journal article·2024-03

Effect of in-situ pre-soaking in seawater on the erosion-corrosion properties and micro-mechanism of nickel aluminium bronze alloy

Wanyu Wang, Wenjing Zhang, Guojie Huang, Xujun Mi, Lei Huang

Corrosion Science· Volume 228
Publisher page

Abstract

The effects of pre-soaking in seawater on the corrosion behaviour of the nickel aluminium bronze alloy were examined using electrochemical and erosion-corrosion tests. The surface passive film of the alloy pre-soaked for 30 d consisted of an outer loose CuO film, a middle dense Cu 2O film, and a denser inner Cu 2O film contained Al 2O 3 . The corrosion properties of the sample pre-soaked for 30 d were significantly improved, with ∼71% reduction in corrosion rate at 3 m/s compared with the unsoaked sample. Strong bonding between the substrate and passive films formed during pre-soaking effectively inhibited the entry of ions from seawater.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgy and Material Science · Corrosion Behavior and Inhibition · Bauxite Residue and Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Improvement of surface resistance to cavitation corrosion of nickel aluminium bronze by electro pulsing-assisted ultrasonic surface rolling process10.1016/j.surfcoat.2019.03.045 ↗
2. Microstructure design to improve the corrosion and cavitation corrosion resistance of a nickel-aluminium bronze10.1016/j.corsci.2018.04.043 ↗
3. The corrosion of nickel-aluminium bronze in seawater10.1016/j.corsci.2005.05.053 ↗
4. Mechanical properties at high temperatures and microstructures of a nickel aluminium bronze alloy10.4028/www.scientific.net/AMR.683.82 ↗
5. The influence of nickel-aluminium bronze microstructure and crevice solution on the initiation of crevice corrosion10.1016/j.electacta.2007.10.047 ↗
6. Effects of microstructure on the stress corrosion cracking behaviour of nickel-aluminium bronze alloy in 3.5% NaCl solution10.1016/j.msea.2018.07.066 ↗
7. Enhancing mechanical properties and corrosion resistance of nickel-aluminium bronze via hot rolling process10.1016/j.jmst.2020.05.024 ↗
8. Studies of the nobility of phases using scanning Kelvin probe microscopy and its relationship to corrosion behaviour of Ni-Al bronze in chloride media10.1016/j.corsci.2014.11.039 ↗
9. Effect of heat treatment on micro-structure evolution and erosion-corrosion behaviour of a nickel-aluminium bronze alloy in chloride solution10.1016/j.corsci.2015.05.037 ↗
10. Flow influenced electrochemical corrosion of nickel aluminium bronze–Part I. Cathodic polarization10.1007/s10800-004-1758-1 ↗
11. The role of nickel in mechanical performance and corrosion behaviour of nickel-aluminium bronze in 3.5wt% NaCl solution10.1016/j.corsci.2018.05.012 ↗
12. Corrosion product film formed on the 90/10 copper-nickel tube in natural seawater: composition/structure and formation mechanism10.1016/j.corsci.2014.11.028 ↗
13. Effects of nickel-aluminium bronze pre-oxidized films on the cathodic kinetics of oxygen reduction10.1080/00032719.2019.1700515 ↗
14. Evolution of the corrosion product film on nickel-aluminium bronze and its corrosion behaviour in 3.5 wt% NaCl solution10.3390/ma12020209 ↗
15. The corrosion of nickel-aluminium bronzes in seawater-I. Protective layer formation and the passivation mechanism10.1016/0010-938X(93)90017-B ↗
16. Evolution of the corrosion product film and its effect on the erosion-corrosion behaviour of two commercial 90Cu-10Ni tubes in seawater10.1007/s40195-018-0745-1 ↗
17. ASTM G1-90 · 2003
18. ISO 8407. Corrosion of metals and alloys-Removal of corrosion products from corrosion test specimens. (2015).
19. JB/T 7901-1999. Metals materials-Uniform corrosion-Methods of laboratory immersion testing.
20. Tailoring microstructure of a nickel aluminium bronze by hot extrusion and its impact on mechanical and corrosion behaviour10.1016/j.corsci.2023.111049 ↗
21. Factors affecting the adhesion of TiN coating by scratch test
22. Reasonable use of scratch method and microscopic method to determine the adhesion of TiN film to substrate, Phys. Test
23. The morphology, crystallography, and chemistry of phases in as-cast nickel-aluminium bronze, Metall
24. Improving corrosion resistance of nickel-aluminium bronzes by surface modification with chromium ion implantation10.1016/j.surfcoat.2017.11.066 ↗
25. Investigation of microstructure and mechanical properties of hot worked NiAl bronze alloy with different deformation degree10.1016/j.msea.2015.06.078 ↗
26. Effect of nickel content on the electrochemical behaviour of Cu–Al–Ni alloys in chloride free neutral solutions10.1016/j.electacta.2010.09.080 ↗
27. Surface characterization and corrosion behaviour of a novel gold-imitation copper alloy with high tarnish resistance in salt spray environment10.1016/j.corsci.2013.05.026 ↗
28. Electrochemical behaviour of copper in neutral aerated chloride solution. II. Impedance investigation10.1007/BF01093752 ↗
29. Introduction to Electrochemical Impedance Spectroscopy
30. Intergranular erosion corrosion of pure copper tube in flowing NaCl solution10.1016/j.corsci.2022.110304 ↗
31. Enhancing the erosion-corrosion resistance of cupronickel alloy through grain boundary engineering10.1016/j.corsci.2023.111228 ↗
32. Antibacterial property, corrosion and discoloration resistance of pure copper containing Zn or Ni10.1007/s12598-022-02098-8 ↗
33. Anomalous chemical shifts of Cu 2p and Cu LMM Auger spectra of silicate glasses10.1016/S0368-2048(03)00126-9 ↗
34. Surface characterization and corrosion behaviour of 70/30 Cu–Ni alloy in pristine and sulfide-containing simulated seawater10.1016/j.corsci.2006.07.003 ↗
35. The synergistic effect of Ns and Fe on the sea water corrosion of copper alloys10.5006/0010-9312-33.10.347 ↗
36. Corrosion and Galvanic Compatibility Studies of a High-Strength Copper-Nickel Alloy10.5006/1.3277305 ↗
37. Flow influenced electrochemical corrosion of nickel aluminium bronze-Part II. Anodic polarisation and derivation of the mixed potential10.1007/s10800-004-1759-0 ↗
38. Impedance and photoelectrochemical study of surface layers on Cu and Cu–10Ni in acetate solution containing benzotriazole10.1016/S0013-4686(98)00367-3 ↗
39. The influence of corrosion product structure on the corrosion rate of Cu-Ni alloys10.1016/S0010-938X(70)80022-1 ↗
40. The behaviour of Cu-xNi (x = 10 to 40 wt%) alloys in alkaline solutions containing chloride ions10.1016/S0013-4686(96)00315-5 ↗
41. Potential-pH diagrams for 90-10 and 70-30 Cu-Ni in sea water10.5006/0010-9312-31.3.77 ↗
42. Characterization of the corrosion product films formed on the As-cast and friction-stir processed Ni-Al Bronze in a 3.5 wt% NaCl solution10.5006/1391 ↗
43. On the microstructure and erosion corrosion behaviour of laser processed Nickel Aluminium Bronze10.4028/www.scientific.net/MSF.979.157 ↗