Effects of 100 ppb dissolved oxygen on low-cycle fatigue behaviors of 316LN austenitic stainless steel in borated and lithiated high temperature water and mechanism behind these effects
Source abstract
Abstract
Abstract In this work, beneficial effects of dissolved oxygen (DO) on the crack initiation and propagation in borated and lithiated high temperature water were observed, which finally increased the low-cycle fatigue (LCF) life of the 316LN in the water. The 100 ppb DO added in the water also reduced the total amount of absorbed hydrogen. Meanwhile, the oxide film formed was more protective compared with the oxide films formed in oxygen free water. Based on the metallurgical and electrochemical characterizations conducted in the present study, a scheme of the mechanism of the LCF life increase is proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Thermal fatigue in french RHR system
2. On the mechanism of environmental cracking introduced by cyclic thermal loading, in: IAEA specialists’ meeting, corrosion and stress corrosion of steel pressure boundary components and steam turbines
3. “Strain induced corrosion cracking of Low-alloy reactor pressure vessel steels under BWR conditions,” proc
4. US NRC · 2007
5. Chopra · 2014
6. Role of inclusions and carbide bands in corrosion fatigue of pressure vessel steel in high-temperature water10.5006/1.3299218 ↗
7. Modelling of crack chemistry in sensitized stainless steel in boiling water reactor environments10.1016/S0010-938X(97)89342-0 ↗
8. Modeling of the chemistry and electrochemistry in cracks—a review10.5006/1.3290342 ↗
9. Inclusion-involved fatigue cracking in high temperature water10.1002/maco.200403845 ↗
10. The crack tip solution chemistry in sensitized stainless steel in simulated boiling water reactor water studied using a microsampling technique10.1080/18811248.2003.9715371 ↗
11. The role of hydrogen and other interstitials in the mechanical behavior of metals10.1007/s13632-016-0319-4 ↗
12. A mechanistic theory of hydrogen embrittlement of steels, Berichte Der Bunsengesellschaft Für Phys
13. Whitney Award Lecture – 1987: hydrogen – the versatile ebrittler10.5006/1.3583875 ↗
14. The necessity of both plasticity and brittleness in the fracture thresholds of iron10.1080/01418619108204854 ↗
15. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
16. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
17. Hydrogen related failure of steels – a new aspect10.1179/026708304225019687 ↗
18. Function of hydrogen in embrittlement of high-strength steels10.2355/isijinternational.41.590 ↗
19. Low cycle fatigue behaviors of type 316LN austenitic stainless steel in 310 ℃ deaerated water-fatigue life and dislocation structure development10.1016/j.msea.2007.07.023 ↗
20. Effects of dissolved hydrogen on low-cycle fatigue behaviors and hydrogen uptake of 316LN austenitic stainless steel in simulated pressurized water reactor primary water10.1016/j.ijfatigue.2019.105457 ↗
21. Hydrogen uptake in austenitic stainless steels by exposure to gaseous hydrogen and its effect on tensile deformation10.1016/j.corsci.2011.04.022 ↗
22. Thermal desorption study of selected austenitic stainless steels10.1116/1.1527953 ↗
23. Raman Spectroscopy for the discrimination of tephras from the Hekla eruptions of 1510 and 194710.1177/0959683615609744 ↗
24. Laser Raman Spectroscopic Study on Magnetite Formation in Magnetotactic Bacteria10.2320/jinstmet.73.334 ↗
25. Growth behavior of surface oxide layer on SUS316L stainless steel at the early stage of exposure to 288 ℃ water10.2320/matertrans.M2011200 ↗
26. Effect of dissolved hydrogen on corrosion of 316NG stainless steel in high temperature water10.1016/j.nucengdes.2015.08.030 ↗
27. Morphology-controlled synthesis and enhanced energy product (BH)mas of CoFe2O4 nanoparticles10.1039/C8NJ02177E ↗
28. Electrochemical behavior of copper-nickel alloys as immobilization matrices for the storage of fission products in CO2-enriched synthetic groundwater10.1016/j.electacta.2013.03.034 ↗
29. Electrochemical properties and growth mechanism of passive films on alloy 690 in high-temperature alkaline environments10.1016/j.corsci.2010.06.016 ↗
30. A study on the localized corrosion and repassivation kinetics of Fe-20Cr-xNi (x=0-20wt%) stainless steels via electro-chemical analysis10.1016/j.corsci.2015.07.022 ↗
31. Study on the passive film of type 316 stainless steel10.1016/S1452-3981(23)13227-5 ↗
32. Effect of zinc on the environmentally-assisted fatigue behavior of 316 stainless steels in simulated PWR primary environment10.1016/j.corsci.2019.02.012 ↗
33. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
34. Surface oxide layers on 316L stainless steel formed in 561 K pure water at different potentials10.1149/2.030208jes ↗
35. Thermal analysis of trapped hydrogen in pure Iron10.1007/BF02642424 ↗
36. Effect of hydrogen on plastic strain localization in single crystals of austenitic stainless steel10.1016/j.scriptamat.2009.10.005 ↗
37. Mechanism of hydrogen absorption during the exposure of alloy 600-like single-crystals to PWR primary simulated media
38. Hydrogen absorption associated with the corrosion mechanism of 316L stainless steels in primary medium of Pressurized Water Reactor (PWR)10.1016/j.corsci.2014.04.025 ↗
39. Jones · 1996
40. Fatigue crack growth behavior in austenitic stainless steels subjected to superficial and entire hydrogenation10.1016/j.msea.2012.03.101 ↗
41. Environmentally assisted cracking of forged 316LN stainless steel and its weld in high temperature water10.1016/j.corsci.2018.10.032 ↗
42. The effect of dissolved oxygen on fatigue behavior of Alloy 690 steam generator tubes in borated and lithiated high temperature water10.1016/j.corsci.2015.10.032 ↗
43. Emerging issues and fundamental processes in environmental cracking in hot water10.5006/1.3278483 ↗
44. Fatigue crack propagation
45. Modelling of short crack propagation–transition from stage I to stage II10.1016/j.engfracmech.2007.02.018 ↗
46. Corrosion fatigue
47. Corrosion fatigue and microstructural characterisation of Type 316 austenitic stainless steels tested in PWR primary water10.1016/j.corsci.2017.10.022 ↗
48. Corrosion deformation interaction during stress corrosion cracking of alloy 600 in primary water
49. Jackson · 1991
50. Investigation of the local austenite stability related to hydrogen environment embrittlement of austenite stainless steels10.4028/www.scientific.net/MSF.941.263 ↗
51. A new mechanism in hydrogen-enhanced fatigue crack growth behavior of a 1900-MPa-class high-strength steel10.1007/s10704-012-9760-9 ↗