journal article·2022-05

Effect of shot-peening on corrosion behavior of austenitic steel in supercritical carbon dioxide at 700 °C

Yong Gui, Qinxin Zhao, Shuo Wang, Zhiyuan Liang

Corrosion Science· Volume 199
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · High-Temperature Coating Behaviors · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. B.A. Pint, J.R. Keiser, Supercritical CO2 Compatibility of Structural Alloys at 400–750 C,; Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States), 2016.
2. Thermoeconomic analysis & optimization of the combined supercritical CO2 (carbon dioxide) recompression Brayton/organic Rankine cycle10.1016/j.energy.2014.10.037 ↗
3. R.C. Moore, T.M. Conboy, Metal corrosion in a supercritical carbon dioxide - liquid sodium power cycle, in, United States, 2012.
4. D. Fleming, A. Kruizenga, J. Pasch, T. Conboy, M. Carlson, Corrosion and Erosion Behavior in Supercritical CO2 Power Cycles, in: ASME Turbo Expo 2014: Turbine Technical Conference and Exposition, 2014.10.1115/GT2014-25136 ↗
5. K. Sridharan, M. Anderson, Corrosion in supercritical carbon dioxide: materials, environmental purity, surface treatments, and flow issues, in, UT-Battelle LLC/ORNL, Oak Ridge, TN (Unted States), 2013.
6. M. Anderson, G. Nellis, M. Corradini, Materials, turbomachinery and heat exchangers for supercritical CO2 systems, in, UT-Battelle LLC/ORNL, Oak Ridge, TN (Unted States), 2012.10.2172/1053848 ↗
7. K. Sridharan, Corrosion of Structural Materials for Advanced Supercritical Carbon-Dioxide Brayton Cycle, in, Univ. of Wisconsin, Madison, WI (United States), 2017.10.2172/1358349 ↗
8. B.A. Pint, R.R. Pillai, Lifetime Model Development for Supercritical CO2 CSP Systems, in, Oak Ridge National Lab.(ORNL), Oak Ridge, TN (United States), 2019.
9. I. Wright, S. Kung, J. Shingledecker, Predicting the Oxidation/Corrosion Performance of Structural Alloys in Supercritical CO2, in, Electric Power Research Inst.(EPRI), Charlotte, NC (United States), 2017.10.2172/1415286 ↗
10. Corrosion and carburization behavior of Al-rich surface layer on Ni-base alloy in supercritical-carbon dioxide environment10.1016/j.apsusc.2015.11.162 ↗
11. Carburization resistance of cu-coated stainless steel in supercritical carbon dioxide environments10.1016/j.corsci.2020.108639 ↗
12. Surface modification of austenitic stainless steel for corrosion resistance in high temperature supercritical-carbon dioxide environment10.1016/j.surfcoat.2018.06.014 ↗
13. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20% Cr steels10.1016/j.corsci.2003.09.004 ↗
14. Effect of Surface Finish on High-Temperature Oxidation of Steels in CO2, Supercritical CO2, and Air10.1007/s11085-019-09938-6 ↗
15. Overview on corrosion in supercritical fluids10.1016/j.supflu.2016.07.022 ↗
16. Influence of Low-Temperature Pre-oxidation by Ozone on Corrosion Resistance of T91 Steel in Steam at 600 °C10.1007/s11085-018-9841-x ↗
17. Effect of Shot-peening on the Oxidation Behaviour of Boiler Steels10.1007/s11085-011-9250-x ↗
18. Effect of shot blasting on oxidation behavior of TP304H steel at 610–770 °C in water vapor10.1016/j.matlet.2005.08.046 ↗
19. Effect of shot-peening on the corrosion resistance of a Zr-based bulk metallic glass10.1016/j.scriptamat.2010.01.004 ↗
20. Effect of shot peening on high temperature oxidation behaviour of boiler steel: experimental results and simulation10.1179/174327809X419177 ↗
21. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
22. Diffusion behavior of aluminum in the surface layer of iron processed by shot peening10.1016/j.matlet.2010.03.046 ↗
23. Beneficial effect of shot peening on steamside oxidation of 300-series austenitic steels: An electrochemical study10.1016/j.apsusc.2017.08.035 ↗
24. Effect of Ultrasonic Shot Peening on Oxidation Behavior of T91 and SS347 Steels in Air and Steam at 650 °C10.1007/s11665-020-05042-y ↗
25. The negative effect of high-intensity shot-peening on the intergranular corrosion behavior of the Super304H austenitic stainless steel10.1016/j.corsci.2018.08.026 ↗
26. Engineering the residual stress state and microstructure of stainless steel with mechanical surface treatments10.1007/s00339-010-5672-6 ↗
27. Nanoscale surface modification of AISI 316L stainless steel by severe shot peening10.1016/j.matdes.2016.03.162 ↗
28. Corrosion of austenitic alloys in high temperature supercritical carbon dioxide10.1016/j.corsci.2012.03.029 ↗
29. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
30. 12 - Sanicro 25: An advanced high-strength, heat-resistant austenitic stainless steel
31. Corrosion and Carburization Behavior of Heat-Resistant Steels in a High-Temperature Supercritical Carbon Dioxide Environment10.1007/s11085-019-09917-x ↗
32. Corrosion behavior and lifetime prediction of VM12, Sanicro 25 and Inconel 617 in supercritical carbon dioxide at 600 °C10.1016/j.corsci.2020.108870 ↗
33. Structure and properties of Fe 3 O 4 films grown on ZnO template via metal organic chemical vapor deposition10.1016/j.jmmm.2015.03.018 ↗
34. Study on Local Residual Stress in a Nanocrystalline Cr2O3 Coating by Micro-Raman Spectroscopy10.3390/coatings9080500 ↗
35. The Effect of Shot Peening on Steam Oxidation of 304H Stainless Steel10.1007/s11085-019-09951-9 ↗
36. Effects of cerium and manganese on corrosion of Fe–Cr and Fe–Cr–Ni alloys in Ar–20CO2 gas at 818°C10.1016/j.corsci.2013.06.046 ↗
37. Carbon Depositions within the Oxide Scale and its Effect on the Oxidation Behavior of Low Alloy Steel in Low (0.1 MPa), Sub-(5 MPa) and Supercritical (10 MPa) CO2 at 550° C10.1016/j.corsci.2020.108950 ↗
38. Corrosion and Mechanical Performance of Grade 92 Ferritic-Martensitic Steel After Exposure to Supercritical Carbon Dioxide10.1007/s11661-020-05691-7 ↗
39. Compatibility of FBR structural materials with supercritical carbon dioxide10.1016/j.pnucene.2011.04.030 ↗
40. Shot-Peening of Pre-Oxidized Plates of Zirconium: Influence of Residual Stress on Oxidation10.1007/s11085-012-9336-0 ↗
41. Corrosion of 9-12Cr ferritic–martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
42. Corrosion Behavior of Heat-Resistant Materials in High-Temperature Carbon Dioxide Environment10.1007/s11837-018-2975-0 ↗
43. Carburisation of ferritic Fe–Cr alloys by low carbon activity gases10.1016/j.corsci.2011.05.013 ↗
44. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
45. Effect of pressure on the corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature carbon dioxide environments10.1016/j.corsci.2016.06.004 ↗
46. Corrosion of SS310 and Alloy 740 in high temperature supercritical CO2 with impurities H2O and O210.1016/j.corsci.2021.109350 ↗
47. R. Moore, T. Conboy, Metal corrosion in a supercritical carbon dioxide–liquid sodium power cycle, Sandia National Laboratory Report SAND2012–0184, (2012).
48. Corrosion of Alloy Haynes 230 in High Temperature Supercritical Carbon Dioxide with Oxygen Impurity Additions10.1007/s11085-016-9654-8 ↗
49. J. Mahaffey, D. Adam, M. Anderson, K. Sridharan, Effect of oxygen impurity on corrosion in supercritical CO2 environments, in: Proceedings of the 5th International Symposium on Supercritical CO2 Power Cycles, San Antonio, TX, 2016.
50. R.P. Oleksak, M. Kapoor, D.E. Perea, G.R. Holcomb, Ö.N. Doğan, The role of metal vacancies during high-temperature oxidation of alloys, npj Materials Degradation, 2 (2018) 25.10.1038/s41529-018-0046-1 ↗
51. Corrosion and Carburization Behaviour of Ni-xCr Binary Alloys in a High-Temperature Supercritical-Carbon Dioxide Environment10.1007/s11085-017-9811-8 ↗
52. Effect of high energy shot-peening on the microstructure and mechanical properties of Al5052/Ti6Al4V lap joints10.1016/j.jmatprotec.2017.12.005 ↗
53. Interpretation for the fast sigma phase precipitation in the high intensity shot peened nanocrystallined Super304H stainless steel10.1016/j.apsusc.2018.08.097 ↗
54. Corrosion of 9Cr Steel in CO at Intermediate Temperature I: Mechanism of Void-Induced Duplex Oxide Formation10.1007/s11085-011-9271-5 ↗