Microstructure and oxidation mechanism of multiphase Mo–Ti–Si–B alloys at 800 °C
Source abstract
Abstract
Abstract Three Mo–Ti–Si–B alloys with compositions of 50Mo–20Ti–20Si–10B, 40Mo–30Ti–20Si–10B and 30Mo–40Ti–20Si–10B (at.%) were designed and prepared by arc-melting. Microstructure evolution at 1600 °C and oxidation mechanism at 800 °C of these alloys were analyzed. 50Mo–20Ti–20Si–10B suffered from pesting because of a large volume fraction of Mo3Si, which produced porous products with severe volume expansion. Both 40Mo–30Ti–20Si–10B and 30Mo–40Ti–20Si–10B have better oxidation resistance. It can be inferred that during long-term oxidation, interactions between constituent phases contributed to the overall oxidation resistance of the alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced materials and composites · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Ultrahigh-temperature materials for jet engines10.1557/mrs2003.189 ↗
2. The balance of mechanical and environmental properties of a multielement niobium-niobium silicide-based in situ composite10.1007/BF02595629 ↗
3. A review of very-high-temperature Nb-silicide-based composites10.1007/s11661-003-0269-8 ↗
4. The hotter the engine, the better10.1126/science.1179327 ↗
5. Mo–Si–B alloys for ultrahigh-temperature structural applications10.1002/adma.201200764 ↗
6. Study of solidification pathway of a MoSiBTiC alloy by optical thermal analysis and in-situ observation with electromagnetic levitation10.1038/s41598-019-50945-z ↗
7. Phase stability and structural defects in high-temperature Mo–Si–B alloys10.1016/j.actamat.2008.07.015 ↗
8. High temperature strength of Mo–Mo3Si–Mo5SiB2 molybdenum silicides10.1016/S0966-9795(03)00044-X ↗
9. Tensile creep of Mo–Si–B alloys10.1016/j.actamat.2009.11.054 ↗
10. Optimization of Mo–Si–B intermetallic alloys10.1007/s11661-005-0166-4 ↗
11. Oxidation behavior of Mo–Si–B alloys at medium-to-high temperatures10.1016/j.jmst.2020.06.004 ↗
12. A Mo–Si–B intermetallic alloy with a continuous α-Mo matrix10.1016/S1359-6462(01)01227-1 ↗
13. Room-temperature fracture toughness of MoSiBTiC alloys10.1016/j.intermet.2017.01.004 ↗
14. Oxidation mechanisms in Mo-reinforced Mo5SiB2(T2)–Mo3Si alloys10.1016/S1359-6454(02)00039-3 ↗
15. Effect of Ti (Macro-) alloying on the high-temperature oxidation behavior of ternary Mo–Si–B alloys at 820-1300 °C10.1007/s11085-013-9375-1 ↗
16. High-temperature creep and oxidation behavior of Mo–Si–B alloys with high Ti contents10.1007/s11661-013-1944-z ↗
17. High-temperature oxidation behavior of Mo–Si–B-based and Co–Re–Cr-based alloys10.1016/j.intermet.2013.10.008 ↗
18. Creep resistance and oxidation behavior of novel Mo–Si–B–Ti alloys10.1007/s11837-015-1560-z ↗
19. Microstructure, high-temperature deformability and oxidation resistance of a Ti5Si3-containing multiphase MoSiBTiC alloy10.1016/j.intermet.2017.07.018 ↗
20. High-temperature oxidation behavior of a Ti5Si3-incorporated MoSiBTiC alloy10.1016/j.intermet.2020.106895 ↗
21. Oxidation behavior of Moss–Ti5Si3–T2 composites at intermediate and high temperatures10.1016/j.intermet.2020.106702 ↗
22. Effect of Cr on microstructure and oxidation resistance of a Ti5Si3-containing MoSiBTiC alloy10.1016/j.corsci.2019.108418 ↗
23. Orientation relationship between bcc precipitates and Ti5Si3 matrix in Mo–Si–B–Ti–C quinary alloys10.1016/j.intermet.2020.106863 ↗
24. Experimental investigation and thermodynamic descriptions of the Mo–Si–Ti system10.1016/S0921-5093(03)00560-4 ↗
25. Multiphase equilibria in the metal-rich region of the Mo–Ti–Si–B system: thermodynamic prediction and experimental validation10.1016/j.actamat.2004.12.020 ↗
26. Effect of Ti, Zr and Hf on the phase stability of Mo_ss+Mo3Si+Mo5SiB2 alloys at 1600 °C10.1016/j.actamat.2009.09.032 ↗
27. Constitution, oxidation and creep of eutectic and eutectoid Mo–Si–Ti alloys10.1016/j.intermet.2018.10.028 ↗
28. Characterisation of the oxidation and creep behaviour of novel Mo–Si–Ti alloys10.1016/j.actamat.2019.11.045 ↗
29. On the chemical and microstructural requirements for the pesting-resistance of Mo–Si–Ti alloys10.1016/j.jmrt.2020.06.002 ↗
30. Microstructural and chemical constitution of the oxide scale formed on a pesting-resistant Mo–Si–Ti alloy10.1016/j.corsci.2020.109081 ↗
31. Phase stability and structural defects in high-temperature Mo–Si–B alloys10.1016/j.actamat.2008.07.015 ↗
32. Improvement of the oxidation-proof property and the scale structure of Mo3Si intermetallic alloy through the addition of chromium and aluminum elements10.1016/j.intermet.2006.01.059 ↗
33. Oxidation behavior of Mo5SiB2-based alloy at elevated temperatures10.1016/S0966-9795(02)00013-4 ↗
34. Transient oxidation of Mo–Si–B alloys: effect of the microstructure size scale10.1016/j.actamat.2009.06.036 ↗
35. High-temperature oxidation behavior of a single-phase (Mo,Ti)5Si3 (Mo–Si–Ti) alloy10.1016/j.scriptamat.2011.10.042 ↗
36. Effect of Ti content and nitrogen on the high-temperature oxidation behavior of (Mo,Ti)5Si310.1016/j.intermet.2017.05.023 ↗
37. Oxidation behavior of Ti5Si3 at temperatures between 1400 and 1700 K10.4028/www.scientific.net/MSF.251-254.227 ↗
38. Elevated-temperature oxidation of titanium silicide and titanium silicide-based alloy and composite10.1007/s11661-998-0089-y ↗
39. Oxidation resistance of Ti5Si3 and Ti5Si3Zx at 1000 °C (Z= C, N, or O)10.1023/A:1016012507682 ↗
40. Role of nitrogen on the oxidative stability of Ti5Si3 based alloys at elevated temperature10.1016/j.intermet.2005.09.006 ↗
41. High temperature oxidation behavior of Ti5Si3-based intermetallics10.1016/j.intermet.2008.06.013 ↗
42. Data on the early oxidation of SiO2-coated pure Ti and bulk Ti5Si3 at 800 °C10.1016/j.dib.2018.08.173 ↗
43. Oxidation behaviour of Mo–Si–B–(Al,Ce) ultrafine-eutectic dendrite composites in the temperature range of 500-700 °C10.1016/j.intermet.2010.08.043 ↗
44. Mechanical behavior and oxidation resistance of structural silicides10.1179/174328006X79454 ↗
45. Effect of third elements on the pesting suppression of Mo–Si–X intermetallics (X=Al, Ta, Ti, Zr and Y)10.1016/0966-9795(96)00019-2 ↗
46. Structural and morphological studies of the growth of MoO3 scales during high-temperature oxidation of Molybdenum10.1007/BF00665191 ↗