNiAlMnB/Cr3C2 coating exposed to Na2SO4 + K2SO4 and Na2SO4 + NaCl10.1016/j.surfcoat.2020.126015 ↗
47. Hot corrosion behaviour of yttrium and aluminium modified wear resistance coating alloy in mixed sulphate at 900 °C10.1016/j.corsci.2019.108369 ↗
48. Accelerated oxidation rate of chromium induced by sodium-chloride10.1007/BF00659274 ↗
49. Cation size mismatch and charge interactions drive dopant segregation at the surfaces of manganite perovskites10.1021/ja3125349 ↗
50. Relationship between microstructure and bonding strength of yttria-stabilized zirconia thermal barrier coatings10.1016/j.ceramint.2021.11.107 ↗
51. Investigation on the performance of air plasma sprayed thermal barrier coating with Lu/Hf-doped NiAl bond coat10.1016/j.surfcoat.2019.01.005 ↗
52. Goldstein · 2003 · 404
53. Evaluation of cyclic hot corrosion behaviour of detonation gun sprayed Cr3C2-25%NiCr coatings on nickel- and iron-based superalloys10.1016/j.surfcoat.2008.09.031 ↗
54. Hot corrosion studies of HVOF sprayed Cr3C2-NiCr and Ni-20Cr coatings on nickel-based superalloy at 900℃10.1016/j.surfcoat.2005.12.030 ↗
55. High velocity oxygen fuel sprayed Cr3C2-NiCr coatings against Na2SO4 hot corrosion at different temperatures10.1016/j.ceramint.2020.06.135 ↗
56. Recent development of nickelbased disc alloys and corresponding cast-wrought processing techniques
57. Electron beam welding process and microstructure and properties of joint of GH4065A alloy
58. High temperature oxidation behaviour of combustion flame sprayed CoNiCrAlY coatings10.1016/j.surfcoat.2020.125431 ↗
59. Achieving superior hot corrosion resistance by PVD/HVOF duplex design10.1016/j.corsci.2020.108845 ↗
60. 12-corrosion in molten salts
61. Influence of the combined-effect of NaCl and Na2SO4 on the hot corrosion behaviour of aluminide coating on Ni-based10.1016/j.jallcom.2019.03.165 ↗
62. The hot corrosion of 310 stainless steel with pre-coated NaCl/Na2SO4 mixtures at 750◦C10.1016/j.matchemphys.2004.10.002 ↗