journal article·2021-02Open access

The effect of composition and thickness on the mechanism and kinetics of filiform corrosion occurring on zinc-aluminium-magnesium coated steel

N. Wint, D. Eaves, G. Williams, H.N. McMurray

Corrosion Science· Volume 179

Abstract

Abstract The effect of coating thickness and composition on the kinetics of acetic acid-induced filiform corrosion (FFC) on Zinc-Aluminium-Magnesium (ZAM) coated steel is investigated. Scribe defects are created in organic coatings applied to ∼10 μm coatings of varying composition (1−6 wt.%. Al, 1−3 wt. % Mg), and fixed composition (Zn-1.5 wt. % Al- 1.5 wt.% Mg) but varying thickness (5−27 μm). FCC decreases with increasing Al (at fixed wt. % Mg) and thickness. A linear trend exists between thickness and iron exposure time. Findings are consistent with FFC advancing via a penetrative coating mechanism whereby exposed iron couples to the coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Atmospheric corrosion of ZnAlMg coated steel during long term atmospheric weathering at different worldwide exposure sites10.1016/j.corsci.2018.12.033 ↗
2. Underfilm/coating corrosion
3. The delamination of polymeric coatings from steel. Part 1: calibration of the Kelvinprobe and basic delamination mechanism10.1016/S0010-938X(98)00166-8 ↗
4. The delamination of polymeric coatings from steel. Part 2: first stage of delamination, effect of type and concentration of cations on delamination, chemical analysis of the interface10.1016/S0010-938X(98)00167-X ↗
5. Chromate inhibition of corrosion-driven organic coating delamination studied using a scanning kelvin probe technique10.1149/1.1396336 ↗
6. Investigation of the delamination of polymer films from galvanized steel with the Scanning Kelvinprobe
7. The delamination of polymeric coatings from electrogalvanised steel – a mechanistic approach.: part 1: delamination from a defect with intact zinc layer10.1016/S0010-938X(00)00047-0 ↗
8. The delamination of polymeric coatings from electrogalvanized steel – a mechanistic approach.: part 2: delamination from a defect down to steel10.1016/S0010-938X(00)00048-2 ↗
9. The delamination of polymeric coatings from electrogalvanized steel – a mechanistic approach.: part 3: delamination kinetics and influence of CO210.1016/S0010-938X(00)00049-4 ↗
10. In situ monitoring of corrosion mechanisms and phosphate inhibitor surface deposition during corrosion of zinc–magnesium–aluminium (ZMA) alloys using novel time-lapse microscopy10.1039/C4FD00251B ↗
11. In situ monitoring of the microstructural corrosion mechanisms of zinc–magnesium–aluminium alloys using time lapse microscopy10.1016/j.corsci.2011.02.043 ↗
12. Nanoscale analysis of surface oxides on ZnMgAl hot-dip-coated steel sheets10.1007/s00216-011-5507-0 ↗
13. Microstructural characterization and quantification of Zn–Al–Mg surface coatings10.1016/j.matchar.2010.06.008 ↗
14. Corrosion of zinc–magnesium coatings: mechanism of paint delamination10.1016/j.corsci.2009.05.042 ↗
15. The physical meaning of electrode potentials at metal surfaces and Polymer/Metal interfaces: consequences for delamination corrosion, passivation, and anodic films10.1149/1.2926589 ↗
16. Zn-Mg and Zn-Mg-Al alloys for improved corrosion protection of steel: some new aspects10.1002/maco.201307586 ↗
17. Delamination resistant zinc alloys: simple concept and results on the system zinc‐magnesium10.1002/srin.200300212 ↗
18. The kinetics and mechanism of filiform corrosion occurring on zinc-aluminium-magnesium coated steel10.1016/j.corsci.2019.06.028 ↗
19. Filiform corrosion in polymer-coated metals10.1016/0300-9440(95)00555-2 ↗
20. An analysis of mass transfer in filiform corrosion10.5006/1.3581907 ↗
21. Corrosion protection by organic coatings: electrochemical mechanism and novel methods of investigation10.1016/S0013-4686(00)00348-0 ↗
22. The mechanism of group (I) chloride initiated filiform corrosion on iron10.1016/j.elecom.2003.08.008 ↗
23. The effect of oxygen partial pressure on the filiform corrosion of organic coated iron10.1016/j.corsci.2014.08.004 ↗
24. Mechanism of filiform corrosion10.1021/ie50533a053 ↗
25. Scanning kelvinprobe investigations of filiform corrosion on aluminum alloy 2024-t310.1016/S0010-938X(98)00044-4 ↗
26. New knowledge on localized corrosion obtained from local measuring techniques10.1016/S0013-4686(01)00642-9 ↗
27. Effect of climatic parameters on filiform corrosion of coated aluminum alloys10.5006/1.3287763 ↗
28. The kinetics of chloride-induced filiform corrosion on aluminum alloy AA2024-T310.1149/1.1589020 ↗
29. Chromate inhibition of filiform corrosion on organic coated AA2024-T3 studied using the scanning kelvin probe10.1149/1.1757460 ↗
30. The kinetics and mechanisms of filiform corrosion on aluminium alloy AA611110.1016/j.electacta.2010.04.035 ↗
31. The role of chromate in filiform corrosion inhibition10.1016/S0013-4686(03)00256-1 ↗
32. The role of chromate in filiform corrosion inhibition10.1016/S0013-4686(02)00829-0 ↗
33. Chloride-induced filiform corrosion of organic-coated magnesium10.1016/j.electacta.2010.09.005 ↗
34. Award lecture: molecular in situ studies of atmospheric corrosion10.5006/1.3278420 ↗
35. Atmospheric corrosion of zinc by organic constituents: I. The role of the Zinc/Water and Water/Air interfaces studied by infrared Reflection/Absorption spectroscopy and vibrational sum frequency spectroscopy10.1149/1.2164788 ↗
36. Atmospheric corrosion of zinc by organic constituents: II. Reaction routes for zinc-acetate formation10.1149/1.2360740 ↗
37. GILDES model simulations of the atmospheric corrosion of zinc induced by low concentrations of carboxylic acids10.1149/2.072203jes ↗
38. Initial atmospheric corrosion of zinc induced by carboxylic acids: a quantitative in situ study10.1149/1.3240878 ↗
39. Molecular structural information of the atmospheric corrosion of zinc studied by vibrational spectroscopy techniques: I. Experimental approach10.1149/1.3479207 ↗
40. Molecular Structural Information of the Atmospheric Corrosion of Zinc Studied by Vibrational Spectroscopy Techniques: II. Two and Three-Dimensional Growth of Reaction Products Induced by Formic and Acetic Acid10.1149/1.3479255 ↗
41. Metal carboxylate formation during indoor atmospheric corrosion of Cu, Zn, and Ni10.1149/1.2048598 ↗
42. Characterisation of corrosivity in indoor atmospheres with different metals and evaluation techniques10.1179/bcj.1998.33.1.59 ↗
43. Chapter F.6 - carboxylic acids and their derivatives
44. Solubilities of magnesium, calcium, barium, cobalt, nickel, copper, and zinc acetates in water from T= (278.15 to 348.15) K10.1006/jcht.1999.0548 ↗
45. Layered zinc hydroxide monolayers by hydrolysis of organozincs10.1039/C7SC04256F ↗
46. The effect of magnesium additions on the microstructure and cut edge corrosion resistance of zinc aluminium alloy galvanised steel10.1016/j.corsci.2008.02.005 ↗
47. Corrosion of zinc and Zn-Mg alloys with varying microstructures and magnesium contents10.1149/2.103403jes ↗
48. Microstructural changes in zinc aluminium alloy galvanising as a function of processing parameters and their influence on corrosion10.1016/j.corsci.2004.11.011 ↗
49. Effect of the microstructure of Zn-Al and Zn-Al-Mg model alloys on corrosion stability10.1016/j.corsci.2016.04.022 ↗
50. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn–Al–Mg coatings on steel10.1016/j.corsci.2011.03.016 ↗
51. The initial release of zinc and aluminium from non-treated Galvalume and the formation of corrosion products in chloride containing media10.1016/j.apsusc.2011.12.112 ↗
52. Nanoscopic view on the initial stages of corrosion of hot dip galvanized Zn–Mg–Al coatings10.1016/j.corsci.2014.02.027 ↗
53. The effect of pH on the selective dissolution of Zn and Al from Zn–Al coatings on steel10.1016/j.corsci.2012.09.042 ↗
54. Corrosion mechanisms of Zn(Mg,Al) coated steel: 2. The effect of Mg and Al alloying on the formation and properties of corrosion products in different electrolytes10.1016/j.corsci.2014.07.042 ↗
55. Composition of corrosion products formed on Zn–Mg, Zn–Al and Zn–Al–Mg coatings in model atmospheric conditions10.1016/j.corsci.2014.05.016 ↗
56. The effect of an artificially synthesized simonkolleite layer on the corrosion of electrogalvanized steel10.1016/j.corsci.2012.10.024 ↗
57. Aqueous corrosion of Mg-Al binary alloys: roles of Al and Mg10.5006/i0010-9312-68-6-557 ↗
58. Zr-based conversion layer on Zn-Al-Mg alloy coated steel sheets: insights into the formation mechanism10.1016/j.electacta.2014.05.163 ↗
59. Innovative steel strip coatings by means of PVD in a continuous pilot line: process technology and coating development10.1016/S0257-8972(02)00660-6 ↗
60. The effect of Mg concentration on the resistance of PVD Zn-Mg coatings to corrosion driven organic coating delamination10.1016/j.corsci.2015.08.036 ↗
61. XPS investigation on the surface chemistry of corrosion products on ZnMgAl-coated steel10.1007/s00216-013-7099-3 ↗
62. Corrosion behaviour of Zn–Al–Mg coated steel sheet in sodium chloride-containing environment10.1016/j.corsci.2009.06.019 ↗
63. Corrosion performance of Zn–Al–Mg coatings in open and confined zones in conditions simulating automotive applications10.1002/maco.200905425 ↗
64. Activation and inhibition of Zn–Al and Zn–Al–Mg coatings on steel by nitrate in phosphoric acid solution10.1016/j.corsci.2012.03.028 ↗
65. Corrosion mechanism of model zinc–magnesium alloys in atmospheric conditions10.1016/j.corsci.2008.06.008 ↗
66. Chemistry of corrosion products of Zn and MgZn pure phases under atmospheric conditions10.1016/j.corsci.2012.08.014 ↗
67. Investigation of the corrosion behaviors of continuously hot-dip galvanizing Zn-Mg coating10.1016/j.surfcoat.2012.03.079 ↗
68. Understanding corrosion via corrosion product characterization: I. Case study of the role of Mg alloying in Zn-Mg coating on steel10.1016/j.corsci.2009.03.005 ↗
69. Corrosion resistance of zinc-magnesium coated steel10.1016/j.corsci.2007.03.032 ↗
70. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn–Al–Mg coatings on steel10.1016/j.corsci.2009.03.005 ↗
71. Corrosion performance of Zn–Mg–Al coated steel in accelerated corrosion tests used in the automotive industry and field exposures10.1002/maco.201206959 ↗
72. Zn-Al-Mg coatings: thermodynamic analysis and microstructure related properties10.4028/www.scientific.net/MSF.539-543.1276 ↗
73. Hot dip ZnAlMg coatings: microstructure and forming properties
74. Baes · 1976
75. Atmospheric corrosion of Galfan coatings on steel in chloride-rich environments10.1016/j.corsci.2013.03.025 ↗
76. Cathodic self-healing at cut-edges: the effect of Zn2+ and Mg2+ ions10.1016/j.corsci.2012.08.008 ↗