journal article·2022-09

Mechanical and stress corrosion cracking behavior of welded 5059H116 alloy

Rajesh Yadav, Ankur Kumar, Gajanan P. Chaudhari, A.G. Paradkar

Corrosion Science· Volume 206
Publisher page

Abstract

5059H116 alloy is welded by friction stir welding (FSW) and gas metal arc welding (GMAW). Both welded specimens exhibited inferior strength and percent elongation as compared to base alloy. Soundness of the weld, passivating tendency of finer grains, and depletion of dissolved magnesium from the nugget zone due to discontinuous precipitation of Al 3Mg 2 phase at the Al 6 Mn/matrix interface contributed to the superior corrosion resistance of FSW alloy. Slow strain rate tests showed shorter time to failure for GMAW sample, which is attributed to the formation of microcells from chemical heterogeneities and iron-containing second phase dispersoids, and presence of micro-porosity.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Mathers · 2002
2. Influences of pin profile and rotational speed of the tool on the formation of friction stir processing zone in AA2219 aluminium alloy10.1016/j.msea.2006.12.124 ↗
3. Characterisation and understanding of the corrosion behaviour of the nugget in a 2050 aluminium alloy Friction Stir Welding joint10.1016/j.corsci.2013.04.001 ↗
4. Temperature evolution, microstructure and mechanical properties of friction stir welded thick 2219-O aluminum alloy joints10.1016/j.matdes.2008.09.021 ↗
5. Characterisation of microstructure, mechanical properties and corrosion behaviour of an AA2219 friction stir weldment10.1016/j.jallcom.2009.11.198 ↗
6. Friction stir welding of aluminium alloys10.1179/174328009X411136 ↗
7. Cold-rolled Mg-14 mass% Li-1 mass% Al alloy and its friction stir welding10.2320/matertrans.47.1077 ↗
8. The optimum combination of tool rotation rate and traveling speed for obtaining the preferable corrosion behavior and mechanical properties of friction stir welded AA5052 aluminum alloy10.1016/j.matdes.2013.03.027 ↗
9. A study on corrosion behavior of friction stir welded and tungsten inert gas welded AA2014 aluminium alloy10.1016/j.corsci.2018.01.012 ↗
10. Microstructural and mechanical properties of friction stir welded Cu–30Zn brass alloy at various feed speeds: Influence of stir bands10.1016/j.matdes.2011.01.015 ↗
11. Establishing a correlation between interfacial microstructures and corrosion initiation sites in Al/Cu joints by SEM–EDS and AFM–SKPFM10.1016/j.corsci.2013.10.039 ↗
12. Hatch · 1984
13. Craig · 1994
14. Relationship between microstructure, microhardness and corrosion sensitivity of an AA 2024-T3 friction stir welded joint10.1016/j.corsci.2011.05.049 ↗
15. Microstructure and corrosion characterization of the interfacial region in dissimilar friction stir welded AA5083 to AA702310.1016/j.corsci.2016.02.027 ↗
16. Microstructures and electrochemical behaviors of the friction stir welding dissimilar weld10.1016/S1001-0742(11)61072-3 ↗
17. Pitting and stress corrosion cracking resistance of friction stir welded AA 508310.1002/1521-4176(200111)52:11<853::AID-MACO853>3.0.CO;2-1 ↗
18. Stress corrosion cracking in Al-Zn-Mg-Cu aluminum alloys in saline environments10.1007/s11661-012-1528-3 ↗
19. The role of magnesium segregation in the intergranular stress corrosion cracking of aluminium alloys10.1016/0010-938X(87)90076-X ↗
20. Effect of pitting corrosion on very high cycle fatigue behavior10.1016/S1359-6462(03)00365-8 ↗
21. Friction stir processing of aluminium alloy AA7075: microstructure, surface chemistry and corrosion resistance10.1016/j.corsci.2016.02.006 ↗
22. Microstructural evolution and corrosion behaviour of friction stir-processed QE22 magnesium alloy10.1515/corrrev-2020-0083 ↗
23. Slow-strain-rate stress corrosion testing of welded joints of Al-Mg alloys
24. Localized corrosion and stress corrosion cracking resistance of friction stir welded aluminum alloy 545410.5006/1.3283974 ↗
25. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
26. Achievement of high-strength 2219 aluminum alloy joint in a broad process window by ultrasonic enhanced friction stir welding10.1016/j.msea.2020.140587 ↗
27. Corrosion mechanism of Al, Al–Zn and Al–Zn–Sn alloys in 3 wt% NaCl solution10.1016/j.corsci.2014.07.018 ↗
28. A comparison of the corrosion behavior of nanocrystalline and conventional Al 5083 samples10.5006/1.3278260 ↗
29. Kelly · 2002
30. Mitigation of intergranular stress corrosion cracking in Al–Mg by electrochemical potential control10.1007/s11837-017-2362-2 ↗
31. Corrosion behaviour of Ti–6Al–7Nb and Ti–6Al–4V ELI alloys in the simulated body fluid solution by electrochemical impedance spectroscopy10.1016/j.electacta.2006.06.018 ↗
32. Constant-phase-element behavior caused by resistivity distributions in films: I. Theory10.1149/1.3499564 ↗
33. Passivation behavior and surface chemistry of 2507 super duplex stainless steel in artificial seawater: influence of dissolved oxygen and pH10.1016/j.corsci.2019.02.002 ↗
34. Impedance spectroscopy as quality control and corrosion test for anodized Al alloys10.5006/1.3583832 ↗
35. Corrosion behavior of a dynamically deformed Al–Mg alloy10.1016/j.electacta.2020.136695 ↗
36. Electrochemical characteristics of intermetallic phases in aluminum alloys: an experimental survey and discussion10.1149/1.1869984 ↗
37. Deformation rate and sensitization effects on environmentally assisted cracking of Al-Mg naval alloys10.5006/1949 ↗
38. Microstructure-strength relationship in friction-stir welded 6061-T6 aluminum alloy10.1016/j.msea.2020.139858 ↗
39. Structure and mechanical properties of nanostructured Al–Mg alloys processed by severe plastic deformation10.1007/s10853-012-7133-4 ↗
40. Microstructure and strength of severely deformed fcc metals10.1016/j.msea.2006.02.455 ↗
41. CDRX modelling in friction stir welding of aluminium alloys10.1016/j.ijmachtools.2004.12.001 ↗
42. Exfoliation corrosion of friction stir welded dissimilar 2024-to-7075 aluminum alloys10.1016/j.matchar.2018.11.002 ↗
43. Wit, Corrosion of aluminium in acidic and neutral solutions10.1016/0013-4686(93)80329-X ↗
44. Impedance studies of the passive film on aluminium10.1016/j.corsci.2005.05.058 ↗
45. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
46. Electrochemical analysis of AA6082 aluminium alloy in chloride media10.20964/2017.07.71 ↗
47. Exploring the effects of intermetallic particle size and spacing on the corrosion of Mg-Al alloys using model electrodes10.1149/2.1151614jes ↗
48. Mechanical properties of 5083 aluminium welds after manual and automatic pulsed gas metal arc welding using E5356 filler10.4028/www.scientific.net/MSF.654-656.2560 ↗
49. Corrosion resistance in FSW and in MIG welding techniques of AA6XXX10.1016/j.jmatprotec.2007.06.034 ↗
50. Mechanical and corrosion behaviour of aluminum alloy 5083 and its weldment for marine applications
51. Effect of preaging temperature on microstructure evolution, mechanical and corrosion behavior of RRA‐treated high‐zinc 7068 alloy10.1002/maco.202213196 ↗
52. Multiscale investigation of corrosion damage initiation and propagation in AA7075-T651 alloy using correlative microscopy10.1016/j.corsci.2021.109429 ↗
53. Analysis of pits induced stresses due to metal corrosion10.1016/j.corsci.2008.05.003 ↗
54. Correlations between intergranular stress corrosion cracking, grain-boundary microchemistry, and grain-boundary electrochemistry for Al–Zn–Mg–Cu alloys10.1016/j.corsci.2010.08.024 ↗
55. The influence of hydrogen on the stress-corrosion cracking of low-strength Al-Mg alloys10.1007/s11837-003-0225-5 ↗
56. The contribution of hydrogen evolution processes during corrosion of aluminium and aluminium alloys investigated by potentiodynamic polarisation coupled with real-time hydrogen measurement10.1038/s41529-017-0011-4 ↗