Abstract Coatings and bulks of enamel with and without CaF2 were prepared to investigate their corrosion behavior in molten Al at 750 °C. Enamel coatings provide high corrosion resistance to the 304 stainless steel against molten-Al. In the presence of 2.5 wt% CaF2, its corrosion resistance was further improved. Detail study on corrosion of the enamel bulks reveals that such role of CaF2 played on the corrosion behavior of enamel relies on the following two aspects: (1) Concentration of fluorides at surface reduces wettability; (2) Adding CaF2 changes crystallization of enamel, and different crystallites result in the varied corrosion resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear Physics and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. High temperature corrosion of carbon/carbon composites in Zr–Ti melts during liquid metal infiltration10.1016/j.corsci.2015.05.014 ↗
2. Corrosion in austenitic steels and nickel-based alloys caused by liquid tin at high temperature10.1016/j.corsci.2017.02.025 ↗
3. A review of steel corrosion by liquid lead and lead–bismuth10.1016/j.corsci.2009.03.013 ↗
4. Corrosion resistance and interfacial morphologies of novel Fe-Cr-Mo-B cast steels in molten aluminum10.1016/j.corsci.2017.05.024 ↗
5. Review on corrosion-wear resistance performance of materials in molten aluminum and its alloys10.1016/S1003-6326(15)63777-3 ↗
6. A liquid aluminum corrosion resistance surface on steel substrate10.1016/S0169-4332(03)00505-1 ↗
7. Crystallography of Fe2Al5 phase at the interface between solid Fe and liquid Al10.1016/j.intermet.2015.07.011 ↗
8. Corrosion mechanisms of steel and cast iron by molten aluminum10.1007/s11661-010-0306-3 ↗
9. Effect of Si on growth kinetics of intermetallic compounds during reaction between solid iron and molten aluminum10.1016/S1003-6326(13)62499-1 ↗
10. Degradation behaviour of boronized carbon and high alloy steels in molten aluminium and zinc10.1016/S0167-577X(98)00077-9 ↗
11. Effect of nitriding treatment on corrosion behaviour of Co–Cr–Mo alloy in liquid Al10.1016/j.corsci.2013.10.004 ↗
12. Interfacial reaction between Co–Cr–Mo alloy and liquid Al10.1016/j.corsci.2013.06.009 ↗
13. Corrosion resistance of 91W–6Ni–3Fe refractory metal, TiAl compound and iron based alloys in molten aluminum10.1016/S1003-6326(11)61466-0 ↗
14. Erosion resistance and performance characteristics of niobium ultrasonic sonotrodes in molten aluminum10.1016/j.ijrmhm.2012.04.004 ↗
15. Protection of carbon steel against molten aluminum attack and high temperature corrosion using high velocity oxygen-fuel WC–Co coatings10.1016/j.surfcoat.2014.12.023 ↗
16. Corrosion of CrN and CrN/TiN coated heat-resistant steels in molten A356 aluminum alloy10.1016/S0257-8972(01)01484-0 ↗
17. Wettability of TiAlN films by molten aluminum10.1016/j.tsf.2006.04.036 ↗
18. Corrosion behavior of zirconium diboride coated stainless steel in molten 6061 aluminum alloy10.1016/j.surfcoat.2017.01.069 ↗
19. Development of zirconium and boron containing coatings for the application on aluminium die casting tools by means of MO–PACVD10.1016/S0257-8972(97)00133-3 ↗
20. Degradation of TiB2 ceramics in liquid aluminum10.1016/j.jeurceramsoc.2008.05.011 ↗
21. Wear of cobalt-based alloys sliding in molten zinc10.1016/S0043-1648(03)00050-4 ↗
22. Corrosion resistance properties of enamels with high B2O3-P2O5 content to molten aluminum10.1016/S0921-5093(02)00527-0 ↗
23. Effect of grain boundary cracks on the corrosion behaviour of aluminium titanate ceramics in a molten aluminium alloy10.1016/j.corsci.2011.09.002 ↗
24. Additives and the corrosion resistance of aluminosilicate refractories in molten Al-5Mg10.1007/s11837-998-0245-2 ↗
25. The effect of SrSO4 and BaSO4 on the corrosion and wetting by molten aluminum alloys of mullite ceramics10.1016/j.ceramint.2010.01.015 ↗
26. Effect of CaF2 on interfacial phenomena of high of high alumina refractories with Al alloy10.1007/s11663-008-9169-z ↗
27. Effects of different calcium compounds on the corrosion resistance of andalusite-base low-cement castables in contact with molten Al-Alloy10.1007/s11663-010-9468-z ↗
28. Influence investigation of CaF2 on the LAS based glass-ceramics and the glass-ceramic/diamond composites10.1016/j.jeurceramsoc.2016.03.020 ↗
29. Crystallization mechanism of the bioactive glasses, 45S5 and S53P410.1111/j.1551-2916.2011.05012.x ↗
30. Furnaces: improving low cement castables by non-wetting additives10.1007/s11837-001-0130-8 ↗
31. Sosman · 1965
32. Microstructures and properties of interpenetrating alumina/aluminium composites made by reaction of SiO2 glass preforms with molten aluminium10.1016/0921-5093(95)10078-4 ↗
33. The structure of quartz at 25 and 590°C determined by neutron diffraction10.1016/0022-4596(81)90449-7 ↗
34. Microstructure and properties of inter-locked mullite framework prepared by the TBA-based gel-casting process10.1016/j.ceramint.2016.06.197 ↗
35. Abnormal behavior of silica doped with small amounts of aluminum
36. Structure and properties of mullite-A review10.1016/j.jeurceramsoc.2007.03.017 ↗